Abstract

Abstract The role of alloying elements on the hydrogen embrittlement (HE) susceptibility of a Fe–18Mn–0.6C alloy was investigated by in situ tensile tests and characterized by the ductility loss associated with intergranular fracture. Under cathodic polarization an improvement of HE resistance is related to the SFE increase with Cu or Al additions reducing the stress–strain and H localization at grain boundaries, which prevents H-induced intergranular cracking. At rest potential, beneficial effects of Cu and Al are related to their influence on hydrogen absorption during the corrosion process. However, residual phosphorus strongly reduces the beneficial effect of aluminum.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Microstructure and Mechanical Properties of Steels · Corrosion Behavior and Inhibition

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (38)

Show source-provided references
1. S. Allain, Caractérisation et modélisation thermomécaniques multi-échelles des mécanismes de déformation et d’écrouissage d’aciers austénitiques à haute teneur en manganèse – application à l’effet TWIP, PhD Thesis, NNT 2004INPL006N, Institut National Polytechnique de Lorraine, France, 2004.
2. Ultra high strength FeMn TWIP steels for automotive safety parts10.1051/metal:2005151 ↗
3. The development of a new Fe–Mn–C austenitic steel for automotive applications10.1051/metal:2006142 ↗
4. Effect of hydrogen on fracture of austenitic Fe–Mn–Al steel10.2355/isijinternational.34.211 ↗
5. Hydrogen delayed fracture properties and internal hydrogen behavior of a Fe–18Mn–1.5Al–0.6C TWIP steel10.2355/isijinternational.49.1952 ↗
6. G. Lovicu, M. Barloscio, M. De Sanctis, A. Dimatteo, C. Santus, R. Valentini, M. Bottazzi, F. D’Aiuto, C. Federici, S. Maggi, Hydrogen embrittlement of advanced high strength steel for automotive use, in: 2nd International Conference “Super High Strength Steels”, Italie, 2010.
7. Hydrogen embrittlement of commercially produced advanced high strength sheet steels10.4271/2010-01-0447 ↗
8. P. Cugy, P. Dietsch, J. Goncalves, C.P. Scott, The development of the K’7 model for the prediction of the stress corrosion cracking in austenitic TWIP steels, in: Steely Hydrogen Conference Proceedings, ISBN 9789081794206, 2011, pp. 175–188.
9. Hydrogen embrittlement in a Fe–Mn–C ternary twinning-induced plasticity steel10.1016/j.corsci.2011.09.022 ↗
10. T. Dieudonné, L. Marchetti, M. Wery, F. Jomard, F. Miserque, M. Tabarant, J. Chêne, C. Allely, P. Cugy, C.P. Scott, Role of Cu and Al on the corrosion behaviour of austenitic Fe–Mn–C TWIP steels in aqueous solutions and the related hydrogen absorption, Corros. Sci., (2014), .
11. SIMS analysis of deuterium absorption and diffusion in austenitic Fe–Mn–C steels10.4028/www.scientific.net/DDF.323-325.477 ↗
12. Effect of hydrogen content on the embrittlement in a Fe–Mn–C twinning-induced plasticity steel10.1016/j.corsci.2012.03.009 ↗
13. T. Dieudonné, Mécanismes d’absorption de l’hydrogène en milieu aqueux dans des aciers austénitiques Fe–Mn–C; conséquences sur l’endommagement, PhD thesis, NNT 2012EVRY011, Université d’Evry Val d’Essonne, France, 2012.
14. Effects of Al addition on deformation and fracture mechanisms in two high manganese TWIP steels10.1016/j.msea.2010.12.085 ↗
15. X. Guo, W. Bleck, Delayed fracture in CrNi- and Mn-based austenitic steels: effects of austenite stability, hydrogen and tensile strain rate, in: Steely Hydrogen Conference Proceedings, ISBN 9789081794206, 2011, pp. 196–208.
16. A. Dumay, Amélioration des propriétés physiques et mécaniques d’aciers TWIP FeMnXC: influence de la solution solide, durcissement par précipitation et effet composite, PhD Thesis, NNT 2008INPL014N, Institut National Polytechnique de Lorraine, France, 2008, .
17. Precipitation strengthening in high manganese austenitic TWIP steels10.3139/146.110508 ↗
18. Effect of grain and twin boundaries on the hardening mechanisms of twinning-induced plasticity steels10.1016/j.scriptamat.2007.10.050 ↗
19. The influence of plastic instabilities on the mechanical properties of a high-manganese austenitic FeMnC steel10.3139/146.101693 ↗
20. On the origin of dynamic strain aging in twinning-induced plasticity steels10.1016/j.actamat.2011.07.040 ↗
21. Effect of Al on the stacking fault energy of Fe–18Mn–0.6C twinning-induced plasticity10.1016/j.scriptamat.2011.05.014 ↗
22. Effects of environmental species and metallurgical structure on the hydrogen entry into steel
23. The effect of phosphorus content on the hydrogen stress cracking of high strength 4130 steel10.1007/BF02642405 ↗
24. Environment-induced crack growth processes in nickel-base alloys
25. Hydrogen-induced intergranular fracture of steels10.1016/S0013-7944(00)00124-7 ↗
26. Influence of phosphorus and boron on hydrogen embrittlement susceptibility of high strength low alloy steel10.2355/isijinternational.43.1851 ↗
27. Hydrogen effects on cathodically charged twinning-induced plasticity steel10.1016/j.scriptamat.2011.12.012 ↗
28. Mechanisms of hydrogen-related fracture of metals
29. Influence de l’écrouissage sur le frottement intérieur du fer et de l’acier, chargés ou non en hydrogène
30. Hydrogen transport by mobile dislocations in nickel base superalloy single crystals10.1016/S1359-6462(98)00451-5 ↗
31. Role of temperature and strain rate on the hydrogen-induced intergranular rupture in alloy 60010.1007/s11661-004-0356-5 ↗
32. Strain assisted transport of hydrogen and related effects on the intergranular stress corrosion cracking of alloy 600
33. Hydrogen-assisted failure in a twinning-induced plasticity steel studied under in situ hydrogen charging by electron channelling contrast imaging10.1016/j.actamat.2013.04.030 ↗
34. Effect of aluminium on hydrogen-induced fracture behaviour in austenitic Fe–Mn–C steel10.1098/rspa.2012.0458 ↗
35. Influence of addition elements on the stacking-fault energy and mechanical properties of an austenitic Fe–Mn–C steel10.1016/j.msea.2006.12.170 ↗
36. Stacking fault energy and plastic deformation of fully austenitic high manganese steels: effect of Al addition10.1016/j.msea.2010.02.058 ↗
37. Hydrogen embrittlement in Al-added twinning-induced plasticity steels evaluated by tensile tests during hydrogen charging10.2355/isijinternational.52.2283 ↗
38. Electrochemical and surface analytical studies on hydrogen permeation with Fe–Cu alloys in sulfuric acid with and without H2S10.1016/0010-938X(84)90077-5 ↗