Stress corrosion cracking of A537 steel in simulated marine environments
Source abstract
Abstract
Slow strain rate testing showed that stress corrosion cracking (SCC) of A537 steels could occur in both simulated seawater and alternating wet–dry environments. The SCC mechanism was anodic dissolution (AD) under anode polarization and open circuit potential, and hydrogen induced cracking (HIC) under cathode polarization with high potential difference. The additive stress σp, induced by the corrosion process controlled susceptibility to SCC, regardless of the AD mechanism or HIC under either anodic or cathodic polarization conditions. SCC initiated at the interface between matrix and MnS inclusions, which was as anodic phases to promote the AD process.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Corrosion Behavior and Inhibition · Concrete Corrosion and Durability
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (39)
Show source-provided references
1. Statistical characterization of surfaces of corroded steel plates
2. Mechanistic features of short fatigue crack growth kinetics for high strength steels in sea water10.1115/1.2185127 ↗
3. Crack growth retardation of single overload for A537 steel in a 3.5% NaCl solution under cathodic potential and free corrosion condition10.1016/S0142-1123(97)00115-1 ↗
4. Anisotropic 3D growth of corrosion pits initiated at MnS inclusions for A537 steel during corrosion fatigue10.1016/j.corsci.2010.04.036 ↗
5. Studies of stress corrosion of high-strength structural steels exposed to seawater10.1002/maco.19960470103 ↗
6. Stress corrosion cracking of low alloy steels and welded joins in sea water
7. The effect of strain-rate and cathodic potential on the tensile ductility of X-65 pipeline steel10.1016/0010-938X(83)90110-5 ↗
8. Effect of cathodic protection on fracture behaviour of low alloy steels in seawater
9. Determination of tensile stress induced by dezincification layer during corrosion for brass10.1016/S0010-938X(98)00063-8 ↗
10. The correspondence between susceptibility to SCC of brass and corrosion-induced tensile stress with various pH values10.1016/S0010-938X(02)00055-0 ↗
11. Study on the role of tarnishing film in stress corrosion cracking of brass in Mattsson’s solution10.1557/JMR.2010.0120 ↗
12. Film-induced tensile stress during corrosion
13. Inhibitive effects and mechanism of phosphates on the stress corrosion cracking of brass in ammonia solutions10.1016/j.corsci.2012.04.011 ↗
14. Study of correlation between hydrogen-induced stress and hydrogen embrittlement10.1016/S0921-5093(02)00600-7 ↗
15. ASTM D1141-98 · 2003
16. Hydrogen induced slow crack growth in stable austenitic stainless steels10.1007/BF02644204 ↗
17. Hydrogen accumulation and hydrogen-induced cracking of API C90 tubular steel10.5006/1.3290260 ↗
18. On the atmospheric corrosion of metal which are covered with thin electrolyte layers—I. Verification of the experimental technique10.1016/0010-938X(90)90032-Z ↗
19. Application of a kelvin microprobe to the corrosion of metals in humid atmospheres
20. Application of a Kelvin microprobe to the corrosion of metals in humid atmospheres
21. Passivity breakdown of high purity iron and AISI 4340 steel in 0.5M NaCl solution10.1016/0010-938X(76)90115-3 ↗
22. Mechanistic aspect of near-neutral pH stress corrosion cracking of pipelines under cathodic polarization10.1016/j.corsci.2011.10.002 ↗
23. Influence of the applied stress rate on the stress corrosion cracking of 4340 and 3.5NiCrMoV steels under conditions of cathodic hydrogen charging10.1016/j.corsci.2011.03.028 ↗
24. On a role of hydrogen-induced ε-martensite in embrittlement of stable austenitic steel10.1016/S1359-6462(03)00338-5 ↗
25. Hydrogen induced cracking (HIC) testing of low alloy steel in sour environment: impact of time of exposure on the extent of damage10.1016/j.corsci.2009.11.044 ↗
26. On the extension of CP models to address cathodic protection under a delaminated coating10.1016/j.corsci.2009.01.023 ↗
27. Corrosion products of reinforcement in concrete in marine and industrial environments10.1016/j.matchemphys.2008.09.063 ↗
28. Interpretation of electrochemical potentiokinetic reactivation data in the presence of sulphide/oxysulphide inclusions in 316LN stainless steel10.1016/j.corsci.2011.05.065 ↗
29. The role of TiN inclusions in stress corrosion crack initiation for Alloy 690TT in high-temperature and high-pressure water10.1016/j.corsci.2009.11.015 ↗
30. Hydrogen trapping on non metallic inclusions in Cr–Mo low alloy steels10.1016/S0010-938X(98)00008-0 ↗
31. Szklarska-Smialowska · 2005
32. Effect of sulphide inclusions in a commercial stainless steel on the nucleation of corrosion pits10.1016/S0010-938X(69)80048-X ↗
33. Recurrent studies of chloride ingress in uncracked marine concrete at various exposure times and elevations10.1016/S0008-8846(98)00124-0 ↗
34. Suitability of sea water for mixing structural concrete exposed to a marine environment10.1016/0958-9465(95)00015-5 ↗
35. The work function of the elements and its periodicity10.1063/1.323539 ↗
36. Variations of work function and corrosion behaviors of deformed copper surfaces10.1016/j.apsusc.2004.07.017 ↗
37. Micro-electrochemical characterization of corrosion of welded X70 pipeline steel in near-neutral pH solution10.1016/j.corsci.2009.04.030 ↗
38. On corrosion-induced stress states in binary noble metal alloys10.1016/S0921-5093(97)00098-1 ↗
39. Molecular dynamics simulation of porous layer-induced stress in Fe single crystal10.1016/j.commatsci.2010.06.006 ↗