journal article·2019-02

Oxidation of stainless steel in vacuum and evolution of surface oxide scales during hot-compression bonding

Bijun Xie, Mingyue Sun, Bin Xu, Chunyang Wang, Haiyang Jiang, Dianzhong Li, Yiyi Li

Corrosion Science· Volume 147
Publisher page

Abstract

Abstract The oxidation behaviour of austenite stainless steel in vacuum and the evolution of oxide scales during vacuum hot-compression bonding were investigated combining XPS and TEM. The results indicate that thick duplex oxide scale with outer MnFe2O4 and inner FeCr2O4 layer was formed in a low vacuum and the complex oxide scale transformed into interfacial oxides MnCr2O4 remaining at the bonding interface after hot-compression bonding at 1200 °C. While in a high vacuum, nanoscale-thick oxide scale with outer Fe3O4 and inner Fe- and Cr-rich layer was observed and it decomposed during the subsequent hot-compression bonding procedure, leading to a well-bonded interface.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced Welding Techniques Analysis · Advanced materials and composites · High-Temperature Coating Behaviors

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (43)

Show source-provided references
1. Development of multilayer steels for improved combinations of high strength and high ductility10.2320/matertrans.M2013382 ↗
2. Clad metals, roll bonding and their applications for SOFC interconnects10.1016/j.jpowsour.2005.01.055 ↗
3. A novel reduction-bonding process to fabricate stainless steel clad plate10.1016/j.jallcom.2014.07.186 ↗
4. Cladding of low-carbon steel to austenitic stainless steel by hot-roll bonding: microstructure and mechanical properties before and after welding10.1016/j.msea.2015.12.088 ↗
5. Interfacial microstructure and properties of a vacuum hot roll-bonded titanium-stainless steel clad plate with a niobium interlayer10.1007/s40195-013-0283-9 ↗
6. Deformation and fracture of Ti/439 stainless steel clad composite at intermediate temperatures10.1016/j.msea.2015.11.041 ↗
7. Effect of heat treatment on tensile deformation characteristics and properties of Al3003/STS439 clad composite10.1016/j.msea.2013.12.019 ↗
8. A hybrid joint based on two kinds of bonding mechanisms for Titanium alloy and stainless steel by pulsed laser welding10.1016/j.matlet.2016.08.138 ↗
9. Joint properties and microstructure of diffusion-bonded grade 2 titanium to AISI 430 ferritic stainless steel using pure Ni interlayer10.1007/s00170-015-8244-2 ↗
10. An investigation into the explosive welding/cladding of Grade A ship steel/AISI 316L austenitic stainless steel
11. Hot rolling bonded multilayered composite steels and varied tensile deformation behaviour10.1179/1743284711Y.0000000116 ↗
12. Interface characteristic and properties of stainless steel/HSLA steel clad plate by vacuum rolling cladding10.2320/matertrans.M2011127 ↗
13. Effect of interface oxides on shear properties of hot-rolled stainless steel clad plate10.1016/j.msea.2016.05.066 ↗
14. Characterization and corrosion behavior of F6NM stainless steel treated in high temperature water10.1016/j.apsusc.2017.11.089 ↗
15. Early oxidation mechanism of austenitic stainless steel TP347H in supercritical water10.1016/j.corsci.2017.09.023 ↗
16. High temperature oxidation of stainless steel AISI316L in air plasma10.1016/j.apsusc.2008.06.017 ↗
17. Multitechnique characterisation of 304L surface states oxidised at high temperature in steam and air atmospheres10.1016/j.apsusc.2016.01.185 ↗
18. Evolution of steel surface composition with heating in vacuum and in air10.1016/j.apsusc.2011.06.128 ↗
19. Effect of surface machining on the corrosion behaviour of 316 austenitic stainless steel in simulated PWR water10.1016/j.corsci.2017.06.019 ↗
20. Intergranular oxidation of 316L stainless steel in the PWR primary water environment10.1016/j.corsci.2017.06.023 ↗
21. Evolution of surface chemistry and morphology of oxide scale formed during initial stage oxidation of modified 9Cr–1Mo steel10.1016/j.corsci.2013.10.026 ↗
22. Characteristics of oxide scale formed on Cu-bearing austenitic stainless steel during early stages of high temperature oxidation10.1016/j.apsusc.2015.06.055 ↗
23. Breakaway oxidation behaviour of ferritic stainless steels at 1150°C in humid air10.1016/j.corsci.2016.02.042 ↗
24. Oxidation of a Fe–18Cr–8Ni austenitic stainless steel at 850°C in O2: microstructure evolution during breakaway oxidation10.1016/j.corsci.2016.10.029 ↗
25. Initial oxidation and chromium diffusion. I. Effects of surface working on 9–20% Cr steels10.1016/j.corsci.2003.09.004 ↗
26. Chastain · 1992
27. Duplex stainless steel passive film electrical properties studied by in situ current sensing atomic force microscopy10.1016/j.corsci.2013.08.031 ↗
28. Multicomponent effects on the crystal structures and electrochemical properties of spinel-structured M3O4 (M = Fe, Mn, Co) anodes in Lithium rechargeable batteries10.1021/cm2036794 ↗
29. Analysis of XPS spectra of Fe2+ and Fe3+ ions in oxide materials10.1016/j.apsusc.2007.09.063 ↗
30. Synthesis and characterization of polymer-coated manganese ferrite nanoparticles as controlled drug delivery10.1016/j.apsusc.2017.09.096 ↗
31. Electrical conductivity of Mn‐Zn ferrites
32. Identification of MnCr2O4 nano-octahedron in catalysing pitting corrosion of austenitic stainless steels10.1016/j.actamat.2010.05.043 ↗
33. Birks · 2006
34. Oxidation of Ni-Cr alloy at intermediate oxygen pressures. II. Towards the lifetime prediction of alloys10.1016/j.corsci.2016.05.024 ↗
35. Corrosion of engineering materials in a supercritical water cooled reactor: characterization of oxide scales on Alloy 800H and stainless steel 31610.1016/j.corsci.2015.07.035 ↗
36. Diffusion of cations in chromia layers grown on iron-base alloys10.1007/BF00665632 ↗
37. The oxidation of iron-chromium-manganese alloys at 900 C10.1007/BF00938460 ↗
38. TEM investigations of the oxide layers formed on a 316L alloy in simulated PWR environment10.1007/s10853-012-6975-0 ↗
39. Samsonov · 2013
40. Microstructural characterization of SCC crack tip and oxide film for SUS 316 stainless steel in simulated PWR primary water at 320°C10.1080/18811248.2005.9726383 ↗
41. Thermo-Calc & DICTRA, computational tools for materials science10.1016/S0364-5916(02)00037-8 ↗
42. Steels · 2016
43. Dissolution and evolution of interfacial oxides improving the mechanical properties of solid state bonding joints10.1016/j.matdes.2018.08.003 ↗