Abstract

Abstract An iron ingot immersed during 2000 years at 12 m depth in the sea has been examined with the help of a combination of microscale techniques. This methodology allowed us to show that the main phase precipitated during the immersion is an iron hydroxychloride (β-Fe 2 (OH) 3 Cl) that is characteristic of corrosion in anoxic and chlorinated medium. Moreover locally on the external part of the corrosion products sulphur containing phases have been identified as mackinawite (FeS) in nanocrystalline or slightly oxidised state. The presence of this phase could be explained by the activity of sulphate-reducing bacteria. The presence of β-Fe 2 (OH) 3 Cl could be interpreted via a thermodynamic modelling taking into account the environmental conditions.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Corrosion Behavior and Inhibition · Hydrogen embrittlement and corrosion behaviors in metals · Building materials and conservation

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (49)

Show source-provided references
1. The corrosion of excavated archaeological iron with details on weeping and akaganeite10.2307/1506652 ↗
2. Post-excavation changes in iron antiquities10.2307/1506144 ↗
3. L. Selwyn, Overview of archaeological iron: the corrosion problem, key factors affecting treatment, and gaps in current knowledge, in: Metal 2004: 2004; National Museum of Australia, Canberra: National Museum of Australia, 2004, pp. 294–306.
4. Thermal decomposition of FeOCl and marine cast iron corrosion products10.2307/1505896 ↗
5. J.-B. Memet, La corrosion marine des structures métalliques portuaires: étude des mécanismes d’amorçage et de croissance des produits de corrosion, Université de La Rochelle; 2000.
6. Electrochemical impedance spectroscopy of a free-standing oxide film10.1016/S0013-4686(01)00816-7 ↗
7. Formation of the Fe(II)-Fe(III) hydroxysulfate green rust during marine corrosion of steel10.1016/S0010-938X(02)00184-1 ↗
8. On the formation of β-FeOOH (Akaganeite) in chloride-containing environments10.1016/j.corsci.2006.06.003 ↗
9. Seawater corrosivity around the world: results from three years of testing
10. Development of high strength low alloy steels for marine applications, part 1: results of long term exposure tests on commercially available and experimental steels10.1179/000705986798272136 ↗
11. The changing topography of corroding mild steel surfaces in seawater10.1016/j.corsci.2006.11.003 ↗
12. Seawater corrosivity around the world: results from five years of testing
13. Pitting corrosion of mild steel in marine immersion environment, part 1: maximum pit depth10.5006/1.3287863 ↗
14. The role of sulphate-reducing and sulphur-oxidizing bacteria in the localized corrosion of iron-based alloys – a review
15. W.A. Hamilton, Biocorrosion: the action of sulphate reducing bacteria, in: Biochemistry of microbial Degradation. Kluwer Academic Publishers, Dordrecht ed, 1994, pp. 555–570.10.1007/978-94-011-1687-9_17 ↗
16. Role of sulfate-reducing bacterie in corrosion of mild steels: a review10.1080/08927019509378271 ↗
17. Bacteriological influence in the development of iron sulphide species in marine immersion environments10.1016/S0010-938X(02)00147-6 ↗
18. Formation of the Fe(II-III) hydroxysulphate green rust during marine corrosion of steel associated to molecular detection of dissimilatory sulphite-reductase10.1016/j.corsci.2007.11.029 ↗
19. Modelling of marine immersion corrosion for mild and low alloy steels – Part 1: phenomenological model10.5006/1.3277564 ↗
20. Models for the anaerobic phases of marine immersion corrosion10.1016/j.corsci.2005.05.039 ↗
21. Corrosion of iron archaeological artefacts in soil: characterisation of the corrosion system10.1016/j.corsci.2004.05.029 ↗
22. Corrosion of iron archaeological artefacts in soil: Estimation of the average corrosion rates involving analytical techniques and thermodynamic calculations10.1016/j.corsci.2005.11.013 ↗
23. Buried iron archaeological artefacts: corrosion mechanisms related to the presence of Cl-containing phases10.1016/j.corsci.2006.11.009 ↗
24. Long-term corrosion behaviour of low-carbon steel in anoxic environment: characterisation of archaeological artefacts10.1016/j.jnucmat.2008.06.019 ↗
25. Dillmann · 2007
26. Corrosion behaviour of reinforced concrete: Laboratory experiments and archaeological analogues for long-term predictive modelling10.1016/j.jnucmat.2008.06.018 ↗
27. 2004
28. 2001
29. L. Long, Au Large des Saintes Maries de la Mer, Bilan scientifique du Département des Recherches Archéologiques Subaquatiques et Sous Marines (DRASSM) 2002. In.; 2003, pp. 51–57.
30. Réseaux de production et standards de commercialisation du fer antique en méditerranée: les demi-produits des épaves romaines des Saintes-Maries-de-la-Mer (Bouches-du-Rhône, France)10.3406/ran.2008.1194 ↗
31. Characterisation of iron archaeological analogues using micro diffraction under synchrotron radiation. Application to the study of long term corrosion behaviour of low alloy steels10.1051/jp4:20020248 ↗
32. Two-dimensional detector software: from real detector to idealised image or two-theta scan10.1080/08957959608201408 ↗
33. Structural characterization of corrosion products on archaeological iron. An integrated analytical approach to establish corrosion forms10.1002/jrs.1130 ↗
34. Deterioration of iron archaeological artefacts: μRaman investigation on chlorinated phases10.1002/jrs.1659 ↗
35. Formation, fast oxidation and thermodynamic data of Fe(II) hydroxychlorides10.1016/j.corsci.2007.08.017 ↗
36. Characterisation of mackinawite by Raman spectroscopy: effects of crystallisation. Drying and oxidation10.1016/j.corsci.2008.08.041 ↗
37. Characterization of ancient Indian iron and entrapped slag inclusions using electron, photon and nuclear microprobes10.1007/BF02704929 ↗
38. Slag inclusion analyses for studying ferrous alloys employed in French medieval buildings: supply of materials and diffusion of smelting processes10.1016/j.jas.2006.12.022 ↗
39. On the akaganeite crystal structure, phase transformations and possible role in post-excavational corrosion of iron artifacts10.1016/S0010-938X(03)00078-7 ↗
40. Energetics of stable and metastable low-temperature iron oxides and oxyhydroxides10.1016/S0016-7037(98)00208-7 ↗
41. Studies on the hydrolysis of metal ions. Part 57. The hydrolysis of the iron(III) ion and the solubility product of Fe(OH)0.7Cl0.3 in 0.5M (Na+)Cl− medium10.3891/acta.chem.scand.20-1376 ↗
42. R.M. Garrels, C.L. Christ, Equilibres des minéraux et de leurs solutions aqueuses, Gauthiers-Villars ed. Paris, 1967.
43. Corrosion des surconteneurs de déchets, cas d’un surconteneur en acier faiblement allié10.1051/jp4:2001127 ↗
44. Characterization of long-term corrosion of rebars embedded in concretes sampled on French historical buildings aged from 50 to 80 years10.1002/maco.200805019 ↗
45. R. Bertholon, La limite de la surface d’origine des objets métalliques archéologiques, Caractérisation, localisation et approche des mécanismes de conservation. Paris: Paris I, 2000.
46. On the influence of carbonate in mineral dissolution: II The solubility of FeCO3(s) at 25 C and 1 atm total pressure10.1016/0016-7037(92)90052-K ↗
47. Soluble iron sulphide species in natural waters: Reappraisal of their stoichiometry and stability constants10.1007/s000270050050 ↗
48. Electrochemical behaviour of ferrosilicides (FexSi) in neutral and alkaline aqueous electrolytes10.1149/1.2085750 ↗
49. D.D. Wagman, W.H. Evans, V.B. Parker, R.H. Schumm, I. Halow, S.M. Bailey, K.L. Churney, R.L. Nutall, The NBS tables of chemical thermodynamic properties. Selected values for inorganic and C1 and C2 organic substances in SI units, Journal of Physical Chemistry Ref Data 2 (1982) 11.