Hydrogen permeation behavior in relation to microstructural evolution of low carbon bainitic steel weldments
Source abstract
Abstract
Abstract The microstructures of high strength bainitic steel weldments were characterized, and their hydrogen permeability was investigated by the electrochemical permeation technique. The effective diffusion coefficient in the welded joint increases with heat input, while the hydrogen concentration at the sub-surface decreases with increasing heat input, mainly due to coarsening grain and inclusion sizes. Compared with as-welded specimens, the tempered membranes have lower effective diffusion coefficient and higher density of hydrogen traps due to newly formed carbides acting as hydrogen trapping sites that are derived from the decomposition of martensite-austenite constituents. These were further confirmed by the partial permeation technique.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Microstructure and Mechanical Properties of Steels · Corrosion Behavior and Inhibition
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (50)
Show source-provided references
1. Anderson · 2005
2. Effects of hydrogen on the properties of iron and steel10.1007/BF02654700 ↗
3. Recent advances in the study of structural materials compatibility with hydrogen10.1002/adma.200904354 ↗
4. Hydrogen effects on the microstructure of a 2.25Cr- 1Mo-0.25 V steel welded joint10.1016/j.ijhydene.2015.07.095 ↗
5. Hydrogen embrittlement of ferritic steels: observations on deformation microstructure, nanoscale dimples and failure by nanovoiding10.1016/j.actamat.2012.06.014 ↗
6. Hydrogen trapping in ferritic steel weld metal10.1179/095066002225006548 ↗
7. ISO 17081:2004(E), Method of Measurement of Hydrogen Permeation and Determination of Hydrogen Uptake and Transport in Metals by an Electrochemical Technique, ISO, Switzerland, 2004.
8. Correlation of microstructural parameters and hydrogen permeation in carbon steel10.1007/BF02649489 ↗
9. The influence of microstructure on hydrogen transport in carbon steels10.1016/0010-938X(96)00109-6 ↗
10. Influence of microstructure on the hydrogen permeability of 9%Cr-1%Mo ferrite steel10.1016/S0022-3115(98)00486-3 ↗
11. Quantification of hydrogen diffusion and trapping in 2.25Cr-1Mo and 3Cr-1Mo-V steels with the electrochemical permeation technique and melt extractions10.1007/s11661-004-0253-y ↗
12. Response of hydrogen trapping capability to microstructural change in tempered Fe-0.2C martensite10.1016/j.scriptamat.2004.11.008 ↗
13. Effect of microstructure on the hydrogen trapping efficiency and hydrogen induced cracking of linepipe steel10.1016/j.corsci.2008.03.007 ↗
14. Characterization of inclusions of X80 pipeline steel and its correlation with hydrogen-induced cracking10.1016/j.corsci.2010.12.011 ↗
15. Modelling the influence of trapping on hydrogen permeation in metals10.1016/j.corsci.2013.07.010 ↗
16. Effects of hydrogen-charging on the susceptibility of X100 pipeline steel to hydrogen-induced cracking10.1016/j.ijhydene.2009.09.090 ↗
17. Effect of microstructure and inclusions on hydrogen induced cracking susceptibility and hydrogen trapping efficiency of X120 pipeline steel10.1016/j.msea.2010.07.022 ↗
18. Determination of trapping parameters and the chemical diffusion coefficient from hydrogen permeation experiments10.1016/j.corsci.2014.01.002 ↗
19. Effect of microstructure and composition on hydrogen permeation in X70 pipeline steels10.1016/j.ijhydene.2012.11.127 ↗
20. Micro-electrochemical characterization of corrosion of welded X70 pipeline steel in near-neutral pH solution10.1016/j.corsci.2009.04.030 ↗
21. Corrosion of simulated weld HAZ of API X-80 pipeline steel10.1016/j.corsci.2012.06.014 ↗
22. In situ corrosion characterization of simulated weld heat affected zone of API X80 pipeline steel10.1016/j.corsci.2014.04.053 ↗
23. Stress corrosion cracking of E690 steel as a welded joint in a simulated marine atmosphere containing sulphur dioxide10.1016/j.corsci.2015.08.039 ↗
24. Hydrogen permeation and electrochemical corrosion behavior of the X80 pipeline steel weld10.1007/s11665-012-0216-1 ↗
25. Hydrogen permeation in a submerged arc weldment of TMCP steel10.1016/S0254-0584(02)00100-1 ↗
26. Welding heat input on the hydrogen permeation in the X80 steel welded joints10.1016/j.matchemphys.2011.11.036 ↗
27. The effect of post-weld heat treatment affecting corrosion resistance and hydrogen embrittlement of HAZ part in FCAW10.1016/S0257-8972(03)00060-4 ↗
28. Effect of post-weld heat treatment on the microstructure and hydrogen permeation of 13CrNiMo steels10.1016/j.corsci.2003.10.006 ↗
29. Microstructure evolution in a low carbon Nb-Ti microalloyed steel10.2355/isijinternational.46.161 ↗
30. Effect of post-weld heat treatment on hydrogen-assisted cracking behavior of high-strength process in a sour environment10.1016/j.scriptamat.2012.08.021 ↗
31. Adaptation of the electrochemical permeation technique for studying entry, transport and trapping of hydrogen in metals10.1016/j.electacta.2005.02.151 ↗
32. Measurement of lattice and apparent diffusion coefficient of hydrogen in X65 and F22 pipeline steels10.1016/j.ijhydene.2012.11.059 ↗
33. Hydrogen diffusion into three metallurgical microstructures of a C-Mn X65 and low alloy F22 sour service steel pipelines10.1016/j.ijhydene.2014.06.122 ↗
34. Reversible hydrogen trapping in a 3.5NiCrMoV medium strength steel10.1016/j.corsci.2015.04.011 ↗
35. Analysis of electrochemical hydrogen permeation through X-65 pipeline steel and its implication on pipeline stress corrosion cracking10.1016/j.ijhydene.2006.07.018 ↗
36. Effect of environmental and metallurgical factors on hydrogen induced cracking of HSLA steels10.1016/j.corsci.2008.09.030 ↗
37. Hydrogen trapping mechanisms by permeation techniques10.1016/0036-9748(79)90392-2 ↗
38. Influence of microstructural aspects on impact toughness of multi-pass submerged arc welded HSLA steel joints10.1016/j.matdes.2015.10.158 ↗
39. The nature of acicular ferrite in HSLA steel weld metals10.1007/BF00540369 ↗
40. Effect of reheat temperature on continuous cooling bainite transformation behavior in low carbon microalloyed steel10.1007/s10853-013-7251-7 ↗
41. Effect of retained austenite on the hydrogen embrittlement of a medium carbon quenching and partitioning steel with refined microstructure10.1016/j.msea.2016.04.025 ↗
42. Microstructural characters and toughness of different sub-regions in the welding heat affected zone of low carbon bainitic steel
43. Study of the hydrogen diffusion and segregation into Fe-C-Mo martensitic HSLA steel using electrochemical permeation test10.1016/j.jpcs.2010.07.017 ↗
44. Effect of retained austenite on the hydrogen content and effective diffusivity of martensitic structure10.1007/BF02851351 ↗
45. Bainite in steels10.1007/BF02656561 ↗
46. Structure-property relationships in bainitic steels10.1007/BF02672567 ↗
47. Interaction of hydrogen with the microstructure of low-carbon steel10.1016/j.msea.2006.07.089 ↗
48. Hydrogen permeation and embrittlement susceptibility of X80 welded joint under high-pressure coal gas environment10.1016/j.corsci.2016.04.029 ↗
49. Absorption of hydrogen in tensile strained iron and high-carbon steel studied by electrochemical permeation and desorption techniques10.1016/j.ijhydene.2008.12.088 ↗
50. Hydrogen trapping in an API 5 L X60 steel10.1016/j.corsci.2011.09.008 ↗