journal article·2013-02

The influence of hydrogen on 3.5NiCrMoV steel studied using the linearly increasing stress test

Qian Liu, Bartolomeus Irwanto, Andrej Atrens

Corrosion Science· Volume 67
Publisher page

Abstract

The linearly increasing stress test (LIST) was used to study the influence of hydrogen on 3.5NiCrMoV steel in acidified 0.1M NaSO, pH 2 at increasingly negative applied potentials to -1700mV. For specimens tested in solution with an applied potential, there were surface cracks in the necked region, but no surface cracks in the uniformly deformed part of the specimen. This implies that there was no influence of hydrogen up to the yield stress of the steel. Hydrogen induced brittle fracture events made a small contribution to the overall ductile fracture, which occurred after the onset of necking.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Corrosion Behavior and Inhibition · Non-Destructive Testing Techniques

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (61)

Show source-provided references
1. R.P. Gangloff, B.P. Somerday (Eds.), Gaseous Hydrogen Embrittlement for Materials in Energy Technologies, Woodhead, 2011.10.1533/9780857095374 ↗
2. Effect of hydrogen and inclusions on the tensile properties and fracture behaviour of A350LF2 steels after exposure to wet H2S environments10.1016/j.corsci.2012.04.012 ↗
3. An evaluation of steels subjected to rock bolt SCC conditions10.1016/j.engfailanal.2006.11.006 ↗
4. Effect of hydrogen on the fracture behavior of high strength steel during slow strain rate test10.1016/j.corsci.2007.03.038 ↗
5. Comparison of hydrogen embrittlement in three pipeline steels in high pressure gaseous hydrogen environments10.1016/j.corsci.2012.01.028 ↗
6. Effect of bainitic microstructure on the susceptibility of pipeline steels to hydrogen induced cracking10.1016/j.msea.2011.03.036 ↗
7. Effect of hydrogen on the properties and fracture characteristics of TRIP 800 steels10.1016/j.corsci.2011.04.015 ↗
8. Effect of microstructure and inclusions on hydrogen induced cracking susceptibility and hydrogen trapping efficiency of X120 pipeline steel10.1016/j.msea.2010.07.022 ↗
9. Effect of microstructure on the hydrogen trapping efficiency and hydrogen induced cracking of linepipe steel10.1016/j.corsci.2008.03.007 ↗
10. Hydrogen effects on cathodically charged twinning-induced plasticity steel10.1016/j.scriptamat.2011.12.012 ↗
11. Hydrogen effects on nanovoid nucleation in face-centered cubic single-crystals10.1016/j.actamat.2007.09.012 ↗
12. Hydrogen embrittlement in a Fe–Mn–C ternary twinning-induced plasticity steel10.1016/j.corsci.2011.09.022 ↗
13. Hydrogen embrittlement of 4340 steel due to condensation during vaporized hydrogen peroxide treatment10.1016/j.msea.2011.01.100 ↗
14. Hydrogen embrittlement risk of high strength galvanized steel in contact with alkaline media10.1016/j.corsci.2011.05.023 ↗
15. Hydrogen embrittlement susceptibility of a high strength steel X8010.1016/j.msea.2010.07.027 ↗
16. Hydrogen embrittlement susceptibility of tempered 9%Cr–1%Mo steel10.1016/j.ijhydene.2011.08.096 ↗
17. Hydrogen environment embrittlement of an ODS RAF steel – Role of irreversible hydrogen trap sites10.1016/j.ijhydene.2010.06.071 ↗
18. Hydrogen-enhanced local plasticity at dilute bulk H concentrations: the role of H–H interactions and the formation of local hydrides10.1016/j.actamat.2011.01.037 ↗
19. Internal and surface damage of multiphase steels and pure iron after electrochemical hydrogen charging10.1016/j.corsci.2011.05.060 ↗
20. D. Pérez Escobar, L. Duprez, A. Atrens, K. Verbeken, Thermal desorption spectroscopy study of experimental Ti/S containing steels, Materials Science and Technology, http://dx.doi.org/10.1179/1743284712Y.0000000141.10.1179/1743284712Y.0000000141 ↗
21. Thermal desorption spectroscopy study of the interaction between hydrogen and different microstructural constituents in lab cast Fe–C alloys10.1016/j.corsci.2012.08.017 ↗
22. Measurement and modeling of hydrogen environment-assisted cracking of ultra-high-strength steel10.1007/s11661-006-9051-z ↗
23. A nanoscale mechanism of hydrogen embrittlement in metals10.1016/j.actamat.2010.11.019 ↗
24. On the role of crystallographic texture in mitigating hydrogen-induced cracking in pipeline steels10.1016/j.corsci.2011.08.031 ↗
25. On the stress corrosion cracking and hydrogen embrittlement of sensitized austenitic stainless steels in boiling saturated magnesium chloride solutions: effect of applied stress10.1016/j.corsci.2008.06.053 ↗
26. Recent developments in the study of hydrogen embrittlement: hydrogen effect on dislocation nucleation10.1016/j.actamat.2010.05.057 ↗
27. Role of drawing-induced residual stresses and strains in the hydrogen embrittlement susceptibility of prestressing steels10.1016/j.corsci.2011.06.012 ↗
28. The role of hydrogen and other interstitials in the mechanical behaviour of metals
29. Hydrogen embrittlement failure of hot dip galvanised high tensile wires10.1016/S1350-6307(98)00038-7 ↗
30. Hydrogen-plasticity interactions in pearlitic steel: a fractographic and numerical study10.1016/S0921-5093(96)10425-1 ↗
31. Hydrogen-enhanced localized plasticity – a mechanism for hydrogen-related fracture10.1016/0921-5093(94)90975-X ↗
32. Woodhead · 2011 · 158
33. Influence of the applied stress rate on the stress corrosion cracking of 4340 and 3.5NiCrMoV steels under conditions of cathodic hydrogen charging10.1016/j.corsci.2011.03.028 ↗
34. The influence of applied stress rate on the stress corrosion cracking of 4340 and 3.5NiCrMoV steels in distilled water at 30°C10.1016/j.corsci.2009.11.033 ↗
35. Hydrogen embrittlement and rock bolt stress corrosion cracking10.1016/j.engfailanal.2008.01.004 ↗
36. Metallurgical aspects of rock bolt stress corrosion cracking10.1016/j.msea.2007.11.086 ↗
37. Material influence on the stress corrosion cracking of rock bolts10.1016/j.engfailanal.2004.07.002 ↗
38. Stress corrosion cracking fracture mechanisms in rock bolts10.1023/A:1025996620197 ↗
39. Environmental influence on the stress corrosion cracking of rock bolts10.1016/S1350-6307(03)00036-0 ↗
40. The initiation and propagation of stress corrosion cracking in AISI 4340 and 3.5 Ni–Cr–Mo–V rotor steel in constant load tests10.1016/0010-938X(96)00010-8 ↗
41. The stress corrosion cracking of as-quenched 4340 and 3.5NiCrMoV steels under stress rate control in distilled water at 90°C10.1016/0010-938X(93)90235-9 ↗
42. The role of crack tip strain rate in the stress corrosion cracking of high strength steels in water10.1007/BF02651655 ↗
43. Initiation of stress corrosion cracking for pipeline steels in a carbonate-bicarbonate solution10.1007/BF02652362 ↗
44. Environmental assisted fracture for 4340 steel in water and air of various humidities10.1023/A:1018659226945 ↗
45. Stress corrosion crack propagation in AerMet 10010.1023/A:1004362400904 ↗
46. Linearly-increasing-stress testing of carbon steel in 4 N NaNO3 and in Bayer liquor10.1023/A:1004314517742 ↗
47. ESEM observations of SCC initiation for 4340 high strength steel in distilled water10.1023/A:1004328031430 ↗
48. The crack tip strain field of AISI 4340 Part III hydrogen influence10.1023/A:1004751420033 ↗
49. The crack tip strain field of AISI 4340 Part II experimental measurements10.1023/A:1004799303195 ↗
50. The crack tip strain field of AISI 4340 Part I Measurement technique10.1023/A:1004747219124 ↗
51. Analysis of service stress corrosion cracking in a natural gas transmission pipeline, active or dormant?10.1016/j.engfailanal.2003.08.001 ↗
52. Linearly increasing stress test (LIST) for SCC research10.1088/0957-0233/4/11/017 ↗
53. SCC of commercial steels exposed to high hydrogen fugacity10.1016/j.engfailanal.2007.10.004 ↗
54. Influence of tensile straining on the permeation of hydrogen in low alloy Cr–Mo steels10.1016/j.corsci.2005.01.007 ↗
55. Theoretical study of hydrogen transport during plastic deformation in iron10.1016/0001-6160(88)90252-0 ↗
56. Comparison of the linearly increasing stress test and the constant extension rate test in the evaluation of transgranular stress corrosion cracking of magnesium10.1016/j.msea.2007.03.021 ↗
57. Electrochemical studies of hydrogen diffusion and permeability in Ni10.1016/0010-938X(80)90102-X ↗
58. The cooperative relation between temper embrittlement and hydrogen embrittlement in a high strength steel10.1007/BF02644103 ↗
59. The equivalent pressure of molecular hydrogen in cavities within metals in terms of the overpotential developed during the evolution of hydrogen10.1016/0013-4686(71)85027-2 ↗
60. Materials needs in the energy industry
61. Progress in the design of an improved high-temperature 1-percent CrMoV rotor steel10.1115/1.2903194 ↗