Multi-cycle and long-term ablation behavior of Cf/ZrB2-SiC composites at 2500 °C

Bo-Wen Chen, De-Wei Ni, Jun Lu, Fei-Yan Cai, Xue-Gang Zou, Hai-Jun Zhou, Shao-Ming Dong

Corrosion Science· Volume 184
Publisher page

Abstract

Abstract Multi-cycle and long-term ablation behavior of Cf/ZrB2-SiC composite was evaluated by plasma ablation flame at 2500 °C. The composites can be protected by the oxide layer with uniform distribution of ZrO2 particles in SiO2 melt. However, the structural stability of the oxide layer could be destroyed due to the phase transition of ZrO2 and violent evaporation of SiO2, resulting from the aggregation and growth of ZrO2 during multi-cycle and long-term ablation. It is of great significance to optimize the composition and microstructure of the oxide layer to retard the aggregation, growth and phase transition of ZrO2.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced ceramic materials synthesis · MXene and MAX Phase Materials · Advanced materials and composites

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (36)

Show source-provided references
1. Ablation-resistant carbide Zr0.8Ti0.2C0.74B0.26 for oxidizing environments up to 3,000 degrees C10.1038/ncomms15836 ↗
2. Is spark plasma sintering suitable for the densification of continuous carbon fibre-UHTCMCs10.1016/j.jeurceramsoc.2019.12.004 ↗
3. Oxidation protection of C/C composites: coating development with thermally stabile SiC@PyC nanowires and an interlocking TaB2-SiC structure10.1016/j.corsci.2018.12.024 ↗
4. Oxidation behavior and ablation mechanism of Cf/ZrB2-SiC composite fabricated by vibration-assisted slurry impregnation combined with low-temperature hot pressing10.1016/j.corsci.2019.108181 ↗
5. Architectural engineering inspired method of preparing Cf/ZrC-SiC with graceful mechanical responses10.1111/jace.16018 ↗
6. Carbon fiber reinforced ultra-high temperature ceramic matrix composites: a review10.1016/j.ceramint.2019.05.065 ↗
7. Ablation behavior of C/C-ZrC and C/SiC-ZrC composites fabricated by a joint process of slurry impregnation and chemical vapor infiltration10.1016/j.ceramint.2017.12.062 ↗
8. Carbon fiber reinforced ZrC based ultra-high temperature ceramic matrix composite subjected to laser ablation: ablation resistance, microstructure and damage mechanism10.1016/j.ceramint.2020.02.236 ↗
9. Ablation behavior and mechanism of C/ZrC, C/ZrC-SiC and C/SiC composites fabricated by polymer infiltration and pyrolysis process10.1016/j.corsci.2014.05.005 ↗
10. Ablation behavior of Cf/ZrC-SiC-based composites fabricated by an improved reactive melt infiltration10.1016/j.jeurceramsoc.2019.07.007 ↗
11. Ablation behavior and mechanism of 3D Cf/ZrC-SiC composites in a plasma wind tunnel environment10.1016/j.jascer.2015.07.005 ↗
12. Microstructures and mechanical properties of 3D 4-directional, Cf/ZrC-SiC composites using ZrC precursor and polycarbosilane10.1016/j.mseb.2013.07.001 ↗
13. Ablation of C/SiC-HfC composite prepared by precursor infiltration and pyrolysis in plasma wind tunnel10.1007/s40145-020-0379-4 ↗
14. Fabrication and properties of 3-dimensional 4-directional Cf/HfC-SiC composites by precursor impregnation and pyrolysis process10.1016/j.jallcom.2017.12.059 ↗
15. Microstructure and ablation behavior of C/C-HfC composites prepared by precursor infiltration and pyrolysis10.1016/j.corsci.2015.01.053 ↗
16. Long-term ablation behavior and mechanisms of 2D-Cf/ZrB2-SiC composites at temperatures up to 2400 °C10.1016/j.corsci.2020.108967 ↗
17. Effects of high-temperature annealing on the microstructure and properties of C/SiC-ZrB2 composites10.1016/j.matdes.2013.06.073 ↗
18. Comparison of thermal and ablation behaviors of C/SiC composites and C/ZrB2-SiC composites10.1016/j.corsci.2008.09.037 ↗
19. Properties and microstructure evolution of Cf/SiC composites fabricated by polymer impregnation and pyrolysis (PIP) with liquid polycarbosilane10.1016/j.ceramint.2017.02.100 ↗
20. Mechanical, oxidation and ablation properties of C/(C-SiC)CVI-(ZrC-SiC)PIP composites10.1016/j.corsci.2019.108200 ↗
21. Effect of ZrC particle distribution on the ablation resistance of C/C-SiC-ZrC composites fabricated using precursor infiltration pyrolysis10.1016/j.ceramint.2020.03.157 ↗
22. Characterization and mechanical properties of Cf/ZrB2-SiC composites fabricated by a hybrid technique based on slurry impregnation, polymer infiltration and pyrolysis and low-temperature hot pressing10.1016/j.ceramint.2018.12.001 ↗
23. The corrosion behavior of CVI SiC matrix in SiCf/SiC composites under molten fluoride salt environment10.1016/j.jnucmat.2017.02.007 ↗
24. Effect of heat treatment on the mechanical properties of SiCf/BN/SiC fabricated by CVI10.1016/j.ceramint.2015.11.030 ↗
25. Ultra-high-temperature ablation behavior of SiC-ZrC-TiC modified carbon/carbon composites fabricated via reactive melt infiltration10.1016/j.jeurceramsoc.2019.10.027 ↗
26. Reactive melt infiltration of carbon fibre reinforced ZrB2/B composites with Zr2Cu10.1016/j.compositesa.2020.105973 ↗
27. Materials characterisation and mechanical properties of Cf-UHTC powder composites10.1016/j.jeurceramsoc.2018.12.043 ↗
28. Selection, processing, properties and applications of ultra-high temperature ceramic matrix composites, UHTCMCs-a review
29. Development of UHTCMCs via water based ZrB2 powder slurry infiltration and polymer infiltration and pyrolysis10.1016/j.jeurceramsoc.2020.05.054 ↗
30. Improved microstructure and high temperature mechanical properties of C/C-SiC composites by introduction of ZrC nanoparticles10.1016/j.ceramint.2019.12.034 ↗
31. Microstructures and mechanical properties of Cf/ZrB2-SiC composite fabricated by nano slurry brushing combined with low-temperature hot pressing10.1016/j.jallcom.2019.03.147 ↗
32. Efficacy of a ZrB2–SiC matrix in protecting C fibres from oxidation in novel UHTCMC materials10.1016/j.matdes.2016.09.104 ↗
33. Carbon carbon composites10.1146/annurev.ms.24.080194.000315 ↗
34. Properties of selected zirconia containing silicate glasses
35. Capillary forces and structuring in layers of colloid particles10.1016/S1359-0294(01)00105-4 ↗
36. Growth modes for monoclinic yttria-stabilized zirconia during the martensitic transformation10.1111/jace.15004 ↗