The role of TiN inclusions in stress corrosion crack initiation for Alloy 690TT in high-temperature and high-pressure water
Source abstract
Abstract
Microchemistry and microstructure of TiN in Alloy 690TT were analyzed using SEM and TEM. Constant loading test was conducted on Alloy 690TT in 325 degrees C water to study effect of TiN on SCC initiation. It was found that TiN-inclusion stringers existed along the longitudinal axis. Numerous micron-size TiN with Al(2)O(3) and/or MgO nuclei and submicron-size TiN existed in this alloy. After holding a constant load equal to 180% of the yield strength for 40 days, cracks about 1-3 mu m initiated at micron-size TiN and TiN-inclusion stringers in the near surface. The mechanisms of Alloy 690TT crack initiation at these TiN are discussed. (C) 2009 Elsevier Ltd. All rights reserved.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Metal and Thin Film Mechanics · Advanced ceramic materials synthesis · Corrosion Behavior and Inhibition
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (20)
Show source-provided references
1. Effect of heat treatment applied potential on the caustic stress corrosion cracking of inconel 60010.5006/1.3583025 ↗
2. Effect of heat treatment on the behavior of alloy 600 in lithiated water containing dissolved hydrogen at 25°C to 350°C10.5006/1.3585218 ↗
3. Effects of heat-treatment on the extent of chromium depletion and caustic corrosion resistance of alloy 69010.1016/j.corsci.2006.05.043 ↗
4. Cavitation erosion behavior of inconel 690 alloy10.1016/j.msea.2007.12.007 ↗
5. Microchemistry of Ti-carbonitrides and their role in the early stage of pit initiation of alloy 60010.5006/1.3280673 ↗
6. Characterization of microstructure and corrosion properties of cold worked alloy 80010.1016/j.corsci.2005.10.012 ↗
7. Microstructural aspects of the corrosion of alloy 80010.1016/j.corsci.2004.04.005 ↗
8. Initiation of pitting at sulfide inclusions in stainless steel10.1149/1.2401840 ↗
9. Effect of microalloy elements on corrosion resistance of high-chromium-containing ferritic stainless steels in chloride solutions10.5006/1.3290381 ↗
10. Corrosion behavior of austenitic alloy 690 under anodic and cathodic potentials10.1007/s11661-002-0067-8 ↗
11. Crack initiation mechanisms for low cycle fatigue of type 316Ti stainless steel in high temperature water10.1016/j.msea.2007.12.043 ↗
12. The role of titanium in the pitting corrosion of commercial stainless steels10.5006/1.3582048 ↗
13. Pitting and sulphide inclusions in steel10.1016/S0010-938X(74)80047-8 ↗
14. Effect of TiN inclusion on fracture toughness in ultrahigh strength steel10.2355/isijinternational.29.158 ↗
15. Calculation of the equilibrium shape of TiN particles in iron10.2355/isijinternational.44.1454 ↗
16. Influence of Ti, C and N concentration on the intergranular corrosion behaviour of AISI 316Ti and 321 stainless steels10.1016/j.actamat.2006.11.021 ↗
17. Proceedings of the International Conference on Physical Metallurgy of Thermomechanical Processing of Steels and Other Metals
18. Beck · 1971 · 644
19. Quantitative assessment of submodes of stress corrosion cracking on the secondary side of steam generator tubing in pressurized water reactors: part I10.5006/1.3277522 ↗
20. Effects of chemical compounds in the stress corrosion cracking of steam generator tubing materials in a caustic solution10.1016/j.jnucmat.2005.01.018 ↗