Oxidation of Fe–10Cr in O2 and in O2+H2O environment at 600°C: A microstructural investigation
Source abstract
Abstract
Oxidation of Fe-10Cr in dry and wet O-2 was studied at 600 degrees C for up to 168 h. Oxide microstructure was investigated by STEM/EDX, FIB/SEM and TEM. Oxidation in dry O-2 gives a Cr-rich protective (Fe1-xCrx)(2)O-3 scale. The same protective oxide initially forms in O-2 + H2O environment, but after an incubation period scale breakdown is triggered by CrO2(OH)(2) evaporation that depletes the substrate in Cr and converts (Fe1-xCrx)(2)O-3 to FeCr spinel oxide. Internal oxidation occurs after breakaway. Alternating external and internal oxidation result in the inward-growing scale showing a characteristic banded morphology.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: High-Temperature Coating Behaviors · Nuclear Materials and Properties · Advanced materials and composites
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (30)
Show source-provided references
1. Kofstad · 1988
2. Birks · 2006
3. D. Young, High Temperature Oxidation and Corrosion of Metals, In: Burnstein (Ed.), Elsevier corrosion series, first ed., Oxford, UK, 2008.
4. The oxidation behaviour of metals and alloys at high temperatures in atmospheres containing water vapour: a review10.1016/j.pmatsci.2007.11.001 ↗
5. Effect of water vapor on high-temperature oxidation of FeCr alloys10.1007/s11837-009-0102-y ↗
6. The mechanism of the high-temperature oxidation of iron–chromium alloys in water vapor10.1149/1.2425963 ↗
7. Enhanced oxidation of the 9%Cr steel P91 in water vapour containing environments10.1016/j.corsci.2006.02.002 ↗
8. Oxidation of iron at 400–600°C in dry and wet O210.1016/j.corsci.2010.01.002 ↗
9. The influence of H2O on iron oxidation at 600°C: a microstructural study10.4028/www.scientific.net/MSF.595-598.1005 ↗
10. An ESEM in situ investigation of the influence of H2O on iron oxidation at 500°C10.1016/j.corsci.2009.05.016 ↗
11. Oxidation of binary FeCr alloys (Fe–2.25Cr, Fe–10Cr, Fe–18Cr and Fe–25Cr) in O2 and in O2+H2O environment at 600°C10.1007/s11085-010-9229-z ↗
12. Theoretical and experimental investigation of the thermochemistry of CrO2(OH)2(g)10.1021/jp0647380 ↗
13. Paralinear oxidation of chromium in O2+H2O environment at 600–700°C10.1007/s11085-008-9114-1 ↗
14. Effect of oxide volatilization on oxidation kinetics of Cr and Fe–Cr alloys10.1149/1.2424115 ↗
15. Influence of water vapor and flow rate on the high-temperature oxidation of 304L; effect of chromium oxide hydroxide evaporation10.1023/A:1004642310974 ↗
16. Evidence for chromium evaporation influencing the oxidation of 304L: the effect of temperature and flowrate10.1023/A:1014877600235 ↗
17. Enhanced internal oxidation as reason for breakdown of protective chromia scales on FeCr-alloys in water vapour containing gases10.4028/www.scientific.net/MSF.595-598.699 ↗
18. Hydrogen in chromium: influence on the high-temperature oxidation kinetics in H2O, oxide-growth mechanisms, and scale adherence10.1023/A:1004610626903 ↗
19. The kinetic behaviour of metals in water vapour at high temperatures: can general rules be proposed?
20. Temperature dependence of oxide scale formation on high-Cr ferritic steels in Ar–H(2)–H(2)O10.1016/j.corsci.2011.02.031 ↗
21. Microstructure investigation of protective and non-protective oxides on 11% chromium steel10.1007/s11085-006-9035-9 ↗
22. Concentration profiles in the underlying alloy during the oxidation of iron–chromium alloys10.1016/0001-6160(67)90066-1 ↗
23. Point-defects and cation tracer diffusion in (CrxFe1–x)(3-delta)O-4 spinels10.1016/0167-2738(95)00190-H ↗
24. Void formation in magnetite scale formed on iron at 823K – elucidation by chemical potential distribution
25. Study of the high-temperature oxidation behaviour of Ti and Ti4Nb with SNMS using tracers10.1002/(SICI)1096-9918(200005)29:5<321::AID-SIA872>3.0.CO;2-Q ↗
26. Low temperature oxidation of pure iron: growth kinetics and scale morphologies
27. Microstructural investigation of the breakdown of the protective oxide scale on a 304 steel in the presence of oxygen and water vapour at 600°C10.1016/j.corsci.2005.08.012 ↗
28. Oxidation of 310 steel in H2O/O2 mixtures at 600°C, the effect of water vapour – enhanced chromium evaporation10.1016/S0010-938X(02)00056-2 ↗
29. Investigation of FIB-thinned TEM cross-sections of oxide scales formed on type 310 steel at 600°C in water vapour-containing oxygen atmospheres10.3184/096034007X207636 ↗
30. Microstructural investigation of the effect of water vapour on the oxidation of alloy 353 MA in oxygen at 700 and 900°C10.1179/mht.2005.027 ↗