journal article·2008-09

Oxidation of single crystal PWA 1483 at 950°C in flowing air

A. Pfennig, B. Fedelich

Corrosion Science· Volume 50· Issue 9
Publisher page

Abstract

Abstract The oxidation behaviour of single crystal PWA 1483 at 950 °C was investigated by means of XRD, SEM and EDS. The parabolic oxidation behaviour, as defined by mass gain and the respective oxide layer thicknesses, is characterized by a parabolic rate constant of about 4 × 10−6 mg2/(cm4 × s) and the formation of a multi-layered oxide scale. An outer scale contains a Ti-bearing thin film composed of TiO2 and NiTiO3 but mostly Cr in Cr2O3 and (Ni/Co)Cr2O4 besides NiTaO4. This outer scale is connected to a discontinuous layer of Al2O3 and an area of γ′-depletion within the base material.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Catalytic Processes in Materials Science · Luminescence Properties of Advanced Materials · Advanced ceramic materials synthesis

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (25)

Show source-provided references
1. Evidence for internal oxidation during oxygen enhanced crack growth in P/M Ni-based superalloys10.1016/S1359-6462(02)00355-X ↗
2. Corrosion kinetics of a directionally solidified Ni-base superalloy10.1016/j.actamat.2007.01.034 ↗
3. Thermodynamic calculations for studying high temperature oxidation of superalloys10.1016/j.calphad.2003.12.002 ↗
4. Microstructure and morphology of high temperature oxidation in superalloys10.1016/S0921-5093(98)01181-2 ↗
5. Textures of alumina scales on FeCrAl alloys10.1016/S1359-6462(03)00403-2 ↗
6. Cyclic oxidation behavior of Ni- and Fe-based superalloys in air and Na2SO4-25% NaCl molten salt environment at 800°C
7. A. Akhtar, S. Hedge, R.C. Reed, The oxidation of single crystal nickel-base superallos, RedOrbit NEWS, http://wwwl.redorbit.com/modules/news/.
8. Oxidation of the single crystal Ni-base superalloy DD32 containing rhenium in air at 900°C and 1000°C10.1016/j.surfcoat.2004.06.003 ↗
9. Some water vapour effects during the oxidation of alloys that are α-Al2O3-formers
10. Oxidation behaviour of the directionally solidified Ni-base superalloy DS951 in air10.1007/s11085-005-8529-1 ↗
11. Improvement of high temperature oxidation and corrosion resistance of superalloy IN-738LC by pack cementation10.1016/j.surfcoat.2003.10.011 ↗
12. The oxidation of MAR M247 superalloy with Na2SO4 coating10.1016/S0254-0584(01)00527-2 ↗
13. Oxidation behaviour of the alloy IC-6 and protective coatings10.1016/S0010-938X(03)00184-7 ↗
14. The oxidation behaviour of the new nickel-based superalloy Inconel 740 with and without Na2SO4 deposit10.1016/j.surfcoat.2003.12.003 ↗
15. A comparative study of oxidation and hot corrosion of a cast nickel-base superalloy in different corrosive environments10.1016/S0167-577X(96)00109-7 ↗
16. Surface orientation dependent oxidation behaviour of aluminized DS CM 247 LC nickel-base superalloy10.1016/j.surfcoat.2003.09.066 ↗
17. Effect of sulphur on the cyclic oxidation behaviour of a single crystalline, nickel-base superalloy
18. POWDER CELL – a program for the representation and manipulation of crystal structures and calculation of the resulting X-ray powder patterns10.1107/S0021889895014920 ↗
19. S. Han, D.J. Young, Oxidation–Nitridation of Ni–Cr–Al alloys, Materials Research 7 No. 1 São Carlos (2004).10.1590/S1516-14392004000100003 ↗
20. Modelling of the partitioning and phase transformation temperatures of an as-cast third generation single crystal Ni-base superalloys10.1016/S0921-5093(01)01825-1 ↗
21. Interaction between oxidation and thermo mechanical fatigue in IN738 Superalloy – I10.1016/0956-716X(95)00004-F ↗
22. Development of a diffusion mobility database for Ni-base superalloys10.1016/S1359-6454(01)00383-4 ↗
23. Kofstad · 1988
24. Selective carbide oxidation and internal nitridationof the Ni-Base superalloys In 738 LC and IN 939 in air
25. Long-term oxidation of an as-cast Ni3Al alloy at 900°C and 1100°C10.1007/s11661-005-0049-8 ↗