Open circuit potentials of metallic chromium and austenitic 304 stainless steel in aqueous sulphuric acid solution and the influence of chloride ions on them
Source abstract
Abstract
Abstract Open circuit potential measurements and cyclic voltammetry of chromium and 304 stainless steel in deaerated aqueous H 2 SO 4 solution of pH 1, without and containing NaCl in the concentration range 1–4 M revealed that chromium exhibits two stable open circuit potentials both having the character of a Wagner–Traud corrosion potential. One, E corr.1 , was established on the passive surface formed by previously exposing Cr to air or by potentiostatic passivation in a controlled manner, and the second one, E corr.2 , at the bare Cr surface obtained by prolonged cathodic activation. There was a small difference in the E corr.1 values depending on the properties of the passive layer. Addition of NaCl accelerates to some extent, the hydrogen evolution reaction on the passive surface, while the same reaction on the bare surface was somewhat inhibited by NaCl. On the other hand, presence of NaCl accelerates the anodic reaction on the bare surface, and it activates the dissolution of the passive layer so that the passivation currents increase with addition of NaCl. This effect is so large that at concentrations of NaCl larger than 3 M, the destruction of the passive layer was so fast that in a matter of seconds the Cr is activated, and the only stable corrosion potential observed was E corr.2 . No pitting of Cr in the presence of NaCl was observed up to the transpassive potentials. 304 stainless steel could not be activated in sulphuric acid solution, and its open circuit potential, unlike the corrosion potential of the 400 types of stainless steel, was established by the hydrogen evolution reaction on the passive steel surface. The small anodic peak often observed on 304 stainless steel if the metal had been cathodically pre-treated is a pseudo-peak due to the anodic oxidation of hydrogen absorbed inside the metal. This finding should be elaborated more in recommendations (e.g. ASTM standards) for the application of electrochemical corrosion rate measurement to 304 stainless steel corrosion. Addition of NaCl activates the anodic dissolution of steel with the current of the passivation peak being proportional to the NaCl concentration. Unlike chromium, austenitic 304 stainless steel achieves only one corrosion potential in sulphuric acid, both in the presence and absence of NaCl, with the value of ca. −0.200 to −0.350 V (SCE) in the absence and −0.450 V (SCE) in the presence of NaCl, when steel corrodes as the active metal.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Corrosion Behavior and Inhibition · Hydrogen embrittlement and corrosion behaviors in metals · Concrete Corrosion and Durability
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (46)
Show source-provided references
1. Wagner · Z. Elektrochem. · 1938 · 44 · 391
2. ASM Handbook, vol. 13b, Corrosion: Materials, ASM International, Materials Park OH, USA, 2005, p. 68.
3. Kolotyrkin · Z. Elektrochem. · 1958 · 62 · 664
4. Heumann · Ber. Bunsenges. Phys. Chem. · 1963 · 63 · 67110.1002/bbpc.19630670711 ↗
5. Wilde · Electrochim. Acta · 1969 · 14 · 61910.1016/0013-4686(69)87044-1 ↗
6. Okuyama · Electrochim. Acta · 1985 · 30 · 75710.1016/0013-4686(85)80124-9 ↗
7. El-Basiouni · Corros. Sci. · 1977 · 17 · 40510.1016/0010-938X(77)90030-0 ↗
8. Shcherbakova · Dokladi AN USSR · 1981 · 258 · 957
9. Shcherbakova · Dokladi AN USSR · 1983 · 273 · 663
10. Chai · Zashchita Metallov · 1993 · 29 · 324
11. Cheng · Corros. Sci. · 1999 · 41 · 77310.1016/S0010-938X(98)00150-4 ↗
12. Dražić · Corrosion · 2004 · 60 · 29710.5006/1.3287734 ↗
13. Popić · Electrochim. Acta · 2004 · 49 · 4877
14. Andreeva · Zh. fiz. khim. · 1964 · 38 · 1825
15. Revez · 1973 · 137
16. Okomoto · Corros. Sci. · 1973 · 19 · 47110.1016/0010-938X(73)90031-0 ↗
17. Bouyssoux · J. Elactroanal. Spectrosc. · 1977 · 11 · 18510.1016/0368-2048(77)85109-8 ↗
18. Sukhotin · Elektrokhimiya · 1977 · 13 · 296
19. Sukhotin · Elektrokhimiya · 1982 · 18 · 132
20. N. Sato, in Ref. [15, p. 29].
21. Sunseri · J. Electrochem. Soc. · 1990 · 137 · 241110.1149/1.2086952 ↗
22. Moffat · J. Electrochem. Soc. · 1992 · 139 · 186910.1149/1.2069514 ↗
23. Maurice · J. Elactrochem. Soc. · 1996 · 143 · 118210.1149/1.1836616 ↗
24. Bastidas · Corros. Sci. · 1998 · 40 · 43110.1016/S0010-938X(97)00149-2 ↗
25. Bera · Corros. Sci. · 2000 · 42 · 120910.1016/S0010-938X(00)00028-7 ↗
26. Olefjord · Corros. Sci. · 1975 · 15 · 69710.1016/0010-938X(75)90034-7 ↗
27. Olefjord · Zashchita Metallov · 1984 · 20 · 515
28. C.R. Clayton, I. Olefjord, in: P. Marcus (Ed.), Corrosion Mechanisms in Theory and Practice, second ed., Marcel Dekker Inc., New York, 2992, p. 277.
29. Yang · Corros. Sci. · 1999 · 41 · 74110.1016/S0010-938X(98)00147-4 ↗
30. Engell · Z. Phys. Chem. · 1960 · 215 · 17610.1515/zpch-1960-0117 ↗
31. Wilde · Corrosion · 1969 · 25 · 30010.5006/0010-9312-25.7.300 ↗
32. Green · Corrosion · 1970 · 26 · 534
33. Bockris · Electrochim. Acta · 1961 · 4 · 32510.1016/0013-4686(61)80026-1 ↗
34. Sato · J. Electrochem. Soc. · 1963 · 110 · 70310.1149/1.2425838 ↗
35. Jegdić · J. Serb. Chem. Soc. · 2006 · 71 · 118710.2298/JSC0611187J ↗
36. Dražić · J. Serb. Chem. Soc. · 2004 · 69 · 106510.2298/JSC0412099D ↗
37. Vračar · J. Electroanal. Chem. · 1992 · 339 · 26910.1016/0022-0728(92)80457-F ↗
38. Dražić · J. Serb. Chem. Soc. · 1987 · 52 · 711
39. Ho · Elektrokhimiya · 1968 · 4 · 990
40. A. N. Frumkin, Potenciali nulevogo zaryada (Zero Charge Potentials), Nauka, Moskva, 1979, p. 248, Figs. 9–11.
41. Lee · Electrochim. Acta · 2005 · 50 · 177710.1016/j.electacta.2004.08.046 ↗
42. Seys · Corrosion · 1974 · 30 · 4710.5006/0010-9312-30.2.47 ↗
43. ASTM G 5-94 Standard Reference Test Method for Making Potentiostatic and Potentiodynamic Anodic Polarization Measurements (Reproved 1999).
44. ASM Handbook, vol. 13a, Corrosion: Fundamentals, Testing and Protection, ASM International, Materials Park, OH, USA, 2003, p. 458.
45. Z. Misirlioğlu, S. Uneri, M.L. Aksu, .
46. Mansfeld · Corros. Sci. · 1976 · 36 · 65310.1016/S0010-938X(76)80025-X ↗