journal article·2009-08

Effect of alternating voltage treatment on the corrosion resistance of pure magnesium

Xiaolan Liu, Tao Zhang, Yawei Shao, Guozhe Meng, Fuhui Wang

Corrosion Science· Volume 51· Issue 8
Publisher page

Abstract

Pure magnesium was treated by alternating voltage (AV) treatment technique. The optimal AV-treatment parameters for greatly improving corrosion resistance were determined by the orthogonal experiments. Polarization curves, electrochemical impedance spectroscopy (EIS), and scanning electrochemical microscopy (SECM) were performed to understand the effect of AV-treatment on the corrosion resistance of pure magnesium. AFM, contact angle measurement and XPS were employed to further investigate the influence of AV-treatment on the properties of the surface film formed on pure magnesium after AV-treatment. The results showed that a uniform and stable film was formed and the corrosion resistance of pure magnesium was greatly improved after AV-treatment. This was caused by the noticeable change of chemical structure and semi conducting properties of surface film after AV-treatment.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Magnesium Alloys: Properties and Applications · Corrosion Behavior and Inhibition · Aluminum Alloys Composites Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (35)

Show source-provided references
1. Understanding magnesium corrosion10.1002/adem.200310405 ↗
2. Emerging technology in surface modification of light metals10.1016/S0257-8972(00)00940-3 ↗
3. Corrosion resistance of WE43 and AZ91D magnesium alloys with phosphate PEO coatings10.1016/j.corsci.2008.03.002 ↗
4. Transport of species during plasma electrolytic oxidation of WE43-T6 magnesium alloy10.1149/1.2823374 ↗
5. Corrosion of AZ91D magnesium alloy with a chemical conversion coating and electroless nickel layer10.1016/j.corsci.2003.09.023 ↗
6. The corrosion performance of anodized magnesium alloys10.1016/j.corsci.2006.02.008 ↗
7. Stannate and permanganate conversion coatings on AZ31 magnesium alloy10.1016/j.corsci.2007.04.011 ↗
8. A chromium-free conversion coating of magnesium alloy by a phosphate–permanganate solution10.1016/j.surfcoat.2005.07.064 ↗
9. Effect of HCl pre-treatment on corrosion resistance of cerium-based conversion coatings on magnesium and magnesium alloys10.1016/j.corsci.2004.06.016 ↗
10. Formation and properties of stannate conversion coatings on AZ61 magnesium alloys10.1016/j.corsci.2004.11.023 ↗
11. Formation of phosphate–permanganate conversion coating on AZ31 magnesium alloy10.1149/1.2164787 ↗
12. Effect of fluorine anions on anodizing behavior of AZ91 magnesium alloy in alkaline solutions10.1149/1.2883739 ↗
13. Protective coatings on magnesium and its alloys – a critical review10.1016/S0925-8388(01)01899-0 ↗
14. Electroless Ni–P coating of different magnesium alloys10.1016/j.surfcoat.2008.05.037 ↗
15. Electrodeposition of a protective copper/nickel deposit on the magnesium alloy (AZ31)10.1016/j.corsci.2007.12.004 ↗
16. Electrochemical behavior of anodized Mg alloy AZ91D in chloride containing aqueous solution10.1016/j.corsci.2005.01.010 ↗
17. Chrome-free surface treatments for magnesium alloy10.1016/S0257-8972(03)00052-5 ↗
18. Formation, structure and composition of anodic films on AM60 magnesium alloy obtained by DC plasma anodising10.1016/j.corsci.2004.07.038 ↗
19. The effects of process parameters on alternating voltage (AV) passivation of 304 stainless steel10.1016/0010-938X(93)90059-P ↗
20. Optimization of the alternating voltage passivation process for stainless steel10.5006/1.3293474 ↗
21. Effects of AC-modulated passivation and post-treatment on composition and stability of passive films10.5006/1.3316049 ↗
22. Electronic structure study of ac modified passive film on stainless steel10.1179/000705902225002402 ↗
23. Effect of alternating voltage passivation on the corrosion resistance of duple stainless steel10.1007/s10800-008-9718-9 ↗
24. The spatial distribution of Zn2+ during galvanic corrosion of a Zn/steel couple10.1016/j.electacta.2004.01.008 ↗
25. Reactivity at the film/solution interface of ex situ prepared bismuth film electrodes: a scanning electrochemical microscopy (SECM) and atomic force microscopy (AFM) investigation10.1016/j.electacta.2007.07.035 ↗
26. Corrosion resistance of WE43 and AZ91D magnesium alloys with phosphate PEO coating10.1016/j.corsci.2008.03.002 ↗
27. The corrosion of pure magnesium in aerated and deaerated sodium sulphate solutions10.1016/S0010-938X(00)00095-0 ↗
28. Electrochemical study of modified non-functional bis-silane layers on Al alloy 2024-T310.1016/j.corsci.2008.01.018 ↗
29. Corrosion protection properties of hydroxamic acid self-assembled monolayer on carbon steel10.1016/j.corsci.2008.02.008 ↗
30. Use of an Auger parameter for characterizing the Mg chemical state in different materials10.1016/j.surfcoat.2003.10.062 ↗
31. Effect of ball milling on the corrosion resistance of magnesium in aqueous media10.1016/j.electacta.2004.02.001 ↗
32. Nature of the passive film on nickel10.1016/S0013-4686(02)00552-2 ↗
33. The electronic properties of sputtered chromium and iron oxide films10.1016/j.corsci.2003.09.022 ↗
34. The electronic properties of sputtered chromium and iron oxide films10.1016/j.corsci.2004.07.002 ↗
35. Effect of electrolyte additives on performance of plasma electrolytic oxidation film formed on magnesium alloy AZ91D10.1016/j.electacta.2006.10.066 ↗