An electrode array study of electrochemical inhomogeneity of zinc in zinc/steel couple during galvanic corrosion
Source abstract
Abstract
The local electrochemical properties of anodic metal within a zinc/steel couple immersed in seawater was studied via an electrode array composed of zinc and mild steel wire sensors. It showed that the potential and current density distribution of zinc wires were inhomogeneous, and the main anodic area moved from the zinc wires adjacent to the steel wires and even further away. Also, some zinc wires behaved as secondary cathodes. The observed electrochemical inhomogeneity was attributed to the variation of distances between the zinc and mild steel wire sensors over the electrode array as well as their surface electrochemical status. (C) 2009 Elsevier Ltd. All rights reserved.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Corrosion Behavior and Inhibition · Concrete Corrosion and Durability · Electrochemical Analysis and Applications
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (23)
Show source-provided references
1. The corrosion behaviour of the zinc–mild steel galvanic cell in hot sodium bicarbonate solution10.1016/0010-938X(85)90066-6 ↗
2. Corrosion mechanism of model zinc–magnesium alloys in atmospheric conditions10.1016/j.corsci.2008.06.008 ↗
3. The effects of inhomogeneity in organic coatings on electrochemical measurement using a wire beam electrode. I10.1016/0033-0655(91)80013-9 ↗
4. Wire beam electrode: a new tool for studying localised corrosion and other heterogeneous electrochemical processes10.1016/S0010-938X(98)00120-6 ↗
5. Mapping non-uniform corrosion using the wire beam electrode method. I. Multi-phase carbon dioxide corrosion10.1016/S0010-938X(00)00190-6 ↗
6. Mapping non-uniform corrosion using the wire beam electrode method. II. Crevice corrosion and crevice corrosion exemption10.1016/S0010-938X(00)00191-8 ↗
7. Mapping non-uniform corrosion using the wire beam electrode method. III. Water-line corrosion10.1016/S0010-938X(00)00192-X ↗
8. Sensing electrode inhomogeneity and electrochemical heterogeneity using an electrochemically integrated multielectrode array10.1149/1.3098477 ↗
9. A novel electrochemical testing method and its use in the investigation of the self-repairing ability of temporarily protective oil coating10.1016/S0010-938X(01)00108-1 ↗
10. Study of anti-contamination performance of temporarily protective oil coatings using wire beam electrode10.1016/S0010-938X(02)00066-5 ↗
11. W. Wang, X. Zhang, J. Wang, The influence of local glucose oxidase activity on the potential/current distribution on stainless steel: a study by the wire beam electrode method, Electrochim. Acta. doi: 10.1016/j.electacta.2009.04.064.10.1016/j.electacta.2009.04.064 ↗
12. A novel device for the wire beam electrode method and its application in the ennoblement study10.1016/j.corsci.2009.03.002 ↗
13. Novel corrosion experiments using the wire beam electrode. (I) Studying electrochemical noise signatures from localized corrosion processes10.1016/j.corsci.2004.11.019 ↗
14. Surface potential distribution over a zinc/steel galvanic couple corroding under thin layer of electrolyte10.1016/j.electacta.2006.09.061 ↗
15. Sacrificial anode cathodic polarization of steel in seawater. Part 2: Design and data analysis10.5006/1.3284858 ↗
16. Galvanic corrosion prediction using long-term and short-term polarization curves10.5006/1.3584889 ↗
17. The spatial distribution of Zn2+ during galvanic corrosion of a Zn/steel couple10.1016/j.electacta.2004.01.008 ↗
18. Measuring system for current distribution and its application to corrosion studies10.2320/jinstmet1952.48.2_191 ↗
19. Use of SVET and SECM to study the galvanic corrosion of an iron–zinc cell10.1016/j.corsci.2006.04.021 ↗
20. Corrosion mechanisms for zinc exposed to the atmosphere10.1149/1.2096868 ↗
21. Adzic · 1998
22. Diffusion-limited current density of oxygen reduction on copper10.1149/1.1526554 ↗
23. Localized electrochemical methods applied to cut edge corrosion10.1149/1.1393954 ↗