Abstract

Abstract A SiO 2 –Al 2 O 3 –glass composite coating was prepared on Ti–6Al–4V alloy by air spraying and subsequent firing. The oxidation behavior of the specimens at 800 °C and 900 °C for 100 h was studied. The thermal shock resistance of the coating was tested by heating up to 900 °C and then quenching in water. The composite coating acted as an oxygen migration barrier and exhibited good resistance against high temperature oxidation, thermal shock, and oxygen permeation on the Ti–6Al–4V alloy. Coating/alloy interfacial reaction occurred, forming a Ti 5 Si 3 /Ti 3 Al bilayer structure. A thin Al 2 O 3 rich layer formed beneath the composite coating during oxidation at 900 °C.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Intermetallics and Advanced Alloy Properties · High-Temperature Coating Behaviors · Metal and Thin Film Mechanics

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (40)

Show source-provided references
1. Titanium alloy for aerospace applications10.1002/adem.200310095 ↗
2. Air oxidation behavior of Ti–6Al–4V alloy between 650 and 850°C10.1016/0010-938X(94)90069-8 ↗
3. High temperature oxidation behaviour of a TiAl–Al2O3 intermetallic matrix composite10.1016/j.corsci.2003.10.026 ↗
4. Oxidation behavior of Ti–46.7Al–1.9W–0.5Si in air and Ar–20%O2 between 750°C and 950°C10.1016/j.corsci.2004.08.014 ↗
5. Oxidation of High-Temperature Intermetallics
6. The oxidation behavior and mechanical performance of Ti60 alloy with enamel coating10.1016/j.surfcoat.2004.09.005 ↗
7. Oxidation and embrittlement of Ti–6AI–2Sn–4Zr–2Mo Alloy10.1007/BF00664276 ↗
8. Influence of long-term annealing on tensile properties and fracture of near-a titanium alloy Ti–6Al–2.75S n–4Zr–0.4Mo–0.45Si10.1007/BF02649829 ↗
9. Microstructure, properties and oxidation behavior of the glass–ceramic based coating on near-α titanium alloy10.1016/j.surfcoat.2009.02.016 ↗
10. Microstructure and properties characterisation of the double layered glass–ceramic coating on near-α titanium alloy10.1016/j.surfcoat.2010.04.008 ↗
11. Synergistic corrosion behavior of coated Ti60 alloys with NaCl deposit in moist air at elevated temperature10.1016/j.corsci.2007.06.007 ↗
12. The oxidation behavior of TiAlNb intermetallics with coatings at 800°C10.1016/j.surfcoat.2004.11.019 ↗
13. Oxidation protection of gamma-titanium aluminide using glass–ceramic coatings10.1016/j.surfcoat.2008.12.029 ↗
14. Effect of Al2O3 and enamel coatings on 900°C oxidation and hot corrosion behaviors of gamma-TiAl10.1016/S0921-5093(99)00513-4 ↗
15. Effect of vitreous enamel coating on the oxidation behavior of Ti6Al4V and TiAl alloys at high temperatures10.1007/s11998-007-9057-5 ↗
16. Glass–ceramic seal to join Crofer 22 APU alloy to YSZ ceramic in planar SOFCs10.1016/j.jeurceramsoc.2007.05.006 ↗
17. Comparison between barium and strontium–glass composites for sealing SOFCs10.1016/j.jeurceramsoc.2005.08.002 ↗
18. Water-based sodium borosilicate sols and their gelation-characterisation by viscosimetry, UV/VIS and infrared spectroscopy10.1023/A:1020283206199 ↗
19. Continuous fiber reinforced titanium matrix composites: fabrication, properties and applications10.1002/adem.200310093 ↗
20. The oxidation and oxygen permeation resistance of quartz particle-reinforced aluminosilicate glass coating on titanium alloy10.1111/j.1551-2916.2011.04587.x ↗
21. M.S. Li (Ed.), High Temperature Corrosion of the Metal, first ed., Beijing, 2001 (in Chinese).
22. Study on controlling thermal expansion coefficient of ZrO2–TiO2 ceramic die for superplastic blow-forming high accuracy Ti–6Al–4V component10.1016/j.matdes.2009.03.023 ↗
23. B.Y. Huang, C.G. Li, L.K. Shi, G.Z. Qiu, T.Y. Zuo (Eds.), China Materials Engineering Canon, vol. 4, first ed., Beijing, 2006 (in Chinese).
24. Cyclic oxidation behavior of glass–ceramic composite coatings on superalloy K38G at 1100°C10.1016/j.tsf.2011.01.047 ↗
25. Hydrogen permeation resistant glass–ceramic coatings for gamma–titanium aluminide10.1016/j.surfcoat.2009.08.001 ↗
26. Oxidation and hot corrosion behavior of a novel enamel-Al2O3 composite coating on K38G superalloy10.1016/j.surfcoat.2005.09.004 ↗
27. The titanium molten glass system interactions and wetting10.1007/BF00553934 ↗
28. Silicate glass coatings on Ti-based implants10.1016/S1359-6454(98)80039-6 ↗
29. Fabrication and characterization of a bioactive glass coating on titanium implant alloys10.1016/S1359-6454(99)00280-3 ↗
30. Glass-based coatings for titanium implant alloys10.1002/(SICI)1097-4636(19990915)46:4<549::AID-JBM13>3.0.CO;2-M ↗
31. Bioactive glass coatings for orthopedic metallic implants10.1016/S0955-2219(03)00303-0 ↗
32. Preparation, properties and chemistry of glass and glass-ceramic-to-metal seals and coatings10.1007/BF00354689 ↗
33. Y.J. Liang, Y.C. Che, Handbook of Thermodynamic Data for Inorganic Compounds, first ed., Shenyang, 1993 (in Chinese).
34. Influence of siliconizing on the oxidation behavior of a γ-TiAl based alloy10.1016/S0966-9795(02)00193-0 ↗
35. Molten glass corrosion resistance of MoxRuySiz compounds at 1350°C in an alkali borosilicate glass10.1016/j.corsci.2005.06.002 ↗
36. Thermal expansion of mixed-alkali silicate glasses10.1063/1.322418 ↗
37. Structure and properties of high Li2O-containing aluminophosphate glasses10.1016/j.jeurceramsoc.2008.12.016 ↗
38. The stability relations of the silica minerals10.2475/ajs.s4-36.214.331 ↗
39. Effect of firing conditions, filler grain size and quartz content on bending strength and physical properties of sanitary ware porcelain10.1016/j.jeurceramsoc.2003.07.003 ↗
40. Fracture patterns of quartz particles in glass feldspar matrix10.1016/j.matlet.2011.12.074 ↗