Effects of dissolved hydrogen and surface condition on the intergranular stress corrosion cracking initiation and short crack growth behavior of non-sensitized 316 stainless steel in simulated PWR primary water
Source abstract
Abstract
Abstract The effects of dissolved hydrogen (DH) and inner surface finish condition of the hollowed specimen on stress corrosion crack (SCC) initiation and small crack growth behaviors of 316 stainless steel were investigated in high temperature water with various DH levels. The drilled specimen showed higher surface hardness and more enhanced SCC initiation and short crack growth behavior than honed specimen but both showed a similar trend in the water chemistry with different DH levels. Fractographic examinations showed mixed modes of transgranular and intergranular cracking. The influences of DH and surface condition on SCC behaviors are discussed.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Material Properties and Failure Mechanisms · Corrosion Behavior and Inhibition
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (57)
Show source-provided references
1. Stress corrosion cracking of current structural materials in commercial nuclear power plants10.5006/0801 ↗
2. Stress corrosion cracking behavior of alloys in aggressive nuclear reactor core environments10.5006/1.3278331 ↗
3. Intergranular stress corrosion cracking behavior of austenitic stainless steels in hydrogenated high-temperature water10.5006/1.3278254 ↗
4. The hydrogen embrittlement of metals10.1016/0079-6425(61)90005-6 ↗
5. Hydrogen embrittlement of the Ni-base Alloy 600 correlated with hydrogen transport by dislocations10.1016/S0921-5093(98)01006-5 ↗
6. Cathodic hydrogen embrittlement in alloy 71810.1016/S0921-5093(99)00167-7 ↗
7. Effects of hydrogen on the electronic properties and stability of the passive films on iron10.1016/S0169-4332(01)00235-5 ↗
8. Effect of low temperature on hydrogen-assisted crack propagation in 304L/308L austenitic stainless steel fusion welds10.1016/j.corsci.2013.08.004 ↗
9. The effect of permeated hydrogen on the pitting of type 304 stainless steel10.1016/S0010-938X(97)00178-9 ↗
10. Stress corrosion cracking of low-alloy reactor pressure vessel steels under boiling water reactor conditions10.1016/j.jnucmat.2007.03.048 ↗
11. Evaluation of the mitigation effect of hydrogen water chemistry in BWRs on the low-frequency corrosion fatigue crack growth in low-alloy steels10.1016/j.jnucmat.2006.07.023 ↗
12. Effects of hydrogen water chemistry on radiation field buildup in BWRs10.1016/0029-5493(96)01196-X ↗
13. Controlling stress corrosion cracking in boiling water reactors10.1016/0029-5493(93)90279-I ↗
14. Hydrogen water chemistry for BWRs10.1016/0149-1970(87)90011-4 ↗
15. Semiconducting behavior and bandgap energies of oxide films grown on alloy 600 under PWR simulated primary water conditions with different dissolved hydrogen contents10.1016/j.jnucmat.2013.07.044 ↗
16. Influence of dissolved hydrogen on oxide film and PWSCC of alloy 600 in PWR primary water10.1080/18811248.2003.9715330 ↗
17. Primary water SCC understanding and characterization through fundamental testing in the vicinity of the nickel/nickel oxide phase transition
18. Influence of dissolved hydrogen on structure of oxide film on alloy 600 formed in primary water of pressurized water reactors10.1080/18811248.2003.9715385 ↗
19. Corrosion behavior of stainless steels in simulated PWR primary water—effect of chromium content in alloys and dissolved hydrogen10.1080/18811248.2008.9711883 ↗
20. Effect of dissolved hydrogen on the electrochemical behaviour of Alloy 600 in simulated PWR primary water at 290°C10.1016/j.corsci.2011.02.020 ↗
21. Stress corrosion cracking of uni-directionally cold worked 316NG stainless steel in simulated PWR primary water with various dissolved hydrogen concentrations10.1016/j.corsci.2011.04.013 ↗
22. Influence of carbide precipitation and rolling direction on intergranular stress corrosion cracking of austenitic stainless steels in hydrogenated high-temperature water10.5006/1.3280670 ↗
23. The influence of dissolved hydrogen on the corrosion of type 304 stainless steels treated with inhibitive chemicals in high temperature pure water10.1080/18811248.2005.9726414 ↗
24. Hydrogen in chromium: influence on corrosion potential and anodic dissolution in neutral NaCl solution10.1016/S0010-938X(00)00154-2 ↗
25. Influence of hydrogen in iron and in two stainless steels on aqueous and gaseous corrosion10.1149/1.1497399 ↗
26. Effect of hydrogen in Inconel Alloy 600 on corrosion in high temperature oxygenated water10.1016/j.corsci.2009.11.037 ↗
27. A sensitive technique for evaluating susceptibility to IGSCC of alloy 600 in high temperature water10.1016/0036-9748(86)90431-X ↗
28. Activation energy for IGSCC of alloy 600 in an aqueous solution containing dissolved H2 at 300 to 350°C10.1016/0036-9748(87)90404-2 ↗
29. Effect of strain rate on primary water stress corrosion cracking fracture mode and crack growth rate of nickel alloy and austenitic stainless steel10.5006/1.3280631 ↗
30. Technical note hydrogen induced IGSCC of two unsensitized austenitic stainless steels in high-temperature water10.5006/1.3583908 ↗
31. Effect of hydrogen on the intergranular stress corrosion cracking of alloy 600 in high temperature aqueous environments10.5006/1.3583894 ↗
32. Effect of machining-induced surface residual stress on initiation of stress corrosion cracking in 316 austenitic stainless steel10.1016/j.corsci.2016.03.008 ↗
33. Effects of scratching on corrosion and stress corrosion cracking of Alloy 690TT at 58°C and 330°C10.1016/j.corsci.2009.07.015 ↗
34. Dependence of stress corrosion cracking for cold-worked stainless steel on temperature and potential, and role of diffusion of vacancies at crack tips10.5006/1.3278507 ↗
35. Cold work and temperature dependence of stress corrosion crack growth of austenitic stainless steels in hydrogenated and oxygenated high-temperature water10.5006/1.3278329 ↗
36. Effects of water chemistry and loading conditions on stress corrosion cracking of cold-rolled 316NG stainless steel in high temperature water10.1016/j.corsci.2010.09.018 ↗
37. IGSCC of non-sensitized stainless steels in high temperature water10.1016/j.jnucmat.2008.08.005 ↗
38. Stress corrosion cracking behavior of cold-drawn 316 austenitic stainless steels in simulated PWR environment10.1016/j.corsci.2016.08.014 ↗
39. Accelerated test for evaluation of intergranular stress corrosion cracking initiation characteristics of non-sensitized 316 austenitic stainless steel in simulated pressure water reactor environment10.1016/j.corsci.2016.11.019 ↗
40. The stress corrosion cracking of type 316 stainless steel in oxygenated and chlorinated high temperature water10.1016/0010-938X(85)90010-1 ↗
41. The stress corrosion cracking of reactor pressure vessel steel in high temperature water10.1016/0010-938X(85)90003-4 ↗
42. Stress corrosion crack coalescence10.5006/1.3585136 ↗
43. Role of work-hardened surface layer in initiation of environmentally assisted cracking in high-temperature water10.5006/1.3278292 ↗
44. Initiation of environmentally assisted cracking in high-Temperature water10.5006/1.3278168 ↗
45. Continuing crack-tip deformation and fracture for plane-strain crack growth in elastic-plastic solids10.1016/0022-5096(78)90007-8 ↗
46. Progression markings, striations, and crack-arrest markings on fracture surfaces10.1016/j.msea.2006.09.083 ↗
47. Mechanistic and fractographic aspects of stress corrosion cracking10.1515/corrrev-2012-0501 ↗
48. Role of slip step emergence in the early stages of stress corrosion cracking in face centered iron-nickel-chromium alloys10.5006/0010-9312-23.5.117 ↗
49. Effects of hydrogen on stress corrosion crack growth rate of nickel alloys in high-temperature water10.5006/1.3278508 ↗
50. The mechanism of plastic deformation of crystals. Part I. Theoretical10.1098/rspa.1934.0106 ↗
51. Formulating stress corrosion cracking growth rates by combination of crack tip mechanics and crack tip oxidation kinetics10.1016/j.corsci.2009.10.041 ↗
52. Quantitative prediction of environmentally assisted cracking10.5006/1.3292125 ↗
53. Strain correlations in alloy 690 materials using electron backscatter diffraction and vickers hardness
54. Increase in the local yield stress near surface of austenitic stainless steel due to invasion by hydrogen10.1016/j.ijhydene.2014.01.190 ↗
55. Whitney award lecture-1987: hydrogen-the versatile embrittler10.5006/1.3583875 ↗
56. The diffusion and trapping of hydrogen in steel10.1016/0001-6160(70)90078-7 ↗
57. Hydrogen embrittlement understood10.1007/s11661-015-2836-1 ↗