Influence of phase dissolution and hydrogen absorption on the stress corrosion cracking behavior of Mg-7%Gd-5%Y-1%Nd-0.5%Zr alloy in 3.5 wt.% NaCl solution
Source abstract
Abstract
Abstract Through investigating the influence of phase dissolution and hydrogen on the stress corrosion cracking (SCC) behavior of an as-cast Mg-7%Gd-5%Y-1%Nd-0.5%Zr alloy in 3.5 wt.% NaCl solution, it revealed that the proposed T4 treatment can improve the SCC resistance. Based on the microstructural analysis, such improvement was mainly ascribed to the complete dissolution of coarse eutectic pockets. Further analysis indicated that the SCC mechanism was associated with hydrogen embrittlement (HE). Through dissolving the eutectic pockets and alleviating the corrosion attack of Mg matrix, the influence of HE on SCC resistance of T4 samples can be weakened.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Magnesium Alloys: Properties and Applications · Corrosion Behavior and Inhibition · Metal and Thin Film Mechanics
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (81)
Show source-provided references
1. Corrosion processes of Mg-Y-Nd-Zr alloys in Na2SO4 electrolyte10.1016/j.corsci.2013.03.036 ↗
2. Combined influence of Be and Ca on improving the high-temperature oxidation resistance of the magnesium alloy Mg-9Al-1Zn10.1016/j.corsci.2017.03.023 ↗
3. Microstructure and corrosion resistance of directionally solidified Mg-2wt.% Zn alloy10.1016/j.corsci.2017.02.023 ↗
4. Corrosion and passivation of magnesium alloys10.1016/j.corsci.2016.05.041 ↗
5. Effect of heat treatment on corrosion behavior of AZ63 magnesium alloy in 3.5 wt.% sodium chloride solution10.1016/j.corsci.2016.05.019 ↗
6. Corrosion resistance of dicalcium phosphate dihydrate/poly(lactic-co-glycolic acid) hybrid coating on AZ31 magnesium alloy10.1016/j.corsci.2015.10.010 ↗
7. Characterisation of stress corrosion cracking (SCC) of Mg-Al alloys10.1016/j.msea.2007.11.064 ↗
8. Intergranular stress corrosion crack propagation in hot-rolled AZ31 Mg alloy sheet10.1016/j.msea.2014.02.077 ↗
9. Stress corrosion cracking of several hot-rolled binary Mg–X alloys10.1016/j.corsci.2015.04.023 ↗
10. Stress corrosion cracking of several solution heat-treated Mg-X alloys10.1016/j.corsci.2015.04.010 ↗
11. Corrosion and electrochemical behavior of as-cast Mg-5Y-7Gd-1Nd-0.5Zr magnesium alloys in 5% NaCl aqueous solution10.1016/S1002-0071(12)60063-X ↗
12. Comparative study on corrosion behavior of as-cast and extruded Mg-5Y-7Gd-1Nd-0.5Zr alloy in 5% NaCl aqueous solution10.1016/S1003-6326(11)61278-8 ↗
13. Stress corrosion cracking susceptibility of a high strength Mg-7% Gd-5% Y-1% Nd-0.5% Zr alloy10.1016/j.jma.2014.11.004 ↗
14. Corrosion mechanisms of magnesium alloys10.1002/(SICI)1527-2648(199909)1:1<11::AID-ADEM11>3.0.CO;2-N ↗
15. Understanding magnesium Corrosion-A framework for improved alloy performance10.1002/adem.200310405 ↗
16. ESEM observation of the process of hydrogen generation around the micro-droplets forming on AZ91 magnesium alloy10.1016/j.elecom.2008.01.027 ↗
17. The behaviour of magnesium during free corrosion and potentiodynamic polarization investigated by real-time hydrogen measurement and optical imaging10.1016/j.electacta.2013.12.109 ↗
18. A critical review of the stress corrosion cracking (SCC) of magnesium alloys10.1002/adem.200500071 ↗
19. Mechanical integrity of magnesium alloys for biomedical applications
20. Pitting-induced hydrogen embrittlement of magnesium-aluminium alloy10.1016/j.matdes.2012.06.007 ↗
21. Hydrogen embrittlement of magnesium and magnesium alloys: a review10.1149/2.023304jes ↗
22. Effects of hydrogen on pitting susceptibility of type 310 stainless steel10.5006/1.3287639 ↗
23. Effects of hydrogen on semiconductivity of passive films and corrosion behavior of 310 stainless steel10.1149/1.1391899 ↗
24. Improving corrosion resistance of magnesium-based alloys by surface modification with hydrogen by electrochemical ion reduction (EIR) and by plasma immersion ion implantation (PIII)10.1016/j.corsci.2004.06.027 ↗
25. Effect of hydrogen on the corrosion behavior of the Mg-xZn alloys10.1016/j.jma.2014.10.002 ↗
26. Effects of hydrogen on the corrosion of pure magnesium10.1016/j.electacta.2006.07.046 ↗
27. Roles of β phase in the corrosion process of AZ91D magnesium alloy10.1016/j.corsci.2005.05.011 ↗
28. States and transport of hydrogen in the corrosion process of an AZ91 magnesium alloy in aqueous solution10.1016/j.corsci.2008.01.028 ↗
29. Effect of hydrogen on stress corrosion cracking of magnesium alloy in 0.1 M Na2SO4 solution10.1016/j.msea.2007.11.035 ↗
30. Effect of corrosion attack on the fatigue behavior of an as-cast Mg-7%Gd-5%Y-1%Nd-0.5%Zr alloy10.1016/j.matdes.2015.06.109 ↗
31. Stress corrosion cracking of rare-earth containing magnesium alloys ZE41, QE22 and Elektron 21 (EV31A) compared with AZ8010.1016/j.msea.2007.07.070 ↗
32. Effect of heat treatment on the corrosion resistance and mechanical properties of an as-forged Mg-Zn-Y-Zr alloy10.1016/j.corsci.2014.12.008 ↗
33. Effects of heat treatment on corrosion behaviors of Mg-3Zn magnesium alloy10.1016/S1003-6326(09)60302-2 ↗
34. Initial stages of corrosion within Mg-Zn-Y-Zr alloy in 1 g/l NaCl solution10.1023/A:1004734725783 ↗
35. Effect of solution treatment on stress corrosion cracking behavior of an as-forged Mg-Zn-Y-Zr alloy10.1038/srep29471 ↗
36. Corrosion characterization of Mg-8Li alloy in NaCl solution10.1016/j.corsci.2009.03.011 ↗
37. Corrosion behaviour in salt spray and in 3.5% NaCl solution saturated with Mg(OH)(2) of as-cast and solution heat-treated binary Mg-X alloys: x = Mn, Sn, Ca, Zn, Al, Zr, Si, Sr10.1016/j.corsci.2013.06.030 ↗
38. Effect of volume fraction of LPSO phases on corrosion and mechanical properties of Mg-Zn-Y alloys10.1016/j.matdes.2017.02.078 ↗
39. Formation of hydrogen blister on AZ91 magnesium alloy during cathodic charging10.1016/j.corsci.2009.02.020 ↗
40. Microstructure and mechanical properties of high performance Mg-Gd based alloys10.1016/j.matdes.2008.04.069 ↗
41. Susceptibility of rare-earth-magnesium alloys to micro-galvanic corrosion10.1016/j.corsci.2010.08.006 ↗
42. Corrosion of magnesium alloy ZE41 - the role of microstructural features10.1016/j.corsci.2008.11.005 ↗
43. Electrochemical corrosion and mechanical behaviors of the charged magnesium10.1016/j.msea.2008.04.012 ↗
44. Influence of microstructure on the corrosion of diecast AZ91D10.1016/S0010-938X(98)00121-8 ↗
45. Influence of pH and chloride ion concentration on the corrosion of Mg alloy ZE4110.1016/j.corsci.2008.08.023 ↗
46. Zhang · 2002
47. Analysis of the electrochemical reaction behavior of alloy AZ91 by EIS technique in H3PO4/KOH buffered K2SO4 solutions10.1016/j.corsci.2006.10.016 ↗
48. Study of the corrosion mechanism of the in situ grown Mg-Al-CO32− hydrotalcite film on AZ31 alloy10.1016/j.corsci.2012.08.026 ↗
49. Corrosion behaviour of stressed magnesium alloys10.1016/S0010-938X(01)00101-9 ↗
50. The analysis of electrode impedances complicated by the presence of a constant phase element10.1016/S0022-0728(84)80324-1 ↗
51. The nitrate reduction process: a way for increasing interfacial pH
52. Orazem · 2017
53. Simultaneous EIS and in situ microscope observation on a partially blocked electrode application to scale electrodeposition10.1016/j.electacta.2005.02.117 ↗
54. Structural and electrochemical characterization of Zr-C-N-Ag coatings deposited by DC dual magnetron sputtering10.1016/j.corsci.2013.11.036 ↗
55. Electrocatalytic reduction of NO3− on palladium/copper electrodes10.1016/S1381-1169(99)00375-1 ↗
56. Stress-corrosion cracking susceptibility of AZ31 alloy after varied heat-treatment in 3.5 wt.% NaCl solution10.3139/146.110394 ↗
57. Corrosion behaviour of AZ21, AZ501 and AZ91 in sodium chloride10.1016/S0010-938X(98)00078-X ↗
58. Evaluation of microstructural effects on corrosion behaviour of AZ91D magnesium alloy10.1016/S0010-938X(99)00143-2 ↗
59. Influence of the beta-phase morphology on the corrosion of the Mg alloy AZ9110.1016/j.corsci.2008.04.010 ↗
60. Volta Potentials Measured by Scanning Kelvin Probe Force Microscopy as Relevant to Corrosion of Magnesium Alloys10.5006/1432 ↗
61. The special role of anodic second phases in the micro-galvanic corrosion of EW75 Mg alloy10.1016/j.electacta.2015.12.075 ↗
62. Volta potential of second phase particles in extruded AZ80 magnesium alloy10.1016/j.electacta.2005.10.010 ↗
63. Microstructure and microgalvanic corrosion of an extruded Mg-10Gd-2Y-0.5Zr magnesium alloy
64. Influence of microstructure and composition on the corrosion behaviour of Mg/Al alloys in chloride media10.1016/j.electacta.2008.06.001 ↗
65. The influence of microstructure on the corrosion behaviour of AZ91D studied by scanning Kelvin probe force microscopy and scanning Kelvin probe10.1016/j.corsci.2005.05.008 ↗
66. Grain character influences on corrosion of ECAPed pure magnesium10.1179/147842209X12559428167805 ↗
67. The influence of yttrium (Y) on the corrosion of Mg-Y binary alloys10.1016/j.corsci.2010.07.019 ↗
68. Investigation of the corrosion for Mg-xGd-3Y-0.4Zr (x=6,8,10,12 wt%) alloys in a peak-aged condition10.1016/j.corsci.2007.06.003 ↗
69. Corrosion behavior of rapidly solidified Mg-Nd and Mg-Y alloys10.1016/0025-5416(88)90386-2 ↗
70. Pourbaix · 1963
71. Review of recent developments in the field of magnesium corrosion10.1002/adem.201400434 ↗
72. Stress corrosion cracking and hydrogen diffusion in magnesium10.1002/adem.200600050 ↗
73. Investigation of stress corrosion cracking in magnesium alloys10.4028/www.scientific.net/SSP.211.89 ↗
74. A study on magnesium corrosion by real-time imaging and electrochemical methods: relationship between local processes and hydrogen evolution10.1016/j.electacta.2016.03.043 ↗
75. The localised corrosion of Mg alloy AZ31 in chloride containing electrolyte studied by a scanning vibrating electrode technique10.1016/j.electacta.2013.07.134 ↗
76. Hydrogen induced delayed plasticity and cracking10.1016/0036-9748(79)90204-7 ↗
77. Hydrogen interactions with defects in crystalline solids10.1103/RevModPhys.64.559 ↗
78. Stress corrosion cracking and liquid metal embrittlement in pure magnesium10.5006/1.3583907 ↗
79. On the fractography of transgranular stress corrosion failures in a Mg-Al alloy10.5006/0010-9312-31.7.247 ↗
80. Hydrogen embrittlement phenomena and mechanisms10.1515/corrrev-2012-0502 ↗
81. Fracture toughness and hydrogen-assisted crack growth in engineering alloys10.1002/9781118803363.ch36 ↗