Significantly improved corrosion resistance of heat-treated Mg–Al–Gd alloy containing profuse needle-like precipitates within grains
Source abstract
Abstract
Abstract Microstructural evolution of a new Mg–Al–Gd alloy during heat treatment and its corrosion behavior in 1 wt.% NaCl solution were investigated by morphological observation, hydrogen evolution and electrochemical measurements. The microstructure of the as-cast alloy mainly consists of α-Mg, network-like Mg5Gd and polygonal Al2Gd phases, while a considerable part of Mg5Gd ones dissolve after T4 treatment. After T6 treatment, profuse micro-sized needle-like precipitates including crossed Mg5Gd-type and parallel Mg12ZnY-type ones appear and occupy different grains. These precipitates, resulting in homogeneous corrosion, continuous and compact oxidation film on the surface, have significantly improved the corrosion resistance of the Mg alloy.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Magnesium Alloys: Properties and Applications · Hydrogen Storage and Materials · Aluminum Alloys Composites Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (59)
Show source-provided references
1. Corrosion and characterisation of dual phase Mg–Li–Ca alloy in Hank’s solution: the influence of microstructural features10.1016/j.corsci.2013.10.028 ↗
2. Comparison of mechanical properties and microstructure of AZ91D alloy motorcycle wheels formed by die casting and double control forming10.1016/j.matdes.2012.04.029 ↗
3. Corrosion behavior of 3C magnesium alloys in simulated sweat solution10.1002/maco.200905510 ↗
4. Effect of long period stacking ordered (LPSO) structure on the damping capacities of Mg–Cu–Mn–Zn–Y alloys10.1016/j.jallcom.2012.05.003 ↗
5. Effects of zirconium and oxygen plasma ion implantation on the corrosion behavior of ZK60 Mg alloy in simulated body fluids10.1016/j.corsci.2013.11.044 ↗
6. Magnesium and its alloys as orthopedic biomaterials: a review10.1016/j.biomaterials.2005.10.003 ↗
7. The in vivo and in vitro corrosion of high-purity magnesium and magnesium alloys WZ21 and AZ9110.1016/j.corsci.2013.06.019 ↗
8. Neuropathology of aluminum toxicity in rats (glutamate and GABA impairment)10.1016/S1043-6618(02)00336-5 ↗
9. Effect of different Ti–6Al–4V surface treatments on osteoblasts behaviour10.1016/S0142-9612(01)00266-6 ↗
10. Differences in behavior among the chlorides of seven rare earth elements administered intravenously to rats10.1093/toxsci/37.2.106 ↗
11. Electrothermal atomic absorption spectrometric determination of Al, Cu, Fe, Pb, V and Zn in clinical samples and in certified environmental reference materials10.1016/0003-2670(94)80350-1 ↗
12. Research on an Mg–Zn alloy as a degradable biomaterial10.1016/j.actbio.2009.06.028 ↗
13. In vitro studies of biomedical magnesium alloys in a simulated physiological environment: a review10.1016/j.actbio.2010.12.004 ↗
14. A review of degradation properties of Mg based biodegradable implants
15. A biodegradable polymer-based coating to control the performance of magnesium alloy orthopaedic implants10.1016/j.biomaterials.2009.11.111 ↗
16. In vitro corrosion and biocompatibility of binary magnesium alloys10.1016/j.biomaterials.2008.10.021 ↗
17. Evaluation of short-term effects of rare earth and other elements used in magnesium alloys on primary cells and cell lines10.1016/j.actbio.2009.09.024 ↗
18. Magnesium alloys as implant materials – principles of property design for Mg–RE alloys10.1016/j.actbio.2009.09.010 ↗
19. Biocorrosion behavior and cytotoxicity of a Mg–Gd–Zn–Zr alloy with long period stacking ordered structure10.1016/j.matlet.2012.07.030 ↗
20. On the in vitro and in vivo degradation performance and biological response of new biodegradable Mg–Y–Zn alloys10.1016/j.actbio.2009.10.008 ↗
21. High temperature oxidation of AZ31+0.3wt.% Ca and AZ31+0.3wt.% CaO magnesium alloys10.1016/j.corsci.2013.01.036 ↗
22. Insights into microstructure based corrosion mechanism of high pressure die cast AM50 alloy10.1016/j.corsci.2012.04.016 ↗
23. Corrosion behavior of rapidly solidified Mg–Zn-rare earth element alloys in NaCl solution10.1016/j.corsci.2006.05.017 ↗
24. Influence of the β-phase morphology on the corrosion of the Mg alloy AZ9110.1016/j.corsci.2008.04.010 ↗
25. Microstructure, mechanical properties, biocorrosion behavior, and cytotoxicity of as-extruded Mg–Nd–Zn–Zr alloy with different extrusion ratios10.1016/j.jmbbm.2012.02.002 ↗
26. Corrosion behaviour of bulk ultra-fine grained AZ91D magnesium alloy fabricated by equal-channel angular pressing10.1016/j.corsci.2010.09.044 ↗
27. The role of second phases in the corrosion behavior of Mg–5Zn alloy10.1016/j.corsci.2012.03.030 ↗
28. Influence of hot rolling on the corrosion behavior of several Mg–X alloys10.1016/j.corsci.2014.10.012 ↗
29. Electrochemical behaviour and corrosion of Mg–Y alloys10.1016/j.corsci.2011.03.010 ↗
30. Corrosion of hot extrusion AZ91 magnesium alloy. Part II: Effect of rare earth element neodymium (Nd) on the corrosion behavior of extruded alloy10.1016/j.corsci.2011.05.035 ↗
31. The role of Mg17Al12 phase in the corrosion of Mg alloy AZ9110.5006/1.3585029 ↗
32. Effect of Mg17Al12 precipitate on corrosion behavior of AZ91D magnesium alloy10.4028/www.scientific.net/MSF.419-422.851 ↗
33. Effect of heat treatment on corrosion behaviour of magnesium alloy AZ91D in simulated body fluid10.1016/j.corsci.2009.11.030 ↗
34. Corrosion behavior of a friction stir processed rare-earth added magnesium alloy10.1016/j.corsci.2012.01.007 ↗
35. Homogeneous corrosion of high pressure torsion treated Mg–Zn–Ca alloy in simulated body fluid10.1016/j.matlet.2010.11.015 ↗
36. Improved corrosion resistance and cytocompatibility of magnesium alloy by two-stage cooling in thermal treatment10.1016/j.corsci.2012.03.020 ↗
37. Effect of extrusion parameters on mechanical properties of Mg97Zn1Y2 alloys at room and elevated temperatures10.2320/matertrans.MAW201026 ↗
38. Formation of 14H long period stacking ordered structure and profuse stacking faults in Mg–Zn–Gd alloys during isothermal aging at high temperature10.1016/j.actamat.2007.08.033 ↗
39. Strengthening and toughening mechanisms in Mg–Zn–Y alloy with a long period stacking ordered structure10.1016/j.actamat.2010.05.012 ↗
40. Elevated-temperature impact toughness of Mg–(Gd, Y)–Zr alloy10.1016/j.scriptamat.2013.02.031 ↗
41. Mg–Zn–Y alloys with long-period stacking ordered structure: in vitro assessments of biodegradation behavior10.1016/j.msec.2013.04.051 ↗
42. Degradation behavior of Mg-based biomaterials containing different long-period stacking ordered phases
43. Uniform corrosion behavior of GZ51K alloy with long period stacking ordered structure for biomedical application10.1016/j.corsci.2014.07.004 ↗
44. Enrichment of Gd and Al atoms in the quadruple close packed planes and their in-plane long-range ordering in the long period stacking-ordered phase in the Mg–Al–Gd system10.1016/j.actamat.2011.08.011 ↗
45. Corrosion performance and mechanical properties of sputter-deposited MgY and MgGd alloys10.1016/j.corsci.2013.08.027 ↗
46. Effect of grain size and twins on corrosion behaviour of AZ31B magnesium alloy10.1016/j.corsci.2009.10.018 ↗
47. An innovative specimen configuration for the study of Mg corrosion10.1016/j.corsci.2010.09.016 ↗
48. Validation of corrosion rates measured by the Tafel extrapolation method10.1016/j.corsci.2005.05.046 ↗
49. Influence of pH and chloride ion concentration on the corrosion of Mg alloy ZE4110.1016/j.corsci.2008.08.023 ↗
50. Electrochemical corrosion behavior of biodegradable Mg–Y–RE and Mg–Zn–Zr alloys in Ringer’s solution and simulated body fluid10.1016/j.corsci.2014.11.015 ↗
51. Solidification microstructure, thermal properties and hardness of magnesium alloy 20mass% Gd added AZ 91D10.2320/matertrans.F-M2009802 ↗
52. Comparison of microstructure in Mg–10Y–5Gd–0.5Zr and Mg–10Y–5Gd–2Zn–0.5Zr alloys by conventional casting10.1016/j.jallcom.2008.10.003 ↗
53. Formation of a lamellar 14H-type long period stacking ordered structure in an as-cast Mg–Gd–Zn–Zr alloy10.1007/s10853-008-3213-x ↗
54. Research on long-period-stacking-ordered phase in Mg–Zn–Dy–Zr alloy10.1016/j.jallcom.2012.12.165 ↗
55. GdMg5: a complex structure with a large cubic cell10.1107/S0108270186097019 ↗
56. Measurement of the corrosion rate of magnesium alloys using Tafel extrapolation10.1016/j.corsci.2009.10.016 ↗
57. Poisoning the corrosion of magnesium10.1016/j.elecom.2013.07.021 ↗
58. Corrosion of heat treated magnesium alloy ZE4110.1016/j.corsci.2011.06.005 ↗
59. Self-protection against corrosion of aged magnesium alloy in simulated physiological environment10.1016/j.corsci.2012.11.029 ↗