Chloride-induced corrosion of steel embedded in mortars containing fly ash and spent cracking catalyst
Source abstract
Abstract
Stationary and non-stationary chloride diffusion coefficients of mortars prepared with ordinary Portland cement partially substituted by spent cracking catalyst (FC3R) and fly ash (FA) have been determined. An accelerated test of chloride migration through the mortar has been performed in order to determine these coefficients. The results show that the presence of FC3R improves chloride binding properties of mortars and the addition of FA reduces the total porosity, both factors leading to a higher resistance to chloride ingress. Corrosion rate of steels embedded in these ternary-binder mortars do not show significant differences compared to reference mortars (with plain cement), so a combined cement substitution as high as 45% by FC3R and FA do not lead to a higher risk of chloride-induced corrosion of steel when tested at an early age.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Concrete Corrosion and Durability · Concrete and Cement Materials Research · Corrosion Behavior and Inhibition
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (31)
Show source-provided references
1. Chloride attack of reinforced concrete: an overview10.1007/BF02473172 ↗
2. Spent FCC catalyst as a pozzolanic material for high-performance mortars10.1016/S0958-9465(03)00048-9 ↗
3. Oil cracking waste catalyst as an active pozzolanic material for superplasticized mortars10.1016/S0008-8846(01)00693-7 ↗
4. Modification of the properties of concrete by a new pozzolan: a waste catalyst from the catalytic process in a fluidized bed10.1016/S0008-8846(01)00646-9 ↗
5. Effect of waste aluminosilicate material on cement hydration and properties of cement mortars10.1016/S0008-8846(02)00873-6 ↗
6. Fluid catalytic cracking catalyst residue (FC3R): an excellent mineral by-product for improving early-strength development of cement mixtures10.1016/S0008-8846(99)00164-7 ↗
7. Advantages in the use of fly ashes in cements containing pozzolanic combustion residues: silica fume, sewage sludge ash, spent fluidized bed catalyst and rice husk ash10.1002/jctb.583 ↗
8. Evaluation of the pozzolanic activity of fluid catalytic cracking residue (FCC): thermogravimetric analysis studies on FCC-portland cement pastes10.1016/S0008-8846(02)01026-8 ↗
9. The effect of waste oil-cracking catalyst on the compressive strength of cement pastes and mortars10.1016/S0008-8846(02)01006-2 ↗
10. Subproducto del fraccionamiento catalítico del petróleo: características, actividad puzolánica y su efecto en las propiedades del mortero
11. Effect of fly ash in concrete on the corrosion of steel reinforcement
12. A model for predicting carbonation of high-volume fly ash concrete10.1016/S0008-8846(00)00227-1 ↗
13. Mechanical treatment of fly ashes. Part I: physico-chemical characterization of ground fly ashes10.1016/0008-8846(95)00141-X ↗
14. Mechanical treatment of fly ashes. Part II: particle morphologies in ground fly ashes (GFA) and workability of GFA-cement mortars10.1016/0008-8846(95)00212-X ↗
15. Comparisons among magnetic and non-magnetic fly ash fractions: strength development of cement-fly ash mortars10.1016/S0956-053X(96)00034-7 ↗
16. Mechanical treatment of fly ashes. Part III: studies on strength development of ground fly ashes (GFA)-cement mortars10.1016/S0008-8846(97)00129-4 ↗
17. Mechanical treatment of fly ashes. Part IV: strength development of ground fly ash cement mortars cured at different temperatures10.1016/S0008-8846(00)00218-0 ↗
18. Calculation of chloride diffusion coefficients in concrete from ionic migration measurements10.1016/0008-8846(93)90023-3 ↗
19. Measurement of the steady and non-steady chloride diffusion coefficients in a migration test by means of monitoring the conductivity in the anolyte chamber. Comparison with natural diffusion tests10.1016/S0008-8846(01)00562-2 ↗
20. A theoretical analysis of the shape of polarization curves10.1149/1.2428496 ↗
21. Determination of the pozzolanic activity of fluid catalytic cracking residue. Thermogravimetric analysis studies on FC3R-lime pastes10.1016/S0008-8846(03)00014-0 ↗
22. Two experimental methods to determine carbonation profiles in concrete
23. 1969
24. Thermogravimetric investigation on the chloride binding behaviour of MK-lime paste10.1016/j.tca.2006.02.012 ↗
25. Mechanism of Friedel’s salt formation in cements rich in tricalcium aluminate10.1016/S0008-8846(96)85009-5 ↗
26. Studies using 27Al MAS NMR of AFm and AFt and the formation of Friedel’s salt10.1016/S0008-8846(02)00901-8 ↗
27. Accelerated carbonation of Friedel’s salt in calcium aluminate paste10.1016/S0008-8846(02)00910-9 ↗
28. Stability of Friedel’s salt in carbonated concrete structural elements10.1016/S0008-8846(96)85010-1 ↗
29. A model for predicting carbonation of high-volume fly ash concrete10.1016/S0008-8846(00)00227-1 ↗
30. The influence of mix parameters and binder choice on the carbonation of cement solidified wastes10.1016/S0956-053X(97)00021-4 ↗
31. Techniques electrochimiques qualitatives et quantitatives pour mésurer les effects des additions sur la corrosion des armatures