Pourbaix diagrams for the nickel-water system extended to high-subcritical and low-supercritical conditions
Source abstract
Abstract
Abstract The supercritical water-cooled reactor (SCWR) is a Generation IV reactor concept that will operate at temperatures and pressures above water’s thermodynamic critical point. Pourbaix diagrams for the iron–water system at temperatures slightly below and above the critical point at 25 MPa have been constructed to aid the evaluation and development of potential construction materials. High temperature data extrapolation was performed using a revised Helgeson–Kirkham–Flowers model and fit to data on magnetite and hematite solubility in high-temperature water. A low-concentration diagram at 350 °C reveals the importance of water chemistry control to avoid transitioning to an active corrosion region.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Subcritical and Supercritical Water Processes · Chemical and Physical Properties in Aqueous Solutions · Crystallization and Solubility Studies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (26)
Show source-provided references
1. CANDU technology for Generation III+ and IV reactors10.1016/j.nucengdes.2006.04.020 ↗
2. Corrosion and stress corrosion cracking in supercritical water10.1016/j.jnucmat.2007.05.017 ↗
3. M. Yetisir, W. Diamond, L.K.H. Leung, D. Martin, R. Duffey, Conceptual mechanical design for a pressure-tube type supercritical water-cooled reactor, in: Proceedings of the 5th International Symposium on Supercritical-Water-Cooled Reactors, Vancouver, BC, 2011.
4. The solubility of nickel oxide and hydrolysis of Ni2+ in water to 573K10.1016/0021-9614(80)90182-2 ↗
5. Solubility and phase behavior of nickel oxide in aqueous sodium phosphate solutions at elevated temperatures10.1007/BF00647269 ↗
6. Solubility of nickel and cobalt oxides in high-temperature water10.13182/NSE92-36 ↗
7. Nickel(II) oxide solubility and phase stability in high temperature aqueous solutions10.1023/B:JOSL.0000048061.87789.81 ↗
8. Solubility measurements of crystalline NiO in aqueous solution as a function of temperature and pH10.1007/s10953-011-9670-x ↗
9. M.K. Edwards, Personal Communication (2010).
10. Revised Pourbaix diagrams for nickel at 25–300°C10.1016/S0010-938X(97)00002-4 ↗
11. Chemical thermodynamics consideration on corrosion products in supercritical-water-cooled reactor coolant10.13182/NT06-A3749 ↗
12. The ionization constant of water over wide ranges of temperature and density10.1063/1.1928231 ↗
13. IAPWS, Release on the Ionization Constant of H2O (2007).
14. Calculation of the thermodynamic and transport properties of aqueous species at high pressures and temperatures: correlation algorithms for ionic species and equation of state predictions to 5kb and 1000°C10.1016/0016-7037(88)90181-0 ↗
15. Calculation of the thermodynamic properties of aqueous species at high pressures and temperatures. effective electrostatic radii, dissociation constants and standard partial molal properties to 1000°C and 5 kbar10.1039/FT9928800803 ↗
16. E.H. Oelkers, H.C. Helgeson, E.L. Shock, D.A. Sverjensky, J.W. Johnson, V.A. Pokrovskii, Summary of the apparent partial molal Gibbs free energies of formation of aqueous species, minerals. and gases at pressures 1 to 5000 bars and temperatures 25 to 1000°C, J. Physical and Chemical Reference Data. 24 (1995) 1401–1561.10.1063/1.555976 ↗
17. Inorganic species in geologic fluids: correlations among standard molal thermodynamic properties of aqueous ions and hydroxide complexes10.1016/S0016-7037(96)00339-0 ↗
18. Predictive model for equilibrium constants of aqueous inorganic species at subcritical and supercritical conditions10.1021/ie010956y ↗
19. Thermodynamic properties for bunsenite, NiO, magnetite, Fe3O4, and hematite, Fe2O3, with comments on selected oxygen buffer reactions
20. P.R. Roberge, Handbook of corrosion engineering, McGraw-Hill, 2000.10.5006/C2000-00478 ↗
21. 2004
22. Understanding chemical conditions in supercritical water oxidation systems
23. Influence of oxide films on primary water stress corrosion cracking initiation of alloy 60010.1016/j.jnucmat.2005.10.002 ↗
24. R.W. Staehle, Critical analysis of “tight cracks”, in: Proceedings of the 13th International Conference on Environmental Degradation of Materials in Nuclear Power Systems, Whistler, BC, 2007.
25. Effect of irradiation on stress corrosion cracking in supercritical water10.1016/j.jnucmat.2007.05.008 ↗
26. IGSCC of grain boundary engineered 316L and 690 in supercritical water10.1016/j.jnucmat.2009.03.008 ↗