The mechanism of aqueous stress-corrosion cracking of α + β titanium alloys

Sheng Cao, Suming Zhu, Chao Voon Samuel Lim, Xigen Zhou, Xiaobo Chen, Bruce R.W. Hinton, Rodney R. Boyer, James C. Williams, Xinhua Wu

Corrosion Science· Volume 125

Abstract

In a previous paper (Cao et al., 2017) [1], a transition in fracture mode in aqueous NaCl Stress-Corrosion Cracking (SCC) of Ti-8Al-1Mo–1 V was reported. This paper attempts to unravel the operating mechanism for SCC by dislocation analysis on the Focus Ion Beam (FIB) lift-out foils from pre-crack and the SCC regions. It is shown that both basal and slips are operative in the SCC region while the basal is the only activated system in the pre-crack region. Moreover, there is an increase in dislocation density in the SCC region compared to the pre-crack region. Based on these observations, combined Absorption Induced Dislocation Emission (AIDE) and Hydrogen Enhanced Localized Plasticity (HELP) is proposed to be the operating mechanisms for SCC in α+β titanium alloys.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Titanium Alloys Microstructure and Properties · Corrosion Behavior and Inhibition

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (47)

Show source-provided references
1. Effects of microtexture and Ti3Al ((2) precipitates on stress-corrosion cracking properties of a Ti-8Al-1Mo–1 V alloy10.1016/j.corsci.2016.12.012 ↗
2. Lütjering · 2007
3. Boyer · 1994
4. Microstructure and mechanical properties of electron beam welded titanium alloy Ti-6246
5. Microstructure and tribological behavior of a TiO2/hBN composite ceramic coating formed via micro-arc oxidation of Ti–6Al–4V alloy10.1016/j.jmst.2016.06.015 ↗
6. Titanium and its alloys: metallurgy, heat treatment and alloy characteristics
7. Corrosion behavior of Ti-8Al-1Mo-1V alloy compared to Ti-6Al-4V10.1016/j.matdes.2010.09.009 ↗
8. Stress corrosion cracking facet crystallography of Ti-8Al-1Mo-1V10.1016/j.corsci.2010.05.046 ↗
9. Aqueous stress corrosion in titanium alloys10.1179/000705975798320783 ↗
10. Stress corrosion cracking (SCC) and hydrogen-assisted cracking in titanium alloys
11. Leyens · 2003
12. The influence of oxygen concentration on the internal stress and dislocation arrangements in α titanium10.1007/BF02652870 ↗
13. Deformation behavior of HCP Ti-Al alloy single crystals10.1007/s11661-002-0153-y ↗
14. Observations of facet formation in near-α titanium and comments on the role of hydrogen10.1007/s11661-010-0507-9 ↗
15. Stress corrosion cracking
16. Hydrogen embrittlement of α titanium: In situ TEM studies10.1016/0001-6160(88)90032-6 ↗
17. The stress corrosion cracking mechanism of α-titanium alloys at room temperature10.1016/S0010-938X(70)80043-9 ↗
18. Mechanistic and fractographic aspects of stress-corrosion cracking (SCC)
19. Hydrogen embrittlement (HE) phenomena and mechanisms
20. Hydrogen embrittlement understood10.1007/s11661-015-2836-1 ↗
21. Environmentally assisted fatigue crack nucleation in Ti-6Al-2Sn-4Zr-6Mo10.1016/j.corsci.2015.03.013 ↗
22. Hydrogen-induced modification in the deformation and fracture of a precipitation-hardened Fe-Ni based austenitic alloy10.1016/j.jmst.2014.03.017 ↗
23. The stress-corrosion cracking susceptibility of near-α titanium alloy IMI 834 in presence of hot salt10.1016/j.corsci.2014.01.013 ↗
24. Fatigue crack growth behaviour of forged Ti-6Al-4V in gaseous hydrogen10.1016/j.corsci.2013.08.009 ↗
25. Explanation for anomalous environmentally assisted cracking behaviour of a wrought Mg-Mn alloy in chloride medium10.1016/j.corsci.2016.11.001 ↗
26. Hot salt stress corrosion cracking behavior of Ti-6242S alloy10.1007/s11661-015-3155-2 ↗
27. Plane strain compression of titanium crystals10.4028/www.scientific.net/MSF.157-162.639 ↗
28. The origins of heterogeneous deformation during primary hot working of Ti-6Al-4V10.1016/S0749-6419(01)00057-2 ↗
29. Direct evidence for plastic deformation of quasicrystals by means of a dislocation mechanism10.1103/PhysRevLett.71.549 ↗
30. The application of focused ion beam microscopy in the material sciences10.1016/j.matchar.2008.11.014 ↗
31. Focused ion beam micromachining10.1557/mrs2007.62 ↗
32. FIB damage of Cu and possible consequences for miniaturized mechanical tests10.1016/j.msea.2007.01.046 ↗
33. The dislocation mechanism of stress corrosion embrittlement in Ti-6Al-2Sn-4Zr-6Mo10.1007/s11661-015-3181-0 ↗
34. 〈1123〉{1011} slip in titanium polycrystals at room temperature10.1016/0036-9748(86)90399-6 ↗
35. Room temperature fracture processes of a near-α titanium alloy following elevated temperature exposure10.1007/s10853-012-6673-y ↗
36. Effect of oxygen and hydrogen on mechanical properties of commercial purity titanium10.1179/imr.1996.41.1.1 ↗
37. The effect of hydrogen on dislocation dynamics10.1016/S0013-7944(01)00011-X ↗
38. Hydrogen effects on plasticity10.1016/S1572-4859(09)01504-6 ↗
39. Hydrogen induced plasticity in stress corrosion cracking of engineering systems10.1016/S0013-7944(00)00121-1 ↗
40. Hydrogen diffusion coefficients in the titanium alloys IMI 834, Ti 10-2-3, Ti 21 S, and alloy C10.1007/s11661-000-0161-8 ↗
41. The diffusion of hydrogen
42. Hydrogen transport by dislocation10.1007/BF02644079 ↗
43. Evidence for dislocation transport of hydrogen in aluminum10.1007/BF02642394 ↗
44. Visualization of hydrogen diffusion in a hydrogen-enhanced fatigue crack growth in type 304 stainless steel10.1007/s11661-011-0661-8 ↗
45. Dislocation interaction with hydrides in titanium containing a low hydrogen concentration10.1080/14786430310001623533 ↗
46. Analysis of frequency and amplitude effects on corrosion fatigue crack propagation in Ti-8Al-1Mo-1V10.1007/BF02662746 ↗
47. A comparison of phase transformations in three commercial titanium alloys