journal article·2010-02

Corrosion of continuous alumina-fibre reinforced Al–2 wt.% Cu–T6 metal–matrix composite in 3.15 wt.% NaCl solution

J. Zhu, L.H. Hihara

Corrosion Science· Volume 52· Issue 2
Publisher page

Abstract

Abstract The corrosion performance of a continuous alumina-fibre reinforced metal–matrix composite (MMC) and its monolithic matrix alloy (Al–2%Cu–T6) was studied in 3.15 wt.% sodium chloride solution. Corrosion initiation sites, mapping of corrosion current density and pH at corrosion sites, mass loss resulting from immersion, and polarization behaviour were studied. Results show that the MMC exhibited inferior corrosion resistance as compared to its monolithic matrix alloy. Corrosion of the MMC initiated preferentially along the fibre/matrix interface or in regions of plastic deformation. The build-up of acidity at localized corrosion sites on the MMC was enhanced by the formation of micro-crevices caused by fibres left in relief as a result of corrosion.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Aluminum Alloys Composites Properties · Aluminum Alloy Microstructure Properties · Advanced Welding Techniques Analysis

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (36)

Show source-provided references
1. Continuous-fiber reinforced Al composites: a new generation10.1007/BF03221227 ↗
2. Advanced ceramic structural materials10.1007/s11148-005-0017-2 ↗
3. The role of wetting and reactivity in infiltration of ceramic–metal composites
4. Continuous fibre reinforced titanium and aluminium composites: a comparison10.1016/S0921-5093(98)01161-7 ↗
5. Reinforcement coatings and interfaces in aluminium metal matrix composites10.1023/A:1004674822751 ↗
6. Better ceramics through metal modification
7. G.H. Schiroky, A.S. Fareed, B. Sonuparlak, C.T. Lee, B.W. Sorenson, Fabrication and properties of fiber-reinforced ceramic composites made by directed metal oxidation, In: S.R. Levine (Ed.), Flight-Vehicle Materials, Structures, and Dynamics, vol. 3, ASME, 1992, pp. 151–163.
8. Corrosion behavior of alumina–aluminium and silicon carbide–aluminium metal–matrix composites10.5006/1.3293621 ↗
9. The effect of fiber volume fraction on the properties of Al–α-Al2O3 metal matrix composites10.1007/BF02834177 ↗
10. Corrosion behavior of AA6061 and AA7005 reinforced with Al2O3 particles in aerated 3.5% chloride solutions: potentiodynamic measurements and microstructure evaluation10.1016/S0010-938X(98)00135-8 ↗
11. Corrosion behavior of a particulate metal–matrix composite10.5006/1.3284003 ↗
12. ANSI H35.5 American National Standard Nomenclature System for Aluminium Metal Matrix Composite Materials, The Aluminium Association Inc., 2003.
13. C. McCullough, A. Mortensen, P.S. Werner, H.E. Deve, T.L. Anderson, Method of making fiber reinforced aluminium matrix composite. US 6460597, 2002.
14. C. McCullough, A. Mortensen, P.S. Werner, H.E. Deve, T.L. Anderson, Fiber reinforced aluminium matrix composite wire. US 6544645, 2003.
15. Fine diameter ceramic fibers10.1016/S0955-2219(00)00090-X ↗
16. Localized corrosion currents and pH profile over B4C, SiC, and Al2O3 reinforced 6092 aluminium composites. I. In 0.5M Na2SO4 solution10.1149/1.1870873 ↗
17. G1-03 Standard Practice for Preparing, Cleaning, and Evaluating Corrosion Test Specimens, ASTM International, 2003.
18. Topographical analysis of pitting corrosion in AA7075-T6 using laser profilometry10.5006/1.3277587 ↗
19. J.E. Bulter, In-Situ Fiber Strength Distribution In Nextel™ 610 Reinforced Aluminium Composites, Thesis, Virginia Tech, Blacksburg, 2006.
20. Damage evolution of Nextel 610™ alumina fibre reinforced aluminium10.1016/j.actamat.2003.09.040 ↗
21. G 46-94 Standard Guide for Examination and Evaluation of Pitting Corrosion, ASTM International, 2005.
22. Pitting corrosion in cast 7XXX aluminium alloys and fibre reinforced MMCs10.1016/j.corsci.2003.09.003 ↗
23. P.P. Trzaskoma, Localized corrosion of metal matrix composites, in: R.H. Jones; R.E. Ricker (Eds.), Environmental Effects on Advanced Materials, The Minerals, Metals & Materials Society, 1991, pp. 249–265.
24. Electrochemical characteristics of intermetallic phases in aluminium alloys: an experimental survey and discussion10.1149/1.1869984 ↗
25. Interfacial microchemistry and microstructure of Al–Mg–Si alloy matrix composites reinforced with Al2O3 particulates10.1016/S1359-6462(96)00467-8 ↗
26. V.S. Agarwala, A.S. Fabiszewski, Processing and corrosion behavior of metal matrix composites, in: First International Symposium on Environmental Effects on Advanced Materials, San Diego, California, 1992, pp. 19/11–19/21.
27. Pitting corrosion of aluminium10.1016/S0010-938X(99)00012-8 ↗
28. Localized corrosion of aluminium alloys – a review10.5006/1.3584905 ↗
29. Transport processes and the mechanism of pitting of metals10.1149/1.2132857 ↗
30. Transport processes in passivity breakdown – II. Full hydrolysis of the metal ions10.1016/0010-938X(81)90009-3 ↗
31. D. Talbot, J. Talbot, Corrosion Science and Technology, second ed., CRC Press LLC, 2007.10.1201/b13606 ↗
32. L.H. Hihara, Metal matrix composites, in: R. Baboian (Ed.), Corrosion Tests and Standards – Application and Interpretation, ASTM International, 2004, pp. 531–542.
33. Bolz · 1973
34. L.H. Hihara, Corrosion of aluminium–matrix composites, Dissertation, MIT, Boston, 1989.
35. Corrosion resistance of Al-based metal matrix composites10.1016/0921-5093(95)80065-3 ↗
36. H.J. Greene, Evaluation of corrosion protection methods for aluminium metal matrix composites, Report, 1992.