Self-healing protective films of 1,2-bis(triethoxysilyl)ethane (C2H5O)3Si(CH2)2Si(OC2H5)3 (abbreviated to BTESE) polymer containing sodium silicate Na2Si2O5 (water glass) and cerium(III) nitrate Ce(NO3)3 were prepared on a zinc electrode previously treated in a 1×10−3 M Ce(NO3)3 solution at 30 °C for 30 min. After the surface of coated electrode was crosswise scratched with a knife edge, the electrode was immersed in an aerated 0.5 M NaCl solution at 30 °C for many hours and polarization measurements of the scratched electrode were carried out for estimating the self-healing effects of the films on zinc corrosion at the scratches. The optimal quantities of Na2Si2O5, Ce(NO3)3 and BTESE in the films were determined by polarization measurements and observation of pit formation at the scratches. No pitting corrosion occurred at the scratches on the zinc electrode covered with a film composed of their optimal quantities after immersion in the solution for 72 h.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Corrosion Behavior and Inhibition · Concrete Corrosion and Durability · Polymer composites and self-healing

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (18)

Show source-provided references
1. Xia · J. Electrochem. Soc. · 1998 · 145 · 308310.1149/1.1838768 ↗
2. Suda · Zairyo-to-Kankyo (Corros. Eng.) · 1997 · 46 · 9510.3323/jcorr1991.46.95 ↗
3. N.I. Sax, R.J. Lewis Sr., Dangerous Properties of Industrial Materials, seventh ed., vol. II, Van Nostrand Reinhold, New York, 1989, p. 745
4. Aramaki · Corrosion · 1999 · 55 · 102010.5006/1.3283939 ↗
5. Aramaki · Corrosion · 2000 · 56 · 90110.5006/1.3280593 ↗
6. Aramaki · Corros. Sci. · 2000 · 42 · 197510.1016/S0010-938X(00)00031-7 ↗
7. Aramaki · Corros. Sci. · 2000 · 42 · 202310.1016/S0010-938X(00)00037-8 ↗
8. Aramaki · 2000 · vol. 1 · 387
9. Aramaki · Corros. Sci. · 2001 · 43 · 59110.1016/S0010-938X(00)00085-8 ↗
10. K. Aramaki, Corros. Sci. 43 (2001) 198510.1016/S0010-938X(00)00174-8 ↗
11. Aramaki · Corros. Sci. · 2001 · 43 · 157310.1016/S0010-938X(00)00144-X ↗
12. Hinton · Corros. Sci. · 1989 · 29 · 96710.1016/0010-938X(89)90087-5 ↗
13. Powell · Corrosion · 1999 · 55 · 104010.5006/1.3283941 ↗
14. Arenas · Corros. Sci. · 2001 · 43 · 15710.1016/S0010-938X(00)00051-2 ↗
15. K. Aramaki, Corros. Sci. 43 (2001) 220110.1016/S0010-938X(00)00189-X ↗
16. K. Aramaki, Corros. Sci. in press
17. Proc. JSCE Materials and Environments 2001, Japan Society of Corrosion Engineering, Tokyo, 2001, p. 235
18. Cunico · J. Org. Chem. · 1980 · 45 · 479710.1021/jo01311a058 ↗