journal article·2009-01

Corrosion behaviour of duplex stainless steels sintered in nitrogen

C. García, F. Martín, Y. Blanco, M.P. de Tiedra, M.L. Aparicio

Corrosion Science· Volume 51· Issue 1
Publisher page

Abstract

Abstract Duplex stainless steels obtained through powder metallurgy (PM) technology from austenitic AISI 316L and ferritic AISI 430L powders were mixed on different amounts to obtain biphasic structures with austenite/ferrite ratio of 50/50, 65/35 and 85/15. Prepared mixes of powders have been compacted at 750 MPa and sintered in N2–H2 (95% and 5%) at 1250 °C for 1 h. Corrosion behaviour, using electrochemical techniques such as anodic polarization measurement, cyclic anodic polarization scan and electrochemical potentio-kinetic reactivation test and double loop electrochemical potentio-kinetic reactivation double loop test were evaluated. For duplex stainless steels, when austenite/ferrite ratio increases the corrosion potential shifts to more noble potential and passive current density decreases. The beneficial effect of annealing solution heat treatment on corrosion behaviour was established and was compared with corrosion behaviour of vacuum sintered duplex stainless steels. The results were correlated with the microstructural features.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Corrosion Behavior and Inhibition · High Temperature Alloys and Creep

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (47)

Show source-provided references
1. P. Lacombe, B. Baroux, G. Beranger (Eds.), Les aciers inoxydables, Les èditions de physique, Les Ulis, France, 1990, pp. 663.
2. J. Charles, 10 years later, obviously duplex grades in industrial applications look like a success story, in: Proc. 6th World Duplex Conference & Expo, Venice, 2000, pp. 1–12.
3. Powder metallurgical duplex austenitic–ferritic stainless steels from prealloyed and mixed powders10.1179/pom.1994.37.1.57 ↗
4. E.M. Daver, C.J. Trombino, State of the North American PM Industry-2006 report, MPIF (Metal Powder Industries Federation), San Diego, June 21, 2006.
5. I. Cremer, Review of the PM industry from a European perspective, in: Plenary Presentation of EURO PM2007 Congress and Exhibition, Toulouse, France, 2007.
6. Corrosion behaviour of P/M duplex stainless steels made from prealloyed and mixed powders10.1016/0924-0136(95)02000-C ↗
7. Corrosion resistance of alloyed powder metallurgy austenitic stainless steels in acid solutions10.1179/bcj.1996.31.4.295 ↗
8. Copper enhances the sintering of duplex PM stainless steels
9. Sintered duplex stainless steel from premixex of 316L and 434L powders10.1016/S0254-0584(00)00477-6 ↗
10. Properties of vacuum sintered duplex stainless steel10.1016/j.jmatprotec.2005.02.038 ↗
11. Activated sintering of P/M duplex stainless steel powders10.1016/j.jmatprotec.2004.07.140 ↗
12. Effect of nitrogen on sintered duplex stainless steels10.1179/003258903225010532 ↗
13. Sintering transformations in mixtures of austenitic and ferritic stainless steel powders10.1179/003258901666167 ↗
14. High density sintering of duplex stainless steels10.1179/003258902225002491 ↗
15. Corrosion behavior of hot-pressed austenitic stainless steel in H2SO4 solutions at room temperature10.1016/0010-938X(83)90090-2 ↗
16. Effects of processing and manufacturing of high nitrogen-containing stainless steels on their mechanical, corrosion and wear properties10.1016/S0924-0136(01)00804-4 ↗
17. Effects of nitrogen and high-temperature aging on σ phase precipitation of duplex stainless steel10.1016/j.msea.2005.03.111 ↗
18. Microstructural evolution and localized corrosion resistance of an aged superduplex stainless steel10.1016/j.corsci.2003.09.024 ↗
19. Effect of nitrogen on corrosion behaviour of 28Cr–7Ni duplex and microduplex stainless steels in air-saturated 3.5wt.% NaCl solution10.1016/j.corsci.2004.11.017 ↗
20. Corrosion studies of austenitic and duplex stainless steels in aqueous lithium bromide solution at different temperatures10.1016/j.corsci.2004.05.025 ↗
21. Microstructure and pitting corrosion resistance of annealed duplex stainless steel10.1016/j.corsci.2006.04.003 ↗
22. Microstructure and pitting corrosion in simulated heat affected zones of duplex stainless steels10.1016/S0254-0584(01)00409-6 ↗
23. Sintered stainless steels: fatigue crack propagation resistance under hydrogen charging conditions10.1016/j.corsci.2006.10.036 ↗
24. Application of double loop electrochemical potentiodynamic reactivation test to austenitic and duplex stainless steels10.1016/S0921-5093(97)00008-7 ↗
25. Pitting corrosion behaviour of PM austenitic stainless steels sintered in nitrogen–hydrogen atmosphere10.1016/j.corsci.2006.10.009 ↗
26. Electrochemical reactivation methods applied to PM austenitic stainless steels sintered in nitrogen–hydrogen atmosphere10.1016/j.corsci.2007.10.001 ↗
27. Sensitization of PM 430l stainless steel sintered in nitrogen–hydrogen atmosphere10.5006/1.3278464 ↗
28. Effects of solution treatment and continuous cooling on σ phase precipitation in a 2205 duplex stainless steel10.1016/S0921-5093(01)00911-X ↗
29. Heat treatment influence on ASTM A890 GR 6A super duplex stainless steel microstructure10.1016/j.matchar.2005.05.008 ↗
30. Effect of homogenization heat treatment on critical pitting temperature and sigma phase formation in super duplex stainless steel
31. C. García, F. Martín, Y. Blanco, M.P. de Tiedra, M.L. Aparicio, Influence of sintering under nitrogen atmosphere on microstructures of powder metallurgy duplex stainless steels, Metall. Mater. Trans. A., in press.
32. F. Martín, C. García, Y. Blanco, J.M. Ruiz, Corrosion behaviour of duplex stainless steels sintered in nitrogen-hydrogen atmosphere, in: Proc. Euro PM2007 Congress & Exhibition, Toulouse, France, 2007.
33. ASTM Standard A262-91, Standard Practice for Detecting Susceptibility to Intergranular Attack on Austenitic Stainless Steels, ASTM, Philadelphia, 1993, pp. 1–18.
34. ASTM Standard G-5-87, Standard Reference Test Method for Making Potentiostatic and Potentiodynamic Anodic Polarization Measurements, ASTM, Philadelphia, 1993, pp. 71–75.
35. ASTM Standard G61-86, Standard Test Method for Conducting Cyclic Potentiodynamic Polarization Measurements for Localized Corrosion Susceptibility of Iron–Nickel- or Cobalt-Based Alloys, ASTM, Philadelphia, 1993, pp. 239–243.
36. ASTM Standard G108-92, Standard Test Method for EPR for Detecting Sensitization of AISI Type 304 and 304L Stainless Steels, ASTM, Philadelphia, 1993, pp. 457–463.
37. W.L.Clarke, V. M. Romero, J.C.Danko, Detection of sensitization in stainless steels using electrochemical techniques, in: Proc. Corrosion/77, Reprint No. 180, NACE International, Houston, 1977.
38. On the development of the electrochemical potentio-kinetic method10.1016/S0013-4686(01)00674-0 ↗
39. Corrosion modes in P/M ferritic stainless steels
40. Density-improved powder metallurgical ferritic stainless steels for high-temperature applications10.1016/j.jmatprotec.2007.02.005 ↗
41. Corrosion resistance of super duplex stainless steels in chloride ion containing environments: investigations by means new microelectrochemical methods II. Influence of precipitates10.1016/S0010-938X(00)00088-3 ↗
42. V. Čihal, M. Blahetová, E. Kalabisová, Z. Krhutová, S. Lasek, Applications of electrochemical polarization reactivation method: EPR test, J. Nucl. Mater. (2007), doi: 101016/j.jnucmat.2007.09.013.
43. Effect of “475°C embrittlement” on duplex stainless steels localized corrosion resistance10.1016/j.corsci.2004.06.012 ↗
44. Stainless steels, Heat treatment, in: ASM Specialty Handbook, ASM International, OH, 1994, pp. 290–313.
45. Soldadura de los aceros ferríticos y martensíticos de 11–14% de cromo
46. Effects of high-temperature annealing on texture and microstructure of an AISI 444 ferritic stainless steel10.1016/j.matchar.2006.02.015 ↗
47. V.S. Moura, L.D. Lima, J.M. Pardal, .Y. Kina, R.R.A. Corte, S.S.M. Tavares, Influence of microstructure on the corrosion resistance of the duplex stainless steel UNS S31803, Mater. Charact. (2007), doi: 10.1016/j.marcar.2007.09.002.