Alloy design employing high Cr concentrations for Mo-free stainless steels with enhanced corrosion resistance
Source abstract
Abstract
Abstract In this study, we demonstrate the strategic replacement of Mo with excess Cr in Fe-Cr alloys and report their corrosion resistances. To better understand pitting corrosion, the electrochemical properties of the passive films observed on different alloys (Fe-20Cr-2Mo and Fe-25Cr) were compared. Mo-free Fe-25Cr offered comparable or better pitting corrosion resistance than Fe-20Cr-2Mo during film breakdown, repassivation, and pit propagation stages. We investigated the reason for enhanced stability against pitting corrosion as a result of Mo exclusion in such alloys. Mo accelerated co-dissolution of Fe and Mo itself, consequently enriching Cr on the surface and ultimately promoting onset of passivity.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Corrosion Behavior and Inhibition · High-Temperature Coating Behaviors
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (63)
Show source-provided references
1. Über das austenitischer Chrom-Nickel-(Molybd än-) Stähle mit und ohne Stickstoffzusatz unter besonderer Berücksichtigung ihrer Beanspruchbarkeit in chloridhaltigen Lösungen
2. Gunn · 1997
3. The effect of phase compositions on the pitting corrosion of 25 Cr duplex stainless steel in chloride solutions10.1016/0010-938X(96)00022-4 ↗
4. What does the pitting resistance equivalent really tell us?10.1016/1350-6307(95)00026-7 ↗
5. Development of a lean duplex stainless steel10.1002/srin.200806154 ↗
6. The role of molybdenum additions to austenitic stainless steels in the inhibition of pitting in acid chloride solutions10.1016/0010-938X(77)90032-4 ↗
7. Influence of molybdenum on passivation of polarised stainless steels in a chloride environment10.1016/S0010-938X(01)00072-5 ↗
8. Influence of Ni, Mo, and Cr on pitting corrosionof steels studied by Raman spectroscopy10.5006/1.3315974 ↗
9. Pitting corrosion behaviour of austenitic stainless steels – combining effects of Mn and Mo additions10.1016/j.corsci.2008.04.005 ↗
10. The role of molybdenum in the crevice corrosion of stainless steels10.1016/0010-938X(81)90031-7 ↗
11. On the conduction mechanisms of passive films on molybdenum-containing stainless steel10.5006/1.3584893 ↗
12. An X-ray photo-electron spectroscopic study on the role of molybdenum in increasing the corrosion resistance of ferritic stainless steels in HC110.1016/0010-938X(79)90003-9 ↗
13. The point defect model for the passive state10.1149/1.2069096 ↗
14. The effect of air exposure on the corrosion behavior of amorphous Fe-8Cr-Mo-13P-7C alloys in 1 M HCl10.1016/0010-938X(95)00035-I ↗
15. The role of Mo in the chemical composition and semiconductive behaviour of oxide films formed on stainless steels10.1016/S0010-938X(98)00126-7 ↗
16. The corrosion behavior of amorphous Fe-Cr-Mo-P-C and Fe-Cr-W-P-C alloys in 6 M HCl solution10.1016/0010-938X(92)90147-U ↗
17. Quantitative analysis of repassivation kinetics of ferritic stainless steels based on the high field ion conduction model10.1016/S0013-4686(99)00415-6 ↗
18. Prediction of stress corrosion cracking susceptibility of stainless steels based on repassivation kinetics10.5006/1.3280519 ↗
19. Test techniques for pitting and crevice corrosion resistance of stainless steels and nickel-base alloys in chloride-containing environments10.1179/095066087790150313 ↗
20. Electrochemical measurement of the crevice corrosion propagation resistance of stainless steels: effect of environmental variables and alloy content
21. Shugar · 1981
22. Ahn · 2015
23. Effects of EDTA on the electronic properties of passive film on Fe–20Cr in pH 8.5 buffer solution10.1016/j.electacta.2004.12.012 ↗
24. Observation of passive films on Fe–20Cr–xNi (x=0, 10, 20wt.%) alloys using TEM and Cs-corrected STEM–EELS10.1016/j.corsci.2013.10.023 ↗
25. Effects of cyclic stress on the metastable pitting characteristic for 304 stainless steel under potentiostatic polarization10.1016/j.corsci.2015.01.009 ↗
26. The metastable pitting potential and its relation to the pitting potential for four materials in chloride solutions10.1016/j.corsci.2013.11.015 ↗
27. The nucleation and growth of corrosion pits on stainless steel10.1016/0010-938X(93)90133-2 ↗
28. Aspects of the effects of electrolyte composition on the occurrence of metastable pitting on stainless steel10.1016/0010-938X(94)90041-8 ↗
29. The role of alloyed molybdenum in the inhibition of pitting corrosion in stainless steels10.1016/S0010-938X(00)00086-X ↗
30. The effect of temperature on the nucleation of corrosion pits on titanium in Ringer’s physiological solution10.1016/j.biomaterials.2004.02.023 ↗
31. Development of high Mn–N duplex stainless steel for automobile structural components10.1016/j.corsci.2007.07.004 ↗
32. Growth of passivating films on scratched 304L stainless steel in alkaline solution10.1016/0010-938X(83)90111-7 ↗
33. The effects of pH on the repassivation of 304L stainless steel10.1016/0010-938X(83)90049-5 ↗
34. The coupled kinetics of film growth and dissolution of stainless steel repassivating in acid solutions10.1016/0010-938X(84)90070-2 ↗
35. Effects of alloyed molybdenum on the kinetics of repassivation on austenitic stainless steels10.1016/0010-938X(84)90071-4 ↗
36. Theory of the oxidation of metals10.1088/0034-4885/12/1/308 ↗
37. Die Konstanz der Dielektrizitätskonstanten bei extrem hohen Feldstärken10.1007/BF01375540 ↗
38. Electrolytic conduction of a solid insulator at high fields the formation of the anodic oxide film on aluminium10.1016/S0031-8914(35)90193-8 ↗
39. Kinetics of repassivation of scratch scars generated on iron in aqueous solutions10.5006/1.3593924 ↗
40. Demonstration of crevice corrosion in alkaline solution without acidification10.1149/1.2086211 ↗
41. The role of chloride ions in the IR& IR* criterion for crevice corrosion in iron10.1149/1.2085386 ↗
42. On electric field induced breakdown of passive films and the mechanism of pitting corrosion10.1149/1.2221108 ↗
43. Transport processes and the mechanism of pitting of metals10.1149/1.2132857 ↗
44. Pitting corrosion of metals10.5006/0010-9312-19.8.261 ↗
45. The dissolution and passivation kinetics of stainless alloys containing molybdenum—I. Coulometric studies of Fe-Cr and Fe-Cr-Mo alloys10.1016/0010-938X(85)90111-8 ↗
46. The dissolution and passivation kinetics of stainless alloys containing molybdenum—II. Dissolution kinetics in artificial pits10.1016/0010-938X(85)90112-X ↗
47. Metastable pitting corrosion of stainless steel and the transition to stability10.1098/rsta.1992.0114 ↗
48. Growth of corrosion pits on stainless steel in chloride solution containing dilute sulphate10.1016/0010-938X(92)90191-5 ↗
49. Surface composition of stainless steels during anodic dissolution and passivation studied by ESCA10.1149/1.2113683 ↗
50. Photoelectrochemical study of passive films on stainless steel in neutral solutions10.1016/0013-4686(91)85260-E ↗
51. The electronic structure of passive films formed on stainless steels10.1016/0010-938X(95)00084-W ↗
52. Chemical composition and electronic structure of passive films formed on alloy 600 in acidic solution10.1016/j.corsci.2007.11.006 ↗
53. Semiconducting properties of passive films formed on nickel–base alloys type alloy 600: influence of the alloying elements10.1016/S0013-4686(98)00372-7 ↗
54. Surface physico-chemistry study of an austenitic stainless steel: effect of simple cold rolling treatment on surface contamination10.1016/j.corsci.2006.12.016 ↗
55. A round robin on combined electrochemical and AES/ESCA characterization of the passive films on Fe-Cr and Fe-Cr-Mo alloys10.1016/0010-938X(88)90026-1 ↗
56. Pourbaix · 1966
57. Case-histories of corrosion in industrial boilers
58. Proc. U.K
59. Intergranular corrosion of austenitic stainless steel10.1149/1.2407966 ↗
60. Why stainless steel corrodes10.1038/415770a ↗
61. Explanation for initiation of pitting corrosion of stainless steels at sulfide inclusions10.1149/1.1393431 ↗
62. Influence of sulfide inclusions on the pitting corrosion of steels10.5006/0010-9312-28.10.388 ↗
63. Effects of Mn on the localized corrosion behavior of Fe–18Cr alloys10.1016/j.electacta.2010.01.006 ↗