journal article·2011-11

Short-term oxidation resistance and degradation of Cr2AlC coating on M38G superalloy at 900–1100 °C

J.J. Li, M.S. Li, H.M. Xiang, X.P. Lu, Y.C. Zhou

Corrosion Science· Volume 53· Issue 11
Publisher page

Abstract

[Li, J. J.; Li, M. S.; Xiang, H. M.; Lu, X. P.; Zhou, Y. C.] Chinese Acad Sci, Inst Met Res, Shenyang Natl Lab Mat Sci, Shenyang 110016, Peoples R China. [Li, J. J.; Xiang, H. M.; Lu, X. P.] Chinese Acad Sci, Grad Sch, Beijing 100039, Peoples R China.;Li, MS (reprint author), Chinese Acad Sci, Inst Met Res, Shenyang Natl Lab Mat Sci, 72 Wenhua Rd, Shenyang 110016, Peoples R China;mshli@imr.ac.cn
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: MXene and MAX Phase Materials · High-Temperature Coating Behaviors · Intermetallics and Advanced Alloy Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (46)

Show source-provided references
1. Protective coatings in the gas turbine engine10.1016/0257-8972(94)90129-5 ↗
2. Simultaneous chromizing and aluminizing using chromium oxide and aluminum: (I) on low alloy steel10.1016/S0257-8972(99)00518-6 ↗
3. The Mn+1AXn phases: a new class of solids; thermodynamically stable nanolaminates10.1016/S0079-6786(00)00006-6 ↗
4. Progress in research and development on MAX phases: a family of layered ternary compounds10.1179/1743280410Y.0000000001 ↗
5. The Mn+1AXn phases: materials science and thin-film processing10.1016/j.tsf.2009.07.184 ↗
6. Kohlenstoffhaltige ternare verbindungen (H-phase)10.1007/BF00913068 ↗
7. In-situ hot pressing/solid-liquid reaction synthesis of bulk Cr2AlC10.3139/146.101033 ↗
8. High-temperature oxidation and hot corrosion of Cr2AlC10.1016/j.actamat.2007.07.024 ↗
9. Synthesis and thermal and electrical properties of bulk Cr2AlC10.1016/j.scriptamat.2005.11.009 ↗
10. Oxidation behavior of Cr2AlC ceramics at 1100 and 1250°C10.1007/s10853-008-2516-2 ↗
11. Oxidation of Cr2 AlC between 900 and 1200°C in air10.1007/s11085-007-9071-0 ↗
12. Oxidation of Cr2AlC at 1300°C in air10.1016/j.corsci.2007.03.044 ↗
13. Cyclic oxidation of Cr2 AlC between 1000 and 1300°C in air10.1016/j.jallcom.2007.10.018 ↗
14. High temperature oxidation of a nanolayer laminated (Cr0.95Ti0.05)2AlC compound in air10.1166/jnn.2010.1522 ↗
15. Ab initio calculations and experimental determination of the structure of Cr2AlC10.1016/j.ssc.2004.02.047 ↗
16. Effect of the composition on the structure of Cr–Al–C investigated by combinatorial thin film synthesis and ab initio calculations10.1002/adem.200400096 ↗
17. Towards large area deposition of Cr2AlC on steel10.1016/j.tsf.2005.12.219 ↗
18. Variation of microstructure and composition of the Cr2AlC coating prepared by sputtering at 370 and 500°C10.1016/j.surfcoat.2010.04.067 ↗
19. M. to Baben, Fabrication and oxidation behavior of Cr2AlC coating on Ti6242 alloy10.1016/j.surfcoat.2010.01.002 ↗
20. Oxide formation of K38G superalloy and its sputtered micrograined coating10.1016/S0257-8972(05)80014-3 ↗
21. Oxidation resistance of Cr1-xAlxN (0.18⩽x⩽0.47) coating on K38G superalloy at 1000–1100°C in air10.1016/j.surfcoat.2006.05.045 ↗
22. XRD and Raman spectroscopic comparative study on phase transformation of γ-Al2O3 at high temperature
23. Florescence spectroscopic study of the phase transformation of γ-Al2 O3 at high temperature10.1002/pssa.200521333 ↗
24. Oxidation of NiAl and FeAl10.1016/S0966-9795(99)00037-0 ↗
25. The oxidation behaviour of NiAl-I. Phase transformations in the alumina scale during oxidation of NiAl and NiAl–Cr alloys10.1016/0010-938X(92)90002-K ↗
26. Oxidation behavior of fine-grain MA 956 superalloy10.1023/A:1004582713929 ↗
27. Effect of NiAl microcrystalline coating on the high-temperature oxidation behavior of NiAl–28Cr–5Mo–1Hf10.1023/A:1020516921239 ↗
28. Influence of columnar microstructure of a sputtered NiAl coating on its oxidation behavior at 1000°C10.1016/S0966-9795(02)00020-1 ↗
29. Atomic scale characterization of layered ternary Cr2AlC ceramic10.1063/1.2188074 ↗
30. The ternary systems: Cr–Al–C, V–Al–C, and Ti–Al–C and the behaviour of H-phases (M2AlC)10.1016/0022-4596(80)90569-1 ↗
31. Kinetics of high temperature oxidation and chromia volatilization for a binary Ni–Cr alloy10.1007/s11085-005-6562-8 ↗
32. Kinetic analysis of high-temperature oxidation of metals accompanied by scale volatilization10.1149/1.1392534 ↗
33. High-temperature oxidation behavior of Ti2AlC in air10.1023/A:1023092027697 ↗
34. Characterization of phase relations and properties in air-oxidized Ti3SiC210.1016/j.msea.2007.02.034 ↗
35. Isothermal oxidation of Ta2AlC in air10.1111/j.1551-2916.2006.01148.x ↗
36. Oxidation of Tin+1AlXn where n=1–3 and X is C, N (part II): experimental and results10.1149/1.1380256 ↗
37. Improving the oxidation resistance of Ti3SiC2 by forming a Ti3Si0.9Al0.1C2 solid solution10.1016/j.actamat.2004.04.015 ↗
38. Oxidation of Ti2AlC bulk and spray deposited coatings10.1016/j.corsci.2010.08.004 ↗
39. Internal nitridation of nickel-base alloys. Part II. behavior of quaternary N–Cr–Al–Ti alloys and computer-based description
40. Selective oxidation and internal nitridation during high-temperature exposure of single-crystalline nickel-base superalloys10.1007/s11661-000-0051-0 ↗
41. The initial stages in the oxidation of TiAl10.1002/maco.19970480104 ↗
42. Internal nitridation behaviour during long-term creep in a nickel-base superalloy10.1016/S1359-6462(01)00953-8 ↗
43. High-temperature oxidation behavior of aluminide coatings on a new cobalt-base superalloy in air10.1016/S0010-938X(00)00137-2 ↗
44. Effect of microcrystallization on the cyclic oxidation behavior of β-NiAl intermetallics at 1000°C in air10.1016/S0966-9795(01)00059-0 ↗
45. Oxidation behavior of sputtered Ni–3Cr–20Al nanocrystalline coating10.1016/S0921-5093(99)00258-0 ↗
46. Isothermal oxidation of β-NiAl alloys and sputtered coating at 1000°C in air