Effect of surface finishing of a Zr-based bulk metallic glass on its corrosion behaviour
Source abstract
Abstract
Abstract Zr-based metallic glasses passivate spontaneously, but exhibit also a certain pitting susceptibility. On the example of the Zr59Ti3Cu20Al10Ni8 alloy studied in 0.01 M Na2SO4 + x M NaCl (x = 0–0.1) electrolytes it is demonstrated that the surface finishing state and the pre-exposure conditions can significantly influence the free corrosion and anodic polarisation behaviour. Mechanical fine-polishing procedures can lead to extremely smooth topographies but also to Cu enrichment at the surface. This yields a pronounced Cu dissolution at low anodic polarisation prior to stable passivity and increases the pitting initiation susceptibility as compared to mechanically ground surface states.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Metallic Glasses and Amorphous Alloys · Phase-change materials and chalcogenides · Electrodeposition and Electroless Coatings
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (48)
Show source-provided references
1. Developments and applications of bulk metallic glasses
2. Bulk metallic glasses: what are they good for?10.1016/j.msea.2003.10.167 ↗
3. Thermoplastic forming of bulk metallic glass – applications for MEMS and microstructure fabrication10.1016/j.msea.2006.02.398 ↗
4. Nano-fabrication with metallic glass – an exotic material for nano-electromechanical systems10.1088/0957-4484/18/3/035302 ↗
5. Nanomoulding with amorphous metals10.1038/nature07718 ↗
6. Fabrication and characterization of metallic glasses with a specific microstructure for micro-electro-mechanical system applications10.1016/j.jnoncrysol.2008.01.030 ↗
7. Preparation of high aspect ratio surface microstructures out of a Zr-based bulk metallic glass10.1016/S0167-9317(03)00096-0 ↗
8. Effect of structural defects, surface irregularities, and quenched-in defects on corrosion of Zr-based metallic glasses10.1007/s11661-009-9810-8 ↗
9. Chip formation, cutting forces, and tool wear in turning of Zr-based bulk metallic glass10.1016/j.ijmachtools.2004.02.002 ↗
10. Electrochemical reactivity of zirconium-based bulk metallic glasses
11. Corrosion and related mechanical properties of bulk metallic glasses10.1557/jmr.2007.0051 ↗
12. Effect of pH on the polarization behavior of Zr65Al7.5Ni10Cu17.5 amorphous alloy in a phosphate-buffered solution10.1016/S0010-938X(00)00056-1 ↗
13. Cyclic-anodic-polarization studies of a Zr41.2Ti13.8Ni10Cu12.5Be22.5 bulk metallic glass10.1016/j.intermet.2004.04.005 ↗
14. Potentiodynamic polarization studies on amorphous Zr46.75Ti8.25Cu7.5Ni10Be27.5, Zr65Cu17.5Ni10Al7.5, Zr67Ni33 and Ti60Ni40 in aqueous HNO3 solutions10.1016/j.jnoncrysol.2007.05.002 ↗
15. Investigations on the electrochemical behaviour of Zr-based bulk metallic glasses10.1016/S0921-5093(99)00105-7 ↗
16. Pitting corrosion of bulk glass-forming zirconium-based alloys10.1016/j.jallcom.2004.01.043 ↗
17. Characterization of oxide layers on amorphous Zr-based alloys by Auger electron spectroscopy with sputter depth profiling10.1016/j.apsusc.2005.02.026 ↗
18. A study of the corrosion behaviour of Zr50Cu(40−x)Al10Pdx bulk metallic glasses with scanning Auger microanalysis10.1016/j.corsci.2008.03.011 ↗
19. Element-specific in situ corrosion behaviour of Zr–Cu–Ni–Al–Nb bulk metallic glass in acidic media studied using a novel microcapillary flow injection inductively coupled plasma mass spectrometry technique10.1016/j.intermet.2008.06.005 ↗
20. An Auger electron spectroscopic study of the corrosion behaviour of an amorphous Zr40Cu60 alloy10.1016/S0010-938X(96)00108-4 ↗
21. Effect of oxygen and hydrogen on the surface segregation of amorphous and crystalline alloys10.1016/S0039-6028(87)80558-7 ↗
22. Cu precipitations at the surface of crystalline Cu–Zr alloys after annealing in hydrogen10.1524/zpch.1989.164.Part_2.1171 ↗
23. In situ observation of pitting corrosion of the Zr50Cu40Al10 bulk metallic glass10.1016/j.intermet.2008.12.011 ↗
24. Electrochemical investigations on the bulk glass forming Zr55Cu30Al10Ni5 alloy10.1002/maco.19970480504 ↗
25. Pitting corrosion of zirconium-based bulk glass–matrix composites10.1016/j.msea.2005.09.062 ↗
26. Comparison of the corrosion behaviour of a bulk amorphous metal, Zr41.2Ti13.8Cu12.5Ni10Be22.5, with its crystallized form10.1016/S1359-6462(98)00089-X ↗
27. Localized corrosion behaviour of a zirconium-based bulk metallic glass relative to its crystalline state10.1016/S0966-9795(02)00130-9 ↗
28. Corrosion behavior of Zr–(Nb–)Al–Ni–Cu glassy alloys10.2320/matertrans1989.41.1490 ↗
29. Formation, corrosion behavior, and mechanical properties of bulk glassy Zr–Al–Co–Nb alloys10.1557/JMR.2003.0227 ↗
30. Corrosion behaviour of Zr-based bulk glass-forming alloys containing Nb or Ti10.1016/S0167-577X(02)00725-5 ↗
31. Effect of microalloying of Nb on corrosion resistance and thermal stability of ZrCu-based bulk metallic glasses10.1016/j.jnoncrysol.2008.10.011 ↗
32. Influence of the degree of polishing of alloy AA 5083 on its behaviour against localised alkaline corrosion10.1016/j.corsci.2003.10.028 ↗
33. The influence of surface condition on the localized corrosion of 316L stainless steel orthopaedic implants10.1023/A:1008918929036 ↗
34. Influence of surface polishing on the electrochemical behaviour of titanium10.1149/1.1996509 ↗
35. Effects of surface finishing and dissolved oxygen on the polarization behaviour of Zr65Al7.5Ni10Cu17.5 amorphous alloy in phosphate buffered solution10.1016/S0010-938X(00)00043-3 ↗
36. Limited quasicrystal formation in Zr–Ti–Cu–Ni–Al bulk metallic glasses10.1016/j.actamat.2006.05.049 ↗
37. Watts · 2003
38. Effect of hydrogen on Zr65Cu17.5Al7.5Ni10 metallic glass10.1016/S0925-8388(00)01211-1 ↗
39. Low temperature annealing: a novel route for making plastic bulk metallic glasses10.1016/j.msea.2008.01.083 ↗
40. Work-hardenable ductile bulk metallic glass10.1103/PhysRevLett.94.205501 ↗
41. The oxidation of amorphous Zr-based binary alloys in air10.1016/0010-938X(93)90308-4 ↗
42. Influence of some parameters on passivation of zirconium and the stability of the anodic oxide film10.5006/1.3284044 ↗
43. Photoelectrochemical characterization of thin anodic oxide films on zirconium metal10.1016/0013-4686(96)00064-3 ↗
44. Pourbaix · 1966
45. Acid corrosion of amorphous and crystalline Cu–Zr alloys10.1016/0169-4332(88)90036-0 ↗
46. The influence of structure on the corrosion of glassy copper–zirconium alloys10.5006/1.3581912 ↗
47. Corrosion behaviour of amorphous and crystalline Cu50Ti50 and Cu50Zr50 alloys10.1016/0022-3093(78)90053-4 ↗
48. Corrosion of a Zr-based bulk metallic glass with different state after surface finishings10.1149/1.3091901 ↗