Corrosion behavior of selected Mn+1AXn phases in hot concentrated HCl solution: Effect of A element and MX layer
Source abstract
Abstract
Reactivity and stability of selected nanolaminated carbides/nitrides (MAX phases) in a concentrated HCl solution are investigated under hydrothermal conditions. The reactivity of the MAX phases strongly depends on the reactivity of A element (Al or Si) with the acid. Al-containing MAX phases suffered severe corrosion, whereas Si-containing Ti3SiC2 survived. For these MAX phases, the reactivity correlates well with the basic structural unit (MX layers). The thicker the MX layers, the less the reactivity is. For carbides, the stability order under hydrothermal condition is TiC > Ti3AlC2 > Ti2AlC. For nitrides, it is TiN > Ti4AlN3 > Ti2AlN. A mechanism is proposed for understanding this interesting phenomenon. (c) 2012 Elsevier Ltd. All rights reserved.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: MXene and MAX Phase Materials · Advanced ceramic materials synthesis · Aluminum Alloys Composites Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (39)
Show source-provided references
1. The MN+1AXN phases: a new class of solids; thermodynamically stable nanolaminates10.1016/S0079-6786(00)00006-6 ↗
2. The Mn+1AXn phases: materials science and thin-film processing10.1016/j.tsf.2009.07.184 ↗
3. Ab initio geometry optimization and ground state properties of layered ternary carbides Ti3MC2 (M=Al, Si and Ge)10.1088/0953-8984/13/44/313 ↗
4. Investigation on reliability of nanolayer-grained Ti3SiC2 via Weibull statistics10.1007/s10853-006-0427-7 ↗
5. Microstructure and properties of Ti3AlC2 prepared by the solid–liquid reaction synthesis and simultaneous in situ hot pressing process10.1016/S1359-6454(02)00117-9 ↗
6. Calculated elastic properties of M2AlC (M=Ti, V, Cr, Nb and Ta)10.1016/j.ssc.2003.12.008 ↗
7. High-temperature oxidation behavior of Ti2AlC in air10.1023/A:1023092027697 ↗
8. Oxidation behavior of Ti3AlC2 at 1000–1400°C in air10.1016/S0010-938X(02)00177-4 ↗
9. Layered machinable and electrically conductive Ti2AlC and Ti3AlC2 ceramics: a review10.1016/S1005-0302(10)60064-3 ↗
10. Progress in research and development on MAX phases: a family of layered ternary compounds10.1179/1743280410Y.0000000001 ↗
11. Hot corrosion and protection of Ti2AlC against Na2SO4 salt in air
12. Hot corrosion of Na2SO4-coated Ti3AlC2 in air at 700–1000 °C10.1149/1.1778171 ↗
13. Corrosion penetration monitoring of advanced ceramics in hot aqueous fluids10.1590/S1516-14392004000100017 ↗
14. Effect of Al dopant on the hydrothermal oxidation behavior of Ti3SiC2 powders10.1016/j.jeurceramsoc.2008.12.010 ↗
15. Mechanisms and kinetics of the hydrothermal oxidation of bulk titanium silicon carbide10.1111/j.1551-2916.2009.03570.x ↗
16. Experimental and thermodynamic study of the hydrothermal oxidation behavior of Ti3SiC2 powders10.1016/j.scriptamat.2008.06.005 ↗
17. Hydrothermal oxidation behavior of bulk titanium aluminum carbide10.1111/j.1551-2916.2011.04590.x ↗
18. Corrosion behavior and passive film characteristics formed on Ti, Ti3SiC2, and Ti4AlN3 in H2SO4 and HCl10.1149/1.1637897 ↗
19. Corrosion behavior of Ti3GeC2 and Ti2AlN in 1M NaOH10.1149/1.2199247 ↗
20. Corrosion behavior of select MAX phases in NaOH, HCl and H2SO410.1016/j.corsci.2006.04.005 ↗
21. Corrosion behavior of Ti3AlC2 in NaOH and H2SO410.1016/j.jeurceramsoc.2010.07.002 ↗
22. Solid–liquid reaction synthesis and simultaneous densification of polycrystalline Ti2AlC10.3139/146.020066 ↗
23. Solid–liquid reaction synthesis of layered machinable Ti3AlC2 ceramic10.1039/b108685e ↗
24. Synthesis and microstructure of layered-ternary Ti2AlN ceramic10.1016/j.scriptamat.2007.01.049 ↗
25. A new computer-program for Rietveld analysis of X-ray powder diffraction patterns10.1107/S0021889881008996 ↗
26. Numerical data for some commonly used solid state reaction equations10.1111/j.1151-2916.1966.tb13289.x ↗
27. Raman active phonon modes and heat capacities of Ti2AlC and Cr2AlC ceramics: first-principles and experimental investigations10.1063/1.1873057 ↗
28. Micro-Raman spectroscopic characterization of nanosized TiO2 powders prepared by vapor hydrolysis10.1557/JMR.1998.0363 ↗
29. Raman-spectra of stoichiometric and defect rutile10.1016/0025-5408(91)90104-T ↗
30. Effects of sample orientationon the corrosion of zinc in ammonium sulfate and sodium hydroxide solutions10.1016/0010-938X(91)90089-8 ↗
31. Electronic and structural properties of the layered ternary carbide Ti3AlC210.1039/b101520f ↗
32. Conversion of magnetron deposited TiC films into rutile TiO210.1002/ppap.200500106 ↗
33. First-principles investigation of intrinsic defects and (N, O) impurity atom stimulated Al vacancy in Ti2AlC10.1063/1.3058718 ↗
34. Insights into high temperature oxidation of Al2O3-forming Ti3AlC210.1016/j.corsci.2012.01.011 ↗
35. Structure stability of Ti3AlC2 in Cu and microstructure evolution of Cu–Ti3AlC2 composites10.1016/j.actamat.2007.03.033 ↗
36. A novel method to make tough Ti2AlC/Al2O3- and Ti3AlC2/Al2O3-laminated composites10.1111/j.1551-2916.2010.03989.x ↗
37. Microstructures and adhesion of the oxide scale formed on titanium aluminum carbide substrates10.1111/j.1551-2916.2006.01141.x ↗
38. Corrosion properties of TiC films prepared by activated reactive evaporation10.1016/0257-8972(90)90170-H ↗
39. Influence of solution concentration on the hydrothermal preparation of titania crystallites10.1039/b105907f ↗