Protection of galvanized steel from corrosion in NaCl solution by coverage with phytic acid SAM modified with some cations and thiols
Source abstract
Abstract
Abstract Ultrathin films of various compounds were prepared on galvanized steel coated with both phytic acid (PA) and diethylene triamine pentamethane phosphonic acid (DETPMPS) self-assembled monolayers (SAM), and in the presence of small amounts of special salt (MnSO4 or Cr(NO3)3). Phytic acid and phytic acid–Mn2+ were modified with dithio-oxamide (DTOA) and 2,3-dimercapto-1-propanol (DMP). Tafel plots and impedance measurements were used. Most investigated conversion coatings of the samples pretreated only in H2SO4/H2O2-mixture, showed that the protective efficiency values (P%) are greater than those of pretreated in both hot alkaline solution and H2SO4/H2O2-mixture.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Corrosion Behavior and Inhibition · Polymer Surface Interaction Studies · Molecular Junctions and Nanostructures
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (64)
Show source-provided references
1. The inhibition effects of chromate-free, anion inhibitors on corrosion of zinc in aerated 0.5M NaCl10.1016/S0010-938X(00)00085-8 ↗
2. Passivity and passivity breakdown of a zinc electrode in aerated neutral sodium nitrate solutions10.1016/j.electacta.2004.07.051 ↗
3. On the role of NO2− ions in passivity breakdown of zinc in deaerated neutral sodium nitrite solutions and the effect of some inorganic inhibitors potentiodynamic polarization, cyclic voltammetry10.1016/j.electacta.2007.10.034 ↗
4. Molybdate and tungstate as corrosion inhibitors and the mechanism of inhibition10.1149/1.2778118 ↗
5. An XPS investigation of dichromate and molybdate inhibitors on aluminium10.1016/0010-938X(85)90089-7 ↗
6. Restriction of Hazardous substance Directive, 2002/95/EC.
7. Surface characterization of cerium layers on galvanised steel10.1016/j.surfcoat.2004.02.033 ↗
8. Preparation of chromate-free, self-healing polymer films containing sodium silicate on zinc pretreated in a cerium (III) nitrate solution for preventing zinc corrosion at scratches in 0.5M NaCl10.1016/S0010-938X(01)00138-X ↗
9. Treatment of zinc surface with cerium (III) nitrate to prevent zinc corrosion in aerated 0.5M NaCl10.1016/S0010-938X(00)00189-X ↗
10. Oxidising alternative species to chromium VI in zinc-galvanized steel surface treatment. Part 2: An electrochemical study10.1016/S0257-8972(98)00476-9 ↗
11. Oxidising alternative species to chromium VI in zinc galvanized steel surface treatment. Part 1: A morphological and chemical study10.1016/S0257-8972(98)00464-2 ↗
12. Molybdate conversion coatings on zinc surfaces10.1016/j.jelechem.2004.07.016 ↗
13. Silanes and rare earth salts as chromate replacers for pre-treatments on galvanized steel10.1016/j.electacta.2004.01.051 ↗
14. The alkaline stability of phosphate coatings I: ICP atomic emission spectroelectrochemistry10.1016/S0010-938X(03)00182-3 ↗
15. The alkaline stability of phosphate coatings. II: In situ Raman spectroscopy10.1016/S0010-938X(03)00183-5 ↗
16. Effect of molybdate post-sealing on the corrosion resistance of zinc phosphate coatings on hot-dip galvanized steel10.1016/j.corsci.2007.12.002 ↗
17. Nucleation and formation of zinc phosphate conversion coating on cold-rolled steel10.1016/0010-938X(91)90112-3 ↗
18. Prevention of zinc corrosion in oxygenated 0.5M NaCl by treatment in a cerium (III) nitrate solution and modification with sodium hexadecanoate10.1016/j.corsci.2005.10.020 ↗
19. Protection of zinc from corrosion by coverage with a hydrated cerium(III) oxide layer and ultrathin polymer films of carboxylate self-assembled monolayer modified with alkyltriethoxysilanes10.1016/j.corsci.2006.07.008 ↗
20. The corrosion resistance of hot dip galvanized steel and AA2024-T3 pre-treatment with bis-[triethoxysilylpropyl] tetrasulfide solutions doped with Ce(NO3)310.1016/j.corsci.2006.01.010 ↗
21. Study of conversion coatings obtained from tungstate–phosphoric acid solutions10.1016/j.corsci.2004.07.008 ↗
22. The development of passivation coatings by cathodic reduction in sodium molybdate solutions10.1016/0010-938X(88)90025-X ↗
23. Molybdate/A(III) composite films on steel and zinc-plated steel by chemical conversion10.1016/S0010-938X(01)00174-3 ↗
24. The molybdate–zinc conversion process10.1016/j.corsci.2008.10.019 ↗
25. Development of a molybdate–phosphate–silane–silicate (MPSS) coating process for electrogalvanized steel10.1016/j.corsci.2004.11.028 ↗
26. Electrochemical study of the corrosion behaviour of zinc treated with a new organic chelating inhibitor10.1016/S0010-938X(99)00132-8 ↗
27. Self-assembly monolayers of α,ω-diphosphonic acids on Ti enable complete or spatially controlled surface derivatization10.1021/la036084h ↗
28. Self-assembled monolayers of alkylphosphonic acids on metal oxides10.1021/la9607621 ↗
29. Effect of interfacial energetics on the protection of steel and aluminium surfaces by alkyl acid coatings10.1021/la011572f ↗
30. Self-assembled monolayers of long-chain hydroxamic acids on the native oxide of metals10.1021/la00003a024 ↗
31. Diphosphonate thin films on zinc: preparation, structure characterization and corrosion protection effects10.1016/j.apsusc.2008.06.039 ↗
32. Zinc corrosion protection with 1,5-diphosphono-pentane10.1016/j.corsci.2008.09.021 ↗
33. Protection of passivated iron against corrosion in a 0.1M NaNO3 solution by coverage with an ultrathin polymer coating of carboxylate SAM10.1016/j.corsci.2008.12.028 ↗
34. Corrosion protection of cold-rolled steel by zinc-rich epoxy paint coatings loaded with nano-size alumina supported polypyrrole10.1016/j.corsci.2011.06.014 ↗
35. The effect of modification with hydrogen peroxide on a hydrated cerium (III) oxide layer for protection of zinc against corrosion in 0.5M NaCl10.1016/j.corsci.2005.01.014 ↗
36. The corrosion and polarization behaviour of copper in domestic water in the presence of Ca, Mg and Na-salts of phytic acid10.1016/0010-938X(94)00105-F ↗
37. Phytic acid as an efficient low-molecular-mass displacer for anion-exchange displacement chromatography of proteins10.1016/S0378-4347(00)00028-1 ↗
38. Phytic acid conversion coating on Mg–Li alloy10.1016/j.jallcom.2009.06.089 ↗
39. Electrochemical and photoelectrochemical study of the self-assembled monolayer phytic acid on cupronickel B3010.1016/j.corsci.2008.09.016 ↗
40. Self-assembled alkanethiol monolayers on a Zn substrate:structure and organization10.1021/la0701879 ↗
41. Self-assembled alkanethiol monolayers on a Zn substrate: interface studied by XPS10.1016/j.susc.2008.03.044 ↗
42. Preparation of ultrathin polymer coatings adsorbed on iron via a covalent bond by multistep modification of a hydroxymethylbenzene SAM with ethoxysilanes and alkanediol for preventing iron corrosion in 0.5M NaCl10.1016/j.corsci.2008.05.020 ↗
43. Cerium–phytic acid passivation treatment on galvanized steel10.4028/www.scientific.net/KEM.373-374.228 ↗
44. The inhibition of mild steel corrosion in acidic medium by 1-methyl-3-pyridin-2-yl-thiourea10.1016/j.corsci.2008.11.019 ↗
45. Corrosion inhibition of tin, indium and tin–indium alloys by adenine or adenosine in hydrochloric acid solution10.1016/j.corsci.2009.08.047 ↗
46. Improvement of the film thickness by modification of the hydroxymethylbenzene SAM with tetraethoxysilane and octanediol for protection of iron from corrosion in 0.5M NaCl10.1016/j.corsci.2007.12.010 ↗
47. Study on the corrosion resistance of phytic acid conversion coating for magnesium alloys10.1016/j.surfcoat.2006.02.020 ↗
48. Protection of copper corrosion by an ultrathin two-dimensional polymer film of alkanethiol monolayer10.1149/1.1838567 ↗
49. Self-assembled monolayers of p-toluene and p-hydroxymethylbenzene moieties adsorbed on iron by the formation of covalent bonds between carbon and iron atoms for protection of iron from corrosion10.1016/j.corsci.2006.06.034 ↗
50. Phenothiazine as inhibitor of the corrosion of cadmium in acidic solutions10.1023/A:1018456008267 ↗
51. Preparation of one-dimensional polymer films by modification of a hydroxymethylbenzene self-assembled monolayer on iron with alkyltriethoxysilanes for preventing iron corrosion10.1016/j.corsci.2007.04.004 ↗
52. Protection of iron against corrosion by coverage with ultra thin two-dimensional polymer films of a hydroxymethylbenzene self-assembled monolayer anchored by the formation of a covalent bond10.1016/j.corsci.2007.05.032 ↗
53. Additional modification to two-dimensional polymer films of a hydroxymethylbenzene self-assembled monolayer with alkyltriethoxysilanes for enhancing the protective abilities against iron corrosion10.1016/j.corsci.2007.08.015 ↗
54. Effect of minor nickel alloying with zinc on the electrochemical and corrosion behaviour of zinc in alkaline solution10.1016/j.jpowsour.2010.03.071 ↗
55. The kinetics of zinc dissolution in aerated sodium sulphate solutions. A measurement of the corrosion rate by impedance techniques10.1016/0010-938X(89)90077-2 ↗
56. Comparison of corrosion behaviour of zinc in NaCl and NaOH solutions. Part II: Electrochemical analyses10.1016/j.corsci.2010.08.018 ↗
57. Corrosion inhibition study of pure Al and some of its alloys in 1.0M HCl solution by impedance technique10.1016/S0010-938X(03)00133-1 ↗
58. Evaluation of organic coatings with electrochemical in Part 2: application of EIS to coatings
59. Phenthiazines as corrosion inhibitors for zinc in NH4Cl solution10.1179/bcj.1983.18.2.102 ↗
60. Inhibitive action of ferricyanide complex anion on both corrosion and passivation of zinc and zinc–nickel alloy in the alkaline solution10.1016/j.jpowsour.2011.03.057 ↗
61. A two-step roll coating phosphate/molybdate passivation treatment for hot-dip galvanized steel10.1016/j.corsci.2010.06.020 ↗
62. Inhibition of mild steel corrosion in hydrochloric acid solution by triazole derivatives. Part II: Time and temperature effects and thermodynamic treatments10.1016/j.electacta.2007.08.021 ↗
63. Aminic nitrogen-bearing polydentate shiff base compounds as corrosion inhibitors for iron in acidic media: a quantum chemical calculation10.1016/j.corsci.2007.10.009 ↗