Oxidation of zirconium diboride–silicon carbide ceramics under an oxygen partial pressure of 200 Pa: Formation of zircon
Source abstract
Abstract
Abstract The formation and evolution of zircon during oxidation of ZrB 2 –20 vol.% SiC ceramics under a low oxygen partial pressure of 200 Pa is studied. The formation mechanism of zircon is proposed according to experimental results and thermodynamic consideration. And the main reason to the formation of zircon can be attributed to the active oxidation of SiC. Two steps can be divided for the formation and evolution of zircon: (1) nucleation from silica glass; and (2) crystal growth into prism like particles. Furthermore, the emergence of zircon significantly improves the oxidation resistance performance.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · Nuclear materials and radiation effects
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (29)
Show source-provided references
1. Materials for temperatures above 1500 °C in oxidizing atmospheres. Part I: basic considerations on materials selection10.1002/1521-4176(200103)52:3<204::AID-MACO204>3.0.CO;2-J ↗
2. Stability of ultra-high-temperature ZrB2–SiC ceramics under simulated atmospheric re-entry conditions10.1016/j.jeurceramsoc.2007.02.201 ↗
3. Resistance to thermal shock and to oxidation of metal diborides–SiC ceramics for aerospace application10.1111/j.1551-2916.2007.01589.x ↗
4. Preparation and thermal ablation behavior of HfB2–SiC-based ultra-high-temperature ceramics under severe heat conditions10.1111/j.1744-7402.2008.02264.x ↗
5. Arc-jet testing on HfB2 and HfC-based ultra-high temperature ceramic materials10.1016/j.jeurceramsoc.2007.11.021 ↗
6. Temperature dependent hardness and strength properties of TiB2 with TiSi2 sinter-aid10.1016/j.jeurceramsoc.2008.11.018 ↗
7. Thermophysical properties of ZrB2 and ZrB2–SiC ceramics10.1111/j.1551-2916.2008.02268.x ↗
8. Thermal and electrical properties in hot-pressed ZrB2–MoSi2–SiC composites10.1111/j.1551-2916.2007.01660.x ↗
9. High-temperature oxidation of zirconium diboride
10. High-temperature oxidation of borides of the group IV metals. II. Oxidation of zirconium and hafnium diboride
11. A model for the oxidation of ZrB2, HfB2 and TiB210.1016/j.actamat.2007.07.027 ↗
12. The ZrB2 volatility diagram10.1111/j.1551-2916.2005.00599.x ↗
13. Thermodynamic analysis of ZrB2–SiC oxidation: formation of a SiC-depleted region10.1111/j.1551-2916.2006.01329.x ↗
14. Oxidation mechanism and resistance of ZrB2–SiC composites10.1016/j.corsci.2009.07.005 ↗
15. Effect of phase change and oxygen permeability in oxide scales on oxidation kinetics of ZrB2 and HfB210.1111/j.1551-2916.2009.03031.x ↗
16. Evolution of structure during the oxidation of zirconium diboride–silicon carbide in air up to 1500 °C10.1016/j.jeurceramsoc.2006.10.012 ↗
17. Improved processing and oxidation-resistance of ZrB2 ultra-high temperature ceramics containing SiC nanodispersoids10.1016/j.msea.2007.03.002 ↗
18. Kinetic analysis of heat resistance of ZrB2–SiC composites10.1007/s10720-005-0087-8 ↗
19. Wen-bo Han, Ping Hu, Xinghong Zhang, et al., High-temperature oxidation at 1900 °C of ZrB2−xSiC ultrahigh-temperature ceramic composites, Journal of the American Ceramic Society 91 (2008) 3328–3334.10.1111/j.1551-2916.2008.02660.x ↗
20. Diletta Sciti, Mylene Brach, Alida Bellosi, Oxidation behavior of a pressure less sintered ZrB2–MoSi2 ceramic composites, Materials Research Society 20 (2005) 922–930.10.1557/JMR.2005.0111 ↗
21. Frédéric Monteverde, Raffaele Savino, Stability of ultra-high-temperature ZrB2–SiC ceramics under simulated atmosphere re-entry conditions, Journal of the European Ceramic Society 27 (2007) 4797–4805.10.1016/j.jeurceramsoc.2007.02.201 ↗
22. Jiecai Han, Ping Hu, Xinghong Zhang, et al., Oxidation-resistant ZrB2–SiC composites at 2200 °C, Composites Science and Technology 68 (2008) 799–806.10.1016/j.compscitech.2007.08.017 ↗
23. Jiecai Han, Ping Hu, Xinghong Zhang, et al., Oxidation behavior of zirconium diboride–silicon carbide at 1800 °C, Scripta Materialia 57 (2007) 825–828.10.1016/j.scriptamat.2007.07.009 ↗
24. Alireza Rezaie, William G. Fahrenholtz, Gregory E. Hilmas, Oxidation of zirconium diboride–silicon carbide at 1500 °C at a low partial pressure of oxygen, Journal of the American Ceramic Society 89 (2006) 3240–3245.10.1111/j.1551-2916.2006.01229.x ↗
25. Ju Li, Thomas J. Lenosky, et al., Thermochemical and mechanical stabilities of the oxide scale of ZrB2–SiC and oxygen transport mechanisms, Journal of the American Ceramic Society 91 (2008) 1475–1480.10.1111/j.1551-2916.2008.02319.x ↗
26. Linhong Guo, Hui Li, Phase transformations and structure characterization of calcium polyphosphate during sintering process, Journal of Materials Science 39 (2004) 7041–7047.10.1023/B:JMSC.0000047549.18666.85 ↗
27. Gerhard Vavra, On the kinematics of zircon growth and its petrogenetic significance: a cathodoluminescence study, Contrib Mineral Petrol 106 (1990) 90–99.10.1007/BF00306410 ↗
28. Daniele J. Cherniak, E. Bruce Watson, Diffusion in zircon, Reviews in Mineralogy and Geochemistry 51 (2003) 113–143.10.2113/0530113 ↗
29. The diffusion of oxygen in zirconia as a function of oxygen pressure10.1007/BF00604736 ↗