journal article·2017-11

Bio-corrosion behaviour of oxygen diffusion layer on Ti-6Al-4V during tribocorrosion

R. Yazdi, H.M. Ghasemi, C. Wang, A. Neville

Corrosion Science· Volume 128
Publisher page

Abstract

Oxygen diffusion layers (ODL) on Ti-6Al-4V were produced by thermal oxidation at a temperature of 850 °C for three and six hours. ODL formation resulted in a β-Ti to α-Ti transformation, causing an increase in hardness. Polarization and EIS studies in stagnant and tribocorrosion conditions were performed under normal loads of 3–30 N in a phosphate buffered saline solution. In a stagnant condition, a passive bilayer film was formed on samples, which led to a low icorr. During tribocorrosion, the formation of a protective tribofilm resulted in a higher Ecorr and a lower icorr in ODLs compared with Ti-6Al-4V.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Metal and Thin Film Mechanics · Titanium Alloys Microstructure and Properties · Advanced materials and composites

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (51)

Show source-provided references
1. Titanium alloys in total joint replacement—a materials science perspective10.1016/S0142-9612(97)00146-4 ↗
2. Ti based biomaterials, the ultimate choice for orthopaedic implants – a review10.1016/j.pmatsci.2008.06.004 ↗
3. Biocompatibility of Ti-alloys for long-term implantation10.1016/j.jmbbm.2012.11.014 ↗
4. Microstructure and wear of in-situ Ti/(TiN+TiB) hybrid composite layers produced using liquid phase process10.1016/j.matchemphys.2014.12.026 ↗
5. Artificial hip joints: the biomaterials challenge10.1016/j.jmbbm.2013.06.001 ↗
6. Surface engineering of Ti6Al4 V surfaces for enhanced tribocorrosion performance in artificial seawater10.1016/j.matdes.2016.04.080 ↗
7. Assessing the tribocorrosion performance of Ti-6Al-4 V, 316 stainless steel and Monel K500 alloys in artificial seawater10.1002/maco.201106249 ↗
8. Influence of surface roughness on corrosion and tribological behaviour of CP-Ti after thermal oxidation treatment10.1007/s11665-009-9504-9 ↗
9. Triboelectrochemical techniques and interpretation methods in tribocorrosion: a comparative evaluation10.1016/j.triboint.2007.11.003 ↗
10. Thermal oxidation of Ti6Al4 V alloy and its biotribological properties under serum lubrication10.1016/j.triboint.2014.12.022 ↗
11. Influence of thermal oxidation duration on the microstructure and fretting wear behaviour of Ti6Al4 V alloy10.1016/j.matchemphys.2015.03.063 ↗
12. Effect of thermal oxidation on corrosion resistance of commercially pure titanium in acid medium
13. Corrosion and tribocorrosion performance of thermally oxidized commercially pure titanium in a 0.9% NaCl solution10.1007/s11665-015-1441-1 ↗
14. Fretting corrosion behaviour of thermally oxidized CP-Ti in Ringer’s solution10.1016/j.corsci.2009.10.029 ↗
15. Effect of thermal oxidation on corrosion and corrosion-wear behaviour of a Ti-6Al-4V alloy10.1016/j.biomaterials.2003.10.009 ↗
16. Principles of alloying titanium
17. Wear of diffusion hardened Ti-6Al-4V sliding against tool steel10.1016/j.wear.2009.10.009 ↗
18. Unlubricated sliding friction and wear characteristics of thermally oxidized commercially pure titanium10.1016/j.wear.2013.09.020 ↗
19. Direct diffusion through interpenetrating networks: oxygen in titanium10.1103/PhysRevLett.107.045504 ↗
20. Oxygen boost diffusion for the deep-case hardening of titanium alloys10.1016/S0921-5093(99)00697-8 ↗
21. The effect of treatment condition on boost diffusion of thermally oxidised titanium alloy10.1016/j.jallcom.2006.05.045 ↗
22. Enhanced wear resistance of titanium surfaces by a new thermal oxidation treatment10.1016/S0043-1648(99)00359-2 ↗
23. Improvement of wear resistance of Ti-6Al-4V alloy by means of thermal oxidation10.1016/j.matlet.2005.02.054 ↗
24. Oxygen diffusion enables anti-wear boundary film formation on titanium surfaces in zinc-dialkyl-dithiophosphate (ZDDP)-containing lubricants10.1016/j.scriptamat.2009.02.009 ↗
25. ASTM F2129-15 · 2015
26. Metallic biomaterials10.1007/978-0-387-84872-3_2 ↗
27. Influence of plastic deformation on the microstructure and corrosion behaviour of Ti-10Mo −4Zr and Ti-6Al −4V alloys in the Ringer’s solution at 37°C10.1016/j.corsci.2015.04.006 ↗
28. Effect of microstructure on oxygen rich layer evolution and its impact on fatigue life during high-temperature application of α/β titanium10.1016/j.actamat.2016.01.058 ↗
29. Fischer-Cripps · 2011
30. Strengthening of alpha titanium by interstitial solutes
31. Corrosion characterization of titanium alloys by electrochemical techniques10.1016/j.electacta.2005.02.121 ↗
32. Corrosion resistance of ultra fine-grained Ti10.1016/j.scriptamat.2004.04.011 ↗
33. Study of Ti-6Al-4V biomaterial using electrochemistry and XPS techniques10.1590/S0100-40422002000100003 ↗
34. Corrosion resistance of Ti-6Al-4 V alloy with nitride coatings in Ringer’s solution10.1016/j.corsci.2012.10.005 ↗
35. In situ impedance spectroscopy study of the electrochemical corrosion of Ti and Ti-6Al-4V in simulated body fluid at 25°C and 37°C10.1016/j.corsci.2009.06.035 ↗
36. Tribocorrosion properties of different type titanium alloys in simulated body fluid
37. Tribological, electrochemical and tribo-electrochemical characterization of bare and nitrided Ti6Al4 V in simulated body fluid solution10.1016/j.corsci.2011.01.057 ↗
38. Synergistic erosion-corrosion behaviour of commercially pure titanium at various impingement angles10.1016/j.wear.2017.03.016 ↗
39. Electrochemical impedance spectroscopy study of the passive oxide film on titanium for implant application10.1016/0013-4686(95)00465-3 ↗
40. Corrosion behaviour of some titanium dental alloys synthesized by cold crucible levitation melting
41. CPE analysis by local electrochemical impedance spectroscopy10.1016/j.electacta.2005.02.128 ↗
42. Electrochemical study of modified bis-[triethoxysilylpropyl] tetrasulfide silane films applied on the AZ31 Mg alloy10.1016/j.electacta.2006.12.086 ↗
43. Effect of surface roughness on leakage current and corrosion resistance of oxide layer on AZ91 Mg alloy prepared by plasma electrolytic oxidation10.1016/j.apsusc.2010.04.067 ↗
44. Study of the corrosion behaviour of titanium and some of its alloys for biomedical and dental implant applications10.1016/S0022-0728(99)00260-0 ↗
45. The corrosion/wear mechanisms of Ti-6Al-4 V alloy for different scratching rates10.1016/j.wear.2006.11.025 ↗
46. Tribocorrosion behaviour of overlay welded Ni-Cr 625 alloy in sulphuric and nitric acids: electrochemical and chemical effects10.1016/j.triboint.2009.12.009 ↗
47. Interstitial Oxygen diffusion hardening – a practical route for the surface protection of titanium10.1016/j.matchar.2011.10.012 ↗
48. A study of the potentials achieved during mechanical abrasion and the repassivation rate of titanium and Ti6Al4 V in inorganic buffer solutions and bovine serum10.1016/j.electacta.2004.07.024 ↗
49. Hutchings · 1992
50. Corrosion and wear resistance of 32CrMoV13 steel nitrided by plasma10.1039/C4RA08326A ↗
51. Corrosion behaviour of Al-brass alloy during erosion –corrosion process: effects of jet velocity and sand concentration10.1002/maco.201508511 ↗