The effect of gas composition on the isothermal oxidation behaviour of PM chromium
Source abstract
Abstract
Abstract The effect of small amounts of water vapour on the isothermal high-temperature oxidation behaviour of powder-metallurgical (PM) chromium in Ar/20% O 2 and N 2 /20% O 2 has been studied. Additional oxidation experiments were performed with isotopically enriched gases, i.e. Ar/20% 18 O 2 and 15 N 2 /20% 18 O 2 under controlled humidity using H 2 16 O in combination with secondary ion mass spectrometry. In argon/oxygen, water vapour slightly increased the oxidation rate and was the main oxygen source for the oxidation process. The presence of water did not influence the type of kinetics and growth mechanism of oxide formation on pure chromium. In nitrogen/oxygen, the addition of water vapour reduced the oxide growth rate by about 50%. Under these conditions, nitrogen affects the reactivity of water molecules participating in the formation of an oxide layer. The mass transport mechanisms responsible for the formation of an oxide layer did not change, however. When nitrogen was present, a nitrogen-rich sub-layer formed near the scale/substrate interface, influencing the stress relaxation mechanism. Here, repetitive scale cracking occurred during isothermal exposure, which finally resulted in a more adherent and protective oxide layer with less internal stress and withstanding high thermal stresses accumulated during cooling from the test to ambient temperature.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced materials and composites · Nuclear Materials and Properties · High-Temperature Coating Behaviors
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (31)
Show source-provided references
1. Caplan · Oxid. Met. · 1975 · 9 · 45910.1007/BF00611694 ↗
2. Skeldon · Oxid. Met. · 1987 · 28 · 10910.1007/BF00666474 ↗
3. Jianian · Oxid. Met. · 1997 · 48 · 34710.1007/BF01670507 ↗
4. Zurek · Solid State Phenom. · 1995 · 41 · 18510.4028/www.scientific.net/SSP.41.185 ↗
5. Caplan · Corros. Sci. · 1963 · 3 · 16110.1016/S0010-938X(63)80086-4 ↗
6. Young · J. Electrochem. Soc. · 1987 · 134 · 225710.1149/1.2100862 ↗
7. Tveten · Oxid. Met. · 1999 · 51 · 22110.1023/A:1018866505708 ↗
8. Graham · J. Am. Ceram. Soc. · 1971 · 54 · 8910.1111/j.1151-2916.1971.tb12225.x ↗
9. Caplan · J. Electrochem. Soc. · 1961 · 108 · 43810.1149/1.2428106 ↗
10. Asteman · Oxid. Met. · 1999 · 52 · 9510.1023/A:1018875024306 ↗
11. Gleeson · Oxid. Met. · 1998 · 49 · 37310.1023/A:1018874206733 ↗
12. de Asmundis · Oxid. Met. · 1980 · 14 · 35110.1007/BF00603790 ↗
13. Mills · Oxid. Met. · 1981 · 15 · 43710.1007/BF00603535 ↗
14. Fox · Oxid. Met. · 1991 · 36 · 49110.1007/BF01151594 ↗
15. Graham · Mater. Sci. Forum · 1989 · 43 · 20710.4028/www.scientific.net/MSF.43.207 ↗
16. Hagel · J. Electrochem. Soc. · 1961 · 108 · 114610.1149/1.2427973 ↗
17. Akermark · Oxid. Met. · 1998 · 50 · 16710.1023/A:1018832103466 ↗
18. Brunner · Fresen. J. Anal. Chem. · 1997 · 358 · 23310.1007/s002160050392 ↗
19. Tsaı̈ · Defect Diffus. Forum · 1997 · 143–147 · 119510.4028/www.scientific.net/DDF.143-147.1195 ↗
20. Kofstad · 1988
21. I. Murris, Y.P. Jacob, V.A.C. Haanappel, M.F. Stroosnijder, The high temperature oxidation behaviour of chromium: the effect of different batches, Oxid. Met., in press
22. Gimpel · 1988 · 272
23. Mantel · Mém. Sci. Rev. Met. · 1989 · 511
24. Mantel · Mém. Sci. Rev. Met. · 1990 · 87 · 637
25. Kofstad · Oxid. Met. · 1995 · 44 · 310.1007/BF01046721 ↗
26. Asteman · Oxid. Met. · 1999 · 52 · 16110.1023/A:1018875024306 ↗
27. Asteman · Oxid. Met. · 2000 · 54 · 1110.1023/A:1004642310974 ↗
28. Stroosnijder · Surf. Coat. Technol. · 1996 · 83 · 20510.1016/0257-8972(95)02741-6 ↗
29. Mevrel · Mater. Sci. Technol. · 1987 · 3 · 53110.1080/02670836.1987.11782264 ↗
30. Jung · Oxid. Met. · 1996 · 46 · 14710.1007/BF01046888 ↗
31. Ramanathan · 1990 · vol. 4 · 177