Corrosion performance of Ti3SiC2, Ti3AlC2, Ti2AlC and Cr2AlC MAX phases in simulated primary water conditions
Source abstract
Abstract
The response of Ti3SiC2, Ti3AlC2, Ti2AlC and Cr2AlC MAX phases under simulated primary water has been explored for the first time. Samples were tested for 28 days in 300 °C water with the addition of 2 ppm LiOH. The Ti-based MAX phases formed oxides of TiO and TiFeO3. X-ray diffraction and scanning electron microscopy showed no evidence of a passive Al or Si-based layer forming during testing. A-layer dissolution was observed to cause delamination of the layered structure. In contrast, Cr2AlC showed little change during autoclave testing, suggesting that a thin passivating chromia layer was formed.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: MXene and MAX Phase Materials · Advanced ceramic materials synthesis · Aluminum Alloys Composites Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (19)
Show source-provided references
1. Mechanical properties of the MAX phases
2. Ti3SiC2–a layered ceramic exhibiting ultra-low friction10.1016/S0167-577X(98)00206-7 ↗
3. Cold spray deposition of Ti2AlC coatings for improved nuclear fuel cladding10.1016/j.jnucmat.2015.06.028 ↗
4. Tribological properties of Ti3SiC2 coupled with different counterfaces10.1016/j.ceramint.2015.01.150 ↗
5. An analysis of the hydrogen explosion in the Fukushima-Daiichi accident10.1016/j.ijhydene.2015.03.154 ↗
6. High-temperature oxidation behavior of Ti2AlC in air10.1023/A:1023092027697 ↗
7. Oxidation behavior of Ti3AlC2 at 1000–1400C in air10.1016/S0010-938X(02)00177-4 ↗
8. Oxidation of Ti3SiC2 in air10.1149/1.1837846 ↗
9. Oxidation of Cr2AlC at 1300 °C in air10.1016/j.corsci.2007.03.044 ↗
10. Anisotropic corrosion of Ti 2 AlC and Ti 3 AlC 2 in supercritical water at 500 °C10.1016/j.ceramint.2017.02.153 ↗
11. Ceramic coating for corrosion (c3) resistance of nuclear fuel cladding10.1016/j.surfcoat.2015.08.062 ↗
12. Multilayer (TiN, TiAlN) ceramic coatings for nuclear fuel cladding10.1016/j.jnucmat.2016.05.021 ↗
13. High-temperature neutron diffraction and the temperature-dependent crystal structures of the MAX phases Ti3SiC2 and Ti3GeC210.1103/PhysRevB.82.174109 ↗
14. On the interactions of Ti2AlC, Ti3AlC2, Ti3SiC2 and Cr2AlC with silicon carbide and pyrolytic carbon at 1300 °C10.1016/j.jeurceramsoc.2015.07.029 ↗
15. Hydrothermal oxidation behavior of bulk titanium aluminum carbide10.1111/j.1551-2916.2011.04590.x ↗
16. Mechanisms and kinetics of the hydrothermal oxidation of bulk titanium silicon carbide10.1111/j.1551-2916.2009.03570.x ↗
17. First-principles investigation of intrinsic defects and (N, O) impurity atom stimulated Al vacancy in first-principles investigation of intrinsic defects and N, O … impurity atom stimulated Al vacancy in Ti 2 AlC10.1063/1.3058718 ↗
18. MAX phase coatings for accident tolerant nuclear fuel
19. Neutronic evaluation of coating and cladding materials for accident tolerant fuels10.1016/j.pnucene.2015.11.006 ↗