journal article·2019-08

Corrosion and degradation mechanism of Ag/Ti3AlC2 composites under dynamic electric arc discharge

Jianxiang Ding, Wubian Tian, Dandan Wang, Peigen Zhang, Jian Chen, Yamei Zhang, ZhengMing Sun

Corrosion Science· Volume 156
Publisher page

Abstract

Abstract The Ag/10 wt%Ti3AlC2 (Ag/10TAC) composite exhibits excellent arc resistance and potential application in various industries. To understand its corrosion mechanism, dynamic electric arc discharge was conducted on the Ag/10TAC surface. The Ag matrix was subjected to melting, vaporization, deposition, absorption, and diffusion, resulting in chemical reactions and various morphologies. The Ti3AlC2 was degraded by a rapid “decomposition–oxidation.” The degradation of the Ag/10TAC composite is attributed to the changes in structure and function on the contact surfaces. The present study facilitates the design, performance optimization, and failure analysis of Ag/Mn + 1AXn (Ag/MAX) composites.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: MXene and MAX Phase Materials · Aluminum Alloys Composites Properties · Advanced materials and composites

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (32)

Show source-provided references
1. Evolution of the AgCdO contact material surface microstructure with the number of arcs10.1007/s11664-010-1097-4 ↗
2. Reinforcement of conducting silver-based materials
3. Corrosion, oxidation, erosion and performance of Ag/W-based circuit breaker contacts: a review10.1016/j.corsci.2018.02.010 ↗
4. Recent researches and new trends of electrical contacts
5. PM helps develop cadmium-free electrical contacts10.1016/S0026-0657(04)00206-1 ↗
6. Replacement of AgCdO by AgSnO2 in DC contactors
7. Silver-metal oxides as contact materials10.1109/TCHMT.1987.1134702 ↗
8. Erosion and resistance characteristics of AgW and AgC contacts10.1109/6144.774755 ↗
9. Investigation on microstructure and performance of Ag/ZnO contact material10.1016/j.jallcom.2007.03.099 ↗
10. Arc erosion behavior of Ag/Ni electrical contact materials10.1016/j.matdes.2015.06.142 ↗
11. Fabrication of Mg-doped ZnO nanofibers with high purities and tailored band gaps10.1016/j.ceramint.2016.03.105 ↗
12. The MN+1AXN phases: a new class of solids: thermodynamically stable nanolaminates10.1016/S0079-6786(00)00006-6 ↗
13. The effects of Sn content on the microstructure and the formation mechanism of Ti2SnC powder by pressureless synthesis10.1016/j.jallcom.2016.11.398 ↗
14. Progress in research and development on MAX phases: a family of layered ternary compounds10.1179/1743280410Y.0000000001 ↗
15. MAX phases: bridging the gap between metals and ceramics
16. Arc erosion behavior of Ag/Ti3AlC2 electrical contact materials10.1016/j.jallcom.2018.01.015 ↗
17. Preparation and arc erosion properties of Ag/Ti2SnC composites under electric arc discharging10.1007/s40145-018-0296-y ↗
18. Anisotropic properties of Ag/Ti3AlC2 electrical contact materials prepared by equal channel angular pressing10.1016/j.jallcom.2019.01.083 ↗
19. Microstructure evolution, oxidation behavior and corrosion mechanism of Ag/Ti2SnC composite during dynamic electric arc discharging10.1016/j.jallcom.2019.01.252 ↗
20. A spectroscopic detecting system for measuring the temperature distribution of silver breaking arc using a CCD color camera10.1109/19.772195 ↗
21. The effect of lithium upon the erosion kinetics of Ag-CdO contacts10.1109/TCHMT.1982.1135947 ↗
22. The statistical estimation of arc temperature between Ag-n% CdO contacts
23. A critical review of the oxidation of Ti2AlC, Ti3AlC2 and Cr2AlC in air10.1080/21663831.2013.806364 ↗
24. Oxidation behavior of Ti3AlC2 at 1000–1400 ℃ in air10.1016/S0010-938X(02)00177-4 ↗
25. Ultra-high-temperature oxidation and thermal stability of Ti2AlC in air at 1600–1800 °C10.1007/s11085-016-9639-7 ↗
26. Synthesis and characterization of Ti3AlC210.1111/j.1151-2916.2000.tb01281.x ↗
27. Layered machinable and electrically conductive Ti2AlC and Ti3AlC2 ceramics: a review10.1016/S1005-0302(10)60064-3 ↗
28. Influence of water vapor on the oxidation behavior of Ti3AlC2 and Ti2AlC10.1016/j.scriptamat.2007.09.011 ↗
29. Oxidation characteristics of Ti3AlC2 over the temperature range 500–900 ℃10.1016/j.matchemphys.2009.06.016 ↗
30. Pang · 2012 · 289
31. Microstructure and properties of Ti3AlC2 prepared by the solid-liquid reaction synthesis and simultaneous in-situ hot pressing process10.1016/S1359-6454(02)00117-9 ↗
32. High-temperature oxidation of Ti3AlC2 between 1173 and 1473 K in air10.1016/j.msea.2006.07.060 ↗