journal article·2004-01

Hydrogen permeation and corrosion behavior of high strength steel MCM 430 in cyclic wet–dry SO2 environment

Rokuro Nishimura, Daisuke Shiraishi, Yasuaki Maeda

Corrosion Science· Volume 46· Issue 1
Publisher page

Abstract

Abstract Hydrogen permeation caused by corrosion under a cyclic wet (2 h)–dry (10 h) SO 2 condition was investigated for a high strength steel of MCM 430 by using an electrochemical technique in addition to the corrosion behavior obtained from weight loss measurement and the determination of corrosion products by using X-ray diffraction method. The hydrogen content converted from hydrogen permeation current density was observed in both wet and dry periods. The origin of proton was estimated to be from (1) the hydrolysis of ferrous ions, (2) the oxidation of ferrous ions and ferrous hydroxide, and (3) hydrolysis of SO 2 and formation of FeSO 4 , but not from the dissociation of H 2 O. With respect to the determination of the corrosion products consisting of inner (adherent) and outer (not adherent) layers, the outer layer is composed of α-FeOOH, amorphous phase and γ-FeOOH, where α-FeOOH increases with the increase in the wet–dry cycle, and amorphous phase shows the reverse trend. The corrosion product in the inner layer is mainly Fe 3 O 4 with them. On the basis of the results obtained, the role of the dry or wet period, the effect of SO 2 and the corrosion process during the cyclic wet–dry periods were discussed.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Corrosion Behavior and Inhibition · Hydrogen embrittlement and corrosion behaviors in metals · Concrete Corrosion and Durability

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (22)

Show source-provided references
1. Johnson · Appl. Mater. Res. · 1965 · 4 · 34
2. Marsh · 1992 · 63
3. Graedel · J. Electrochem. Soc. · 1990 · 137 · 238510.1149/1.2086948 ↗
4. Stratmann · Corros. Sci. · 1990 · 30 · 68110.1016/0010-938X(90)90032-Z ↗
5. Yoshizawa · Boshoku Gijutsu (Corros. Eng.) · 1975 · 24 · 365
6. Lukovtsev · Electrochem. Acta · 1962 · 6 · 1710.1016/0013-4686(62)87020-0 ↗
7. Takehara · Electrochem. Acta · 1971 · 16 · 83310.1016/0013-4686(71)85050-8 ↗
8. Devanathan · Proc. Roy. Soc. London A · 1962 · 270 · 9010.1098/rspa.1962.0205 ↗
9. McBreen · J. Electrochem. Soc. · 1966 · 113 · 121810.1149/1.3087209 ↗
10. Nanis · J. Electrochem. Soc. · 1972 · 119 · 69110.1149/1.2404296 ↗
11. Misawa · Corros. Sci. · 1974 · 14 · 27910.1016/S0010-938X(74)80037-5 ↗
12. Suzuki · J. Electrochem. Soc. · 1980 · 127 · 221010.1149/1.2129376 ↗
13. Townsend · 1982 · 45
14. Atmospheric Degradation and Corrosion Control
15. Barton · Werkst. Korros. · 1970 · 21 · 2510.1002/maco.19700210106 ↗
16. Schikorr · Werkst. Korros. · 1963 · 14 · 6910.1002/maco.19630140203 ↗
17. K.A. Chandler, J.E. Stanners, in: Proc. 2nd Intl. Congr. Met. Corr., NACE, 1963, p. 32510.1016/0042-6822(63)90206-X ↗
18. Schwarz · Werkst. Korros. · 1965 · 16 · 20810.1002/maco.19650160306 ↗
19. Ross · Corros. Sci. · 1966 · 6 · 33710.1016/S0010-938X(66)80040-9 ↗
20. Evans · Nature, London · 1965 · 206 · 98010.1038/206980a0 ↗
21. Stratmann · Corros. Sci. · 1987 · 27 · 90510.1016/0010-938X(87)90058-8 ↗
22. Wo · Prot. Metals · 1982 · 20 · 62