Effect of prior deformation and heat treatment on the corrosion-induced hydrogen trapping in aluminium alloy 2024
Source abstract
Abstract
Abstract The nature of the corrosion-induced hydrogen trapping in Al-alloy 2024-T351 was studied by thermal desorption spectroscopy. The microstructure was altered by solution treatment and plastic deformation, prior to corrosion. The results showed that the high temperature, 500 °C, trap state (T4 state) is associated with the S-phase. In the absence of S-phase, hydrogen is trapped at vacancies, which liberate hydrogen at higher temperatures. Plastic deformation prior to corrosion revealed that the trap state at 400 °C (T3 state) is associated with dislocations. High plastic strains (above 0.06) lead to a reduction of hydrogen trapped in both dislocations and the S-phase.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Corrosion Behavior and Inhibition · Metal and Thin Film Mechanics
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (26)
Show source-provided references
1. Corrosion-induced hydrogen embrittlement in aluminum alloy 202410.1016/j.corsci.2005.05.015 ↗
2. A classification of hydrogen traps in steel10.1007/BF02812023 ↗
3. Grain size and grain-boundary effects on diffusion and trapping of hydrogen in pure nickel10.1016/j.actamat.2012.09.004 ↗
4. Modelling of thermal desorption of hydrogen from metals10.1016/S0921-5093(97)00426-7 ↗
5. The diffusion and trapping of hydrogen in high purity aluminum10.1016/S1359-6454(98)00333-4 ↗
6. The diffusion and trapping of hydrogen along the grain boundaries in polycrystalline nickel10.1016/j.scriptamat.2011.09.036 ↗
7. Thermal desorption spectroscopy study on the hydrogen trapping states in a pure aluminum10.2320/matertrans.L-M2010825 ↗
8. Behaviour of hydrogen in pure aluminium, Al–4 mass% Cu and Al–1 mass% Mg2Si alloys studied by tritium electron microautoradiography10.1007/BF00349974 ↗
9. Diffusion of hydrogen in pure large grain aluminum10.1016/0036-9748(82)90354-4 ↗
10. Hydrogen diffusion in Al–Li alloys10.1007/BF02654243 ↗
11. The identification of hydrogen trapping states in an Al–Li–Cu–Zr alloy using thermal desorption spectroscopy10.1007/s11661-000-0064-8 ↗
12. Absorption of hydrogen in tensile strained iron and high-carbon steel studied by electrochemical permeation and desorption techniques10.1016/j.ijhydene.2008.12.088 ↗
13. Study of the hydrogen diffusion and segregation into Fe–C–Mo martensitic HSLA steel using electrochemical permeation test10.1016/j.jpcs.2010.07.017 ↗
14. Thermal desorption spectroscopy study of the interaction between hydrogen and different microstructural constituents in lab cast Fe–C alloys10.1016/j.corsci.2012.08.017 ↗
15. Structures revealed in zone refined aluminum by tritium decoration10.1007/BF03038427 ↗
16. The trapping and transport phenomena of hydrogen in nickel10.1007/BF02643893 ↗
17. Hydrogen trapping by dislocations and grain boundaries in Fe–3%Si AHoy
18. Hydrogen diffusion and trapping in a precipitation-hardened nickel–copper–aluminum alloy Monel K-500 (UNS N05500)10.1016/j.actamat.2013.02.007 ↗
19. Evidence for the transport of impurity hydrogen with gliding dislocations in aluminum10.1016/1359-6462(96)00200-X ↗
20. Hydrogen trapping and repelling in an Al–6wt% Zn–2wt% Mg alloy10.1007/BF01119730 ↗
21. An investigation of hydrogen-induced hardening in 7075–T6 aluminum alloy10.1016/j.jallcom.2007.10.126 ↗
22. Characterization of trapped hydrogen in exfoliation corroded aluminium alloy 202410.1016/S1359-6462(99)00292-4 ↗
23. The contribution of hydrogen to the corrosion of 2024 aluminium alloy exposed to thermal and environmental cycling in chloride media10.1016/j.corsci.2012.12.005 ↗
24. Hydrogen in aluminum10.1016/S0925-8388(96)02968-4 ↗
25. Hydrogen trapping in an API 5L X60 steel10.1016/j.corsci.2011.09.008 ↗
26. Hydrogen trapping by cold-worked X-52 steel10.1016/S0010-938X(97)00100-5 ↗