Corrosion of nickel–chromium alloys, stainless steel and niobium at supercritical water oxidation conditions
Source abstract
Abstract
Abstract Results of immersion tests of UNS N06625 (alloy 625), UNS S31609 (alloy 316 L), Ni–20Cr alloy and Nb coupons exposed to oxygenated ammoniacal sulphate solution at supercritical water oxidation (SCWO) conditions are presented. The corrosion behavior of the alloy 316 L (UNS S31603) SCWO reactor tubing is also presented under the same conditions. Immersion coupons corroded at a rate not exceeding 40 mm yr−1 while the reactor tube itself corroded at a rate of between 160–1500 mm yr−1, depending on which length of the reactor is considered to have corroded. Morphological and chemical analysis of the oxides present on the coupon samples suggest that iron oxides, which had initially precipitated on the corroding alloy 316 tube surface, were removed by heat flux-driven fluid mechanical action and transported through the reactor where they deposited on the coupons. Niobium was resistant to corrosion at the tested conditions.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Subcritical and Supercritical Water Processes · Environmental remediation with nanomaterials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (27)
Show source-provided references
1. Supercritical water oxidation: state of the art10.1002/(SICI)1521-4125(199911)22:11<903::AID-CEAT903>3.0.CO;2-E ↗
2. I. Vera-Perez, Supercritical water oxidation of phenol and 2,4 dinitrophenol, Masters Thesis, The University of British Columbia, 2002.
3. Thermodynamics of the corrosion of alloy 625 supercritical water oxidation reactor tubing in ammoniacal sulphate solution10.5006/1.3278474 ↗
4. Factors controlling corrosion in high-temperature aqueous solutions: a contribution to the dissociation and solubility data influencing corrosion processes10.1016/S0896-8446(99)00009-1 ↗
5. A mechanistic study of silicon etching in NH3/H2O2 cleaning solutions10.1149/1.2086639 ↗
6. Decolorization of synthetic dyes by hydrogen peroxide with heterogeneous catalysis by mixed iron oxides10.1016/j.apcatb.2006.04.001 ↗
7. Two-stage peroxide bleaching of eucalypt-SGW with chromium catalysts10.1080/02773819108050278 ↗
8. J.T. Burton, L.L. Campbell, Hydrogen peroxide decomposition by metal catalysts: bad actors in a bleaching stage, in: Proceedings of the 1985 International Symposium on Wood and Pulping Chemistry, American Chemical Society, Vancouver, BC, 1985, pp. 255–259.
9. Stainless steel flow reactor for supercritical water oxidation: corrosion tests10.1016/S0896-8446(02)00264-4 ↗
10. N. Boukis, C. Friedrich, W. Habicht, M. Schacht, E. Dinjus, Corrosion screening tests in supercritical water containing hydrochloric acid and oxygen, in: Proceedings of Eurocorr 1997, Event No. 208, European Federation of Corrosion, Trondheim, Norway, vol. 1, 1997, pp. 617–622.
11. M. Son, Y. Kurata, Y. Ikushima, Corrosion behavior of metals in SCW environments containing salts and oxygen, Corrosion, 2002, Paper No. 02357, NACE International.
12. An assessment of supercritical water oxidation (SCWO) existing problems, possible solutions and new reactor concepts10.1016/S1385-8947(00)00255-2 ↗
13. Transpassive dissolution of alloy 625, chromium, nickel and molybdenum in high temperature solutions containing hydrochloric acid and oxygen10.5006/1.3287652 ↗
14. Review of the corrosion of nickel-based alloys and stainless steels in strongly oxidizing pressurized high-temperature solutions at subcritical and supercritical temperatures10.5006/1.3294394 ↗
15. Corrosion of alloy 625 in high-temperature, high pressure sulphate solutions10.5006/1.3284888 ↗
16. Effect of oxygen on the corrosion behavior of alloy 625 from 25 to 200 degrees C10.1149/1.2435620 ↗
17. K. Sue, N. Tsujinaka, T. Adschiri, K. Arai, Y. Watanabe, Relationship between corrosion rate and metal oxide solubility in supercritical water, Corrosion, 2002, Paper No. 02354, NACE International.
18. Oxidation of simple compounds and mixtures in supercritical water: carbon monoxide, ammonia, and ethanol10.1021/es00176a012 ↗
19. Oxidation kinetics of ammonia and ammonia–methanol mixtures in supercritical water in the temperature range 530–700°C at 246 bar10.1021/ie00056a010 ↗
20. Bjerrum · 1957
21. Polarization Study of Alloy 625, Ni, Cr and Mo in Ammoniated Sulphate Solutions10.5006/1.3278193 ↗
22. The point defect model for the passive state10.1149/1.2069096 ↗
23. C. Shroer, J. Konys, J. Novotny, J. Hausselt, Corrosion investigations on binary and ternary Ni–Cr alloys in SCWO systems, Corrosion, 2002, Paper No. 02359, NACE International.
24. Oxidation of 316 stainless steel in supercritical water10.1016/j.corsci.2009.03.008 ↗
25. The high temperature aqueous corrosion of ferritic steels: effect of heat flux on corrosion and magnetite deposition10.1016/0010-938X(90)90054-9 ↗
26. A.H. Harvey, A.P. Peskin, S.A. Klein, NIST Standard Reference Database 10, NIST/ASME Steam Properties Database.
27. The corrosion of niobium in oxidizing sub- and supercritical aqueous solutions of HCl and H2SO410.1023/A:1006660906845 ↗