Influence of dissolved oxygen concentration on the oxide film formed on Alloy 690 in high temperature water
Source abstract
Abstract
Abstract Characteristics of the oxide films formed on Alloy 690 under different dissolved oxygen (DO) concentrations in 290 °C water were examined. Under 3 ppm DO, the oxide film mainly consisted of outer spinel particles and porous NiO base layer. A thin Cr-rich film gradually develops with decreasing DO. Fe and Ni levels in the film decrease while Cr level increases concomitantly. The film preformed under high DO changes slightly when further immersed under low DO. The film preformed under low DO becomes much thicker when immersed under high DO, with gradual development of spinel particles and NiO base layer.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: High-Temperature Coating Behaviors · Semiconductor materials and devices · Catalytic Processes in Materials Science
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (40)
Show source-provided references
1. P.M. Scott, P. Combrade, in: Corrosion in the Nuclear Power Industry, ASM Handbook, vol. 13C, ASM International, OH, 2006, pp. 362–385.
2. X-ray photoelectron studies of the aqueous oxidation of Inconel-600 Alloy10.1149/1.2129132 ↗
3. Analysis and TEM examination of corrosion scales grown on Alloy 690 exposed to pressurized water at 325°C10.1002/sia.1269 ↗
4. XPS study of oxides formed on nickel-base alloys in high-temperature and high-pressure water10.1002/sia.1282 ↗
5. Corrosion behavior of NiCrMo Alloy 625 in high temperature, hydrogenated water10.1016/S0010-938X(02)00230-5 ↗
6. XPS and STM study of the growth and structure of passive films in high temperature water on a nickel-base alloy10.1016/j.electacta.2004.04.032 ↗
7. Influence of oxide films on primary water stress corrosion cracking initiation of Alloy 60010.1016/j.jnucmat.2005.10.002 ↗
8. Corrosion behavior of NiCrFe Alloy 600 in high temperature, hydrogenated water10.1016/j.corsci.2005.01.006 ↗
9. A detailed TEM and SEM study of Ni-base alloys oxide scales formed in primary conditions of pressurized water reactor10.1016/j.jnucmat.2010.05.010 ↗
10. Influence of dissolved hydrogen on oxide film and PWSCC of Alloy 600 in PWR primary water10.1080/18811248.2003.9715330 ↗
11. Influence of dissolved hydrogen on structure of oxide film on Alloy 600 formed in primary water of pressurized water reactors10.1080/18811248.2003.9715385 ↗
12. Effect of hydrogen in Inconel Alloy 600 on corrosion in high temperature oxygenated water10.1016/j.corsci.2009.11.037 ↗
13. Effect of dissolved hydrogen on corrosion of Inconel Alloy 600 in high temperature hydrogenated water10.1016/j.electacta.2011.07.032 ↗
14. Effect of dissolved hydrogen on the electrochemical behavior of Alloy 600 in simulated PWR primary water at 290°C10.1016/j.corsci.2011.02.020 ↗
15. Effects of the solution temperature and the pH on the electrochemical properties of the surface oxide films formed on Alloy 60010.1016/j.corsci.2008.01.008 ↗
16. Influence of pH on electrochemical properties of passive films formed on Alloy 690 in high temperature aqueous environments10.1016/j.corsci.2009.08.002 ↗
17. Effects of temperature on the protective property, structure and composition of the oxide film on Alloy 62510.1016/j.corsci.2009.06.043 ↗
18. Electrochemical characterization of oxide film formed at high temperature on Alloy 69010.1016/j.nucengdes.2011.11.018 ↗
19. Effect of water chemistry on the oxide film on Alloy 690 during simulated hot functional testing of a pressurised water reactor10.1016/j.corsci.2012.01.002 ↗
20. Zinc treatment effects on corrosion behavior of Alloy 600 in high temperature, hydrogenated water10.1016/j.corsci.2005.11.002 ↗
21. Influence of Zn on oxide films on Alloy 690 in borated and lithiated high temperature water10.1016/j.corsci.2011.06.001 ↗
22. P. Schnongs, R. Lecocp, A. Minne, R. Wyckmans, E. Girasa, Primary chemistry as an action lever to reduce the source term. Review of the experience at Doel 3 and 4, in: Nuclear Plant Chemistry Conference, Quebec City, Canada, 2010.
23. S. Taunier, P. Varry, A. Tigeras, M. Bachet, L. Guinard, J.L. Bretelle, A. Rocher, New Primary Shutdown and Startup Chemistry Guidelines recently developed for EDF PWRs, in: International Conference on Water Chemistry of Nuclear Reactor Systems, Berlin, Germany, 2008.
24. I. Mailand, H. Venz, Shutdown Chemistry – an approved method to reduce dose rate, in: International Conference on Water Chemistry of Nuclear Reactor Systems, Berlin, Germany, 2008.
25. The mechanism of oxide film formation on Alloy 690 in oxygenated high temperature water10.1016/j.corsci.2011.07.038 ↗
26. Influence of dissolved oxygen on oxide films of Alloy 690TT with different surface status in simulated primary water10.1016/j.corsci.2011.07.012 ↗
27. Microstructural characteristics of the oxide scale formed on 304 stainless steel in oxygenated high temperature water10.1016/j.corsci.2010.07.015 ↗
28. The oxidation behavior of 304 stainless steel in oxygenated high temperature water10.1016/j.corsci.2010.09.001 ↗
29. Effect of nickel ion from autoclave material on oxidation behavior of 304 stainless steel in oxygenated high temperature water10.1016/j.corsci.2010.12.008 ↗
30. The corrosion of Alloy 690 in high-temperature aqueous media – thermodynamic considerations10.1016/S0022-3115(01)00468-8 ↗
31. In situ Raman spectroscopic investigation of chromium surfaces under hydrothermal conditions10.1016/S0169-4332(01)00338-5 ↗
32. Data quality, issues and guidelines for ECP measurement in high temperature water10.5006/1.3277589 ↗
33. Influence of dissolved oxygen concentration on the oxide film formed on 304 stainless steel in high temperature water10.1016/j.corsci.2012.06.007 ↗
34. Effect of alternately changing the dissolved Ni ion concentration on the oxidation of 304 stainless steel in oxygenated high temperature water10.1016/j.corsci.2011.04.016 ↗
35. Pourbaix diagrams for the ternary system of iron–chromium–nickel10.5006/1.3283945 ↗
36. General corrosion of materials under simulated BWR primary water conditions10.1080/18811248.1994.9735174 ↗
37. Characterization of the oxide film formed on type 316 stainless steel in 288°C water in cyclic normal and hydrogen water chemistries10.5006/1.3293562 ↗
38. Recent studies of pre-filming technique for light water reactor materials10.2320/matertrans1989.33.1004 ↗
39. J. Sarver, P. King, Oxidation behavior of austenitic materials exposed to secondary side water at 282°C, in: Proceedings of the 12th International Conference on Environmental Degradation of Materials in Nuclear Power System – Water Reactor, TMS, 2005, pp. 1317–1325.
40. A review of corrosion product transport and radiation field buildup in boiling water reactors10.1016/j.pnucene.2008.05.005 ↗