Abstract
Abstract The effect of Ti precipitates on hydrogen embrittlement (HE) was investigated using Ti-free and Ti-bearing TWIP steels through slow tensile tests and thermal desorption analysis. Whereas Ti-free steel did not show the reduction in elongation by hydrogen charging, Ti-bearing steel revealed a great reduction in elongation, indicative of the low resistance to HE. During plastic deformation, hydrogen atoms migrated from grain boundaries and dislocations to twin boundaries for Ti-free steel and to the interfaces of Ti particles for Ti-bearing steel. The low resistance to HE of Ti-bearing steel was due to a ductile to brittle transition near hydrogen-trapped TiN particles.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Microstructure and Mechanical Properties of Steels · Corrosion Behavior and Inhibition
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (45)
Show source-provided references
1. High manganese austenitic twinning induced plasticity steels: a review of the microstructure properties relationships10.1016/j.cossms.2011.04.002 ↗
2. Effects of recrystallization annealing temperature on carbide precipitation, microstructure, and mechanical properties in Fe–18Mn–0.6C–1.5Al TWIP steel10.1016/j.msea.2009.08.048 ↗
3. On the transitions of deformation modes of fully austenitic steels at room temperature10.1007/s12540-010-0001-3 ↗
4. Effects of Al on microstructure and tensile properties of C-bearing high Mn TWIP steel10.1016/j.actamat.2011.12.004 ↗
5. Effects of the strain induced martensite transformation on the delayed fracture for Al-added TWIP steel
6. Microstructural influences on hydrogen delayed fracture of high strength steels10.1016/j.msea.2008.11.040 ↗
7. Sub critical crack growth in hydrogen assisted cracking of cold drawn eutectoid steel10.1016/j.corsci.2006.12.005 ↗
8. Role of ɛ martensite in tensile properties and hydrogen degradation of high-Mn steels10.1016/j.msea.2011.11.039 ↗
9. Selective appearance of ɛ-martensitic transformation and dynamic strain aging in Fe–Mn–C austenitic steels
10. Premature fracture mechanism in an Fe–Mn–C austenitic steel10.1007/s11661-012-1220-7 ↗
11. Hydrogen embrittlement in a Fe–Mn–C ternary twinning-induced plasticity steel10.1016/j.corsci.2011.09.022 ↗
12. Effect of hydrogen content on the embrittlement in a Fe–Mn–C twinning-induced plasticity steel10.1016/j.corsci.2012.03.009 ↗
13. The mechanism of enhanced resistance to the hydrogen delayed fracture in Al-added Fe–18Mn–0.6C twinning-induced plasticity steels10.1016/j.ijhydene.2012.03.100 ↗
14. Hydrogen-induced cracking at grain and twin boundaries in an Fe–Mn–C austenitic steel10.1016/j.scriptamat.2011.12.015 ↗
15. Hydrogen-induced delayed fracture of a Fe–22Mn–0.6C steel pre-strained at different strain rates10.1016/j.scriptamat.2012.02.040 ↗
16. Effects of Al addition on deformation and fracture mechanisms in two high manganese TWIP steels10.1016/j.msea.2010.12.085 ↗
17. Influence of machining-induced martensite on hydrogen-assisted fracture of AISI type 304 austenitic stainless steel10.1016/j.ijhydene.2011.05.133 ↗
18. Effects of alloy composition and strain hardening on tensile fracture of hydrogen-precharged type 316 stainless steels10.1016/j.ijhydene.2007.10.046 ↗
19. Caliber-rolled TWIP steel for high-strength wire rods with enhanced hydrogen-delayed fracture resistance10.1016/j.scriptamat.2012.07.006 ↗
20. Delayed static failure of twinning-induced plasticity steels10.1016/j.scriptamat.2012.02.038 ↗
21. Hydrogen delayed fracture properties and internal hydrogen behavior of a Fe–18Mn–1.5AI–0.6C TWIP steel10.2355/isijinternational.49.1952 ↗
22. Hydrogen embrittlement in Al-added twinning-induced plasticity steels evaluated by tensile tests during hydrogen charging10.2355/isijinternational.52.2283 ↗
23. Effect of aluminium on hydrogen-induced fracture behaviour in austenitic Fe–Mn–C steel10.1098/rspa.2012.0458 ↗
24. High strength Fe–Mn–(Al, Si) TRIP/TWIP steels development – properties – application10.1016/S0749-6419(00)00015-2 ↗
25. Hydrogen effects in prestrained transformation induced plasticity steel10.1007/s11661-011-1075-3 ↗
26. Effects of niobium on mechanical twinning and tensile properties of a high Mn twinning-induced plasticity steel10.2320/matertrans.M2012273 ↗
27. Precipitation strengthening in high manganese austenitic TWIP steels10.3139/146.110508 ↗
28. Effect of microalloying elements (Nb, V and Ti) on the hot flow behavior of high-Mn austenitic twinning induced plasticity (TWIP) steel10.1016/j.msea.2012.09.101 ↗
29. Hot deformation activation energy (QHW) of austenitic Fe–22Mn–1.5Al–1.5Si–0.4C TWIP steels microalloyed with Nb, V, and Ti10.1016/j.msea.2012.10.091 ↗
30. Strengthening mechanisms of a new 700MPa hot rolled Ti-microalloyed steel produced by compact strip production10.1016/j.jmatprotec.2010.05.018 ↗
31. Precipitation strengthening in high manganese austenitic TWIP steels10.3139/146.110508 ↗
32. A classification of hydrogen traps in steel10.1007/BF02812023 ↗
33. The effect of the interface character of TiC particles on hydrogen trapping in steel10.1016/0001-6160(87)90268-9 ↗
34. Transport of hydrogen in the films made of metals, semiconductors, and dielectrics10.1007/s11003-008-9001-6 ↗
35. Trap theory of hydrogen embrittlement10.1016/0001-6160(80)90106-6 ↗
36. Cu precipitation kinetics during martensite tempering in a medium C steel10.1016/j.jallcom.2012.11.108 ↗
37. Hydrogen-assisted quasi-cleavage fracture in a single crystalline type 316 austenitic stainless steel10.1016/j.corsci.2013.06.018 ↗
38. Effect of hydrogen on the fracture behavior of high strength steel during slow strain rate test10.1016/j.corsci.2007.03.038 ↗
39. Changes of microstructures and high temperature properties during high temperature service of Niobium added ferritic stainless steels10.1016/S0921-5093(02)00831-6 ↗
40. Effects of tungsten on the hydrogen embrittlement behaviour of microalloyed steels10.1016/j.corsci.2014.01.042 ↗
41. A Q-DLTS investigation of aluminum nitride surface termination10.1557/jmr.2012.50 ↗
42. Hydrogen-induced softening and hardening in high purity Fe–C alloys10.1016/0025-5416(82)90055-6 ↗
43. Hydrogen-induced hardening of Ti–6Al–4V alloy in β phase field10.1016/j.matdes.2013.09.035 ↗
44. The effect of pre-strain on hydrogen embrittlement in 310S stainless steel10.1016/j.jallcom.2014.02.038 ↗
45. The effect of pre-strain on the resistance to hydrogen embrittlement in 316L austenitic stainless steel10.2320/matertrans.M2014036 ↗