Effect of dissolved hydrogen on the corrosion behavior of chemically vapor deposited SiC in a simulated pressurized water reactor environment

Daejong Kim, Hyeon-Geun Lee, Ji Yeon Park, Jeong-Yong Park, Weon-Ju Kim

Corrosion Science· Volume 98
Publisher page

Abstract

Abstract The corrosion behavior of chemically vapor deposited SiC was investigated in relation to its application as fuel cladding in a pressurized water reactor (PWR). Corrosion tests were conducted in deoxygenated, pressurized water at 360 °C with control of dissolved hydrogen. The dissolved hydrogen dramatically reduced the corrosion rate of SiC compared with that in water without the dissolved hydrogen. It was revealed that the dissolution of the surface oxide of SiC primarily contributed to the weight loss at the initial stage of corrosion. Further weight loss was minimal for 210 d because dissolved hydrogen effectively retarded the formation of SiO2.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced ceramic materials synthesis · High-Temperature Coating Behaviors · Nuclear Materials and Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (33)

Show source-provided references
1. Properties and applications of silicon carbide ceramics
2. Design, preparation and properties of non-oxide CMCs for application in engines and nuclear reactors: an overview10.1016/S0266-3538(03)00230-6 ↗
3. Preparation and oxidation protection of CVD SiC/a-BC/SiC coating for 3D C/SiC composite10.1016/j.corsci.2009.01.026 ↗
4. Resistance to oxidation and ablation of SiC coating on graphite prepared by chemical vapor reaction10.1016/j.corsci.2013.05.009 ↗
5. Coated particle fuel for high temperature gas cooled reactors10.5516/NET.2007.39.5.603 ↗
6. Research and development of HTTR coated particle fuel10.1080/18811248.1991.9731396 ↗
7. Compatibility of CVD SiC and SiCf/SiC composites with high temperature helium simulating very high temperature gas-cooled reactor coolant chemistry10.1007/s11085-012-9346-y ↗
8. Handbook of SiC properties for fuel performance modeling10.1016/j.jnucmat.2007.05.016 ↗
9. Stability of SiC and its composites at high neutron fluence10.1016/j.jnucmat.2010.12.088 ↗
10. Chemical degradation of SiC/SiC composite for the cladding of gas-cooled fast reactor in case of severe accident scenarios10.1016/j.corsci.2012.02.019 ↗
11. Youinou · 2013
12. Clad in clay
13. Mechanical strength of CTP triplex SiC fuel clad tubes after irradiation in MIT research reactor under PWR coolant conditions10.1002/9780470584002.ch4 ↗
14. Fabrication and material issues for the application of SiC composites to LWR fuel cladding10.5516/NET.07.2012.084 ↗
15. Oxidation of fuel cladding candidate materials in steam environments at high temperature and pressure10.1016/j.jnucmat.2012.05.007 ↗
16. Recession of silicon carbide in steam under nuclear plant LOCA conditions up to 1400°C
17. Silicon carbide oxidation in steam up to 2MPa10.1111/jace.13094 ↗
18. Radiation effects in SiC for nuclear structural applications10.1016/j.cossms.2012.03.005 ↗
19. Accident tolerant fuels for LWRs: a perspective10.1016/j.jnucmat.2013.12.005 ↗
20. Barrett · 2012
21. Oxidation behavior of silicon carbide at 1200°C in both air and water-vapor-rich environments10.1016/j.corsci.2014.07.052 ↗
22. Oxidation behavior of Hi-Nicalon SiC monofilament fibers in air and O2H2OAr atmospheres10.1016/j.corsci.2011.12.019 ↗
23. Corrosion behavior of silicon carbide in 290°C water10.1111/j.1151-2916.1989.tb06029.x ↗
24. Corrosion behavior of reaction-bonded silicon carbide ceramics in high-temperature water10.1023/A:1015797324658 ↗
25. Corrosion behaviors of sintered and chemically vapor deposited silicon carbide ceramics in water at 360°C10.1023/A:1023390111074 ↗
26. Effect of microstructure on the corrosion of CVD-SiC exposed to supercritical water10.1016/j.jnucmat.2009.08.008 ↗
27. Long-term corrosion behavior of CVD SiC in 360°C water and 400°C10.1016/j.jnucmat.2013.07.058 ↗
28. Pitting corrosion in CVD SiC at 300°C in deoxygenated high-purity water10.1016/j.jnucmat.2008.03.025 ↗
29. Ahluwalia · 2007
30. Hot water corrosion at ion-irradiated surface of SiC
31. EBSD investigation of SiC for HTR fuel particles10.1016/j.jnucmat.2006.01.010 ↗
32. Hydrothermal corrosion of SiC-based materials in LWR environments
33. Carpenter · 2010