Cathodic protection afforded by an intermittent current applied to reinforced concrete
Source abstract
Abstract
Abstract In this work, intermittent cathodic protection was applied to chloride contaminated reinforced concrete exposed to simulated tidal zone conditions. It was observed that an integrated protection current of just 6 mA/m 2 induced the passivation of steel exhibiting an initial corrosion rate of 60 mA/m 2 in conditions characterised by weakly polarised cathodic reaction kinetics. This provides the first direct laboratory evidence that protection may be achieved with a cathodic current that is small compared to the corrosion rate. In this case the protective effects of a negative potential shift may be ignored; it is the changes in the environment at the cathode that induce passivation and provide the basis for cathodic protection. Such changes occur slowly and do not give the instantaneous protection offered by a large negative potential shift. A large potential shift combined with a reducing environment may be generated in saturated conditions characterised by strongly polarised cathodic reaction kinetics. Both passivating and reducing environments at the steel will persist following current interruption. The dominance of these persistent effects suggests that the integrated value of the current required for protection will be insensitive to current variations. Positive trends in open circuit potentials or sustained negative potentials are indicative of passivating and reducing conditions respectively, although an intermittent current complicates non-destructive performance assessment.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Concrete Corrosion and Durability · Corrosion Behavior and Inhibition · Smart Materials for Construction
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (37)
Show source-provided references
1. Glass · Corros. Sci. · 1986 · 26 · 44110.1016/0010-938X(86)90139-3 ↗
2. G.K. Glass, W.K. Green, J.R. Chadwick, Proceedings of UK Corrosion 91, vol. 3, Institute of Corrosion, Leighton Buzzard, UK, 1991
3. Hassanein · Brit. Corros. J. · 1999 · 34 · 25410.1179/000705999101500932 ↗
4. Glass · Corros. Sci. · 1995 · 37 · 164310.1016/0010-938X(95)00116-2 ↗
5. Glass · Corros. Sci. · 1994 · 36 · 219310.1016/0010-938X(94)90017-5 ↗
6. Hassanein · Corrosion · 1999 · 55 · 84010.5006/1.3284040 ↗
7. G.K. Glass, A.M. Hassanein, N.R. Buenfeld, Proceedings of UK Corrosion 95, vol. 1, Institute of Corrosion, Leighton Buzzard, UK, 1995, p. 17
8. Glass · J. Mater. Civil Eng. · 2000 · 12 · 16410.1061/(ASCE)0899-1561(2000)12:2(164) ↗
9. A.M. Hassanein, G.K. Glass, N.R. Buenfeld, in: C.L. Page, P.B. Bamforth, J.W. Figg (Eds.), Corrosion of Reinforcement in Concrete Construction, Society of Chemical Industry, London, UK, 1996, p. 407
10. Kessler · Mater. Performance · 1998 · 37 · 14
11. Glass · Corros. Sci. · 1997 · 39 · 145110.1016/S0010-938X(97)00051-6 ↗
12. Glass · Corros. Sci. · 1997 · 39 · 165710.1016/S0010-938X(97)00071-1 ↗
13. Gowers · Brit. Corros. J. · 1994 · 29 · 2510.1179/000705994798267999 ↗
14. González · Brit. Corros. J. · 1982 · 17 · 2110.1179/000705982798274589 ↗
15. H. Arup, in: A.P. Crane (Ed.), Proceedings of the First International Symposium on Corrosion of Reinforcement in Concrete Construction, Ellis Horwood, Chichester, 1983, p. 151
16. C.L. Page, in: P. Schiessl (Ed.), Corrosion of Steel in Concrete, Chapman and Hall, London, 1988, pp. 17–21
17. Glass · Corros. Sci. · 1991 · 32 · 128310.1016/0010-938X(91)90048-T ↗
18. V. Ashworth, in: L.L. Shreir, R.A. Jarman, G.T. Burstein (Eds.), Corrosion, vol. 2, Corrosion Control, third ed., Butterworth–Heinemann, Oxford, 1994, pp. 10:3–10:28
19. Glass · Brit. Corros. J. · 1997 · 32 · 17910.1179/bcj.1997.32.3.179 ↗
20. Concrete Society Technical Report No 37, Model specification for cathodic protection of reinforced concrete, The Concrete Society, Slough, UK, 1991
21. Flis · Corrosion · 1993 · 49 · 60110.5006/1.3316091 ↗
22. Glass · Mater. Performance · 1996 · 35 · 36
23. J.P. Broomfield, J.S. Tinnea, Cathodic protection of reinforced concrete bridge components, Report no. SHRP-C/UWP-92-618, Strategic Highway Research Program, Washington DC, 1993
24. BS 7361: Part 1, Cathodic protection – code of practice for land and marine applications, British Standards Institute, London, UK, 1991
25. Glass · Corros. Sci. · 2000 · 42 · 92310.1016/S0010-938X(99)00121-3 ↗
26. G.K. Glass, B. Reddy, N.R. Buenfeld, Corros. Sci. 42 (2000) 201310.1016/S0010-938X(00)00040-8 ↗
27. Glass · Corros. Sci. · 2000 · 42 · 32910.1016/S0010-938X(99)00083-9 ↗
28. Sagues · Corrosion · 1992 · 48 · 62410.5006/1.3315982 ↗
29. Glass · Corrosion · 1998 · 54 · 88710.5006/1.3284808 ↗
30. Diakow · Mater. Performance · 1998 · 37 · 17
31. Takewaka · Corros. Sci. · 1993 · 35 · 161710.1016/0010-938X(93)90391-S ↗
32. Glass · Corrosion · 1999 · 55 · 28610.5006/1.3283989 ↗
33. J. Bennett, K.C. Clear, W.H. Hartt, D.R. Lankard, T.J. Schue, W.J. Swiat, Electrochemical chloride removal and protection of concrete bridge components: laboratory studies, Report no. SHRP-S-657, Strategic Highway Research Program, Washington, DC, 1993
34. K.M Lawson, N.G. Thompson, An electrochemical method for detecting ongoing corrosion of steel in a concrete structure with CP applied, Report no. SHRP-ID/UFR-91-512, Strategic Highway Research Program, Washington, DC, 1991
35. M. Pourbaix, Atlas of Electrochemical Equilibria in Aqueous Solutions, first ed., NACE, Houston, TX, 1966, p. 312
36. J. Bennett, T. Turk, Technical alert–criteria for the cathodic protection of reinforced concrete bridge elements, Report no. SHRP-S-359, Strategic Highway Research Program, Washington, DC, 1994
37. Glass · Corrosion · 1995 · 51 · 72110.5006/1.3293635 ↗