Breakaway oxidation of Ti3AlC2 during long-term exposure in air at 1100 °C
Source abstract
Abstract
Abstract Catastrophic breakaway oxidation of Ti3AlC2 occurs during long-term oxidation at 1100 °C in air up to 4000 h. Correspondingly, the oxidation kinetics transforms from cubic law to linear law. The transition time is about 3171 h, and the corresponding critical Al content is about 5.99% lower than the initial content. Afterwards, Ti and C start to be oxidized instead of selective oxidation of Al, and Al2O3 scale loses its protectiveness. Meanwhile, voids generated at the Al2O3/Ti3AlC2 interface reduce the oxide scale adhesion. After 3250 h oxidation, Ti3AlC2 still maintains its crystal structure, indicating the capability of bearing great Al lack.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: MXene and MAX Phase Materials · Aluminum Alloys Composites Properties · Advanced Photocatalysis Techniques
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (45)
Show source-provided references
1. The MN+1AXN phases: a new class of solids; thermodynamically stable nanolaminates10.1016/S0079-6786(00)00006-6 ↗
2. Layered machinable and electrically conductive Ti2AlC and Ti3AlC2 ceramics: a review10.1016/S1005-0302(10)60064-3 ↗
3. Elastic and mechanical properties of the MAX phases10.1146/annurev-matsci-062910-100448 ↗
4. MAX phases: bridging the gap between metals and ceramics
5. Damage accumulation and hysteretic behavior of MAX phase materials10.1016/j.jmps.2011.03.012 ↗
6. Electronic and structural properties of the layered ternary carbide Ti3AlC210.1039/b101520f ↗
7. Microstructure and properties of Ti3AlC2 prepared by the solid–liquid reaction synthesis and simultaneous in-situ hot pressing process10.1016/S1359-6454(02)00117-9 ↗
8. Deformation and fracture behavior of ternary compound Ti3SiC2 at 25–1300°C10.1016/S0167-577X(02)00974-6 ↗
9. Room-temperature ductile carbides10.1007/s11661-999-0325-0 ↗
10. Synthesis and thermal and electrical properties of bulk Cr2AlC10.1016/j.scriptamat.2005.11.009 ↗
11. Synthesis and mechanical properties of high-purity Cr2AlC ceramic10.1016/j.msea.2010.12.039 ↗
12. Oxidation behavior of Ti3AlC2 at 1000–1400°C in air10.1016/S0010-938X(02)00177-4 ↗
13. High-temperature oxidation behavior of Ti2AlC in air10.1023/A:1023092027697 ↗
14. High-temperature oxidation and hot corrosion of Cr2AlC10.1016/j.actamat.2007.07.024 ↗
15. Early stages of oxidation of Ti3AlC2 ceramics10.1016/j.matchemphys.2008.06.038 ↗
16. Oxidation behavior of Ti3SiC2-based ceramic at 900–1300°C in air10.1016/S0010-938X(00)00142-6 ↗
17. Microstructures and adhesion of the oxide scale formed on titanium aluminum carbide substrates10.1111/j.1551-2916.2006.01141.x ↗
18. Oxidation behavior of a Ti3AlC2/TiB2 composite at 1000°–1400°C in air10.1111/j.1551-2916.2009.03434.x ↗
19. Oxidation behavior of ODS Fe–Cr–Al alloys: aluminum depletion and lifetime10.1023/A:1024604428747 ↗
20. The effect of aluminum depletion on the oxidation behavior of FeCrAl foil10.1179/mht.2000.014 ↗
21. Life-time extension of alumina forming FeCrAl-RE alloys: influence of alloy thickness10.1179/mht.2000.019 ↗
22. Characterization of the breakaway al content in alumina-forming alloys10.1179/mht.2004.021 ↗
23. The application of a wedge-shaped sample technique for the study of breakaway oxidation in Fe–20Cr–5Al base alloys10.1023/A:1004590915746 ↗
24. Structure stability of Ti3AlC2 in Cu and microstructure evolution of Cu–Ti3AlC2 composites10.1016/j.actamat.2007.03.033 ↗
25. Stability and selective oxidation of aluminum in nano-laminate Ti3AlC2 upon heating in argon10.1021/cm030022v ↗
26. A critical review of the oxidation of Ti2AlC, Ti3AlC2 and Cr2AlC in air, mater
27. Oxidation of Cr2AlC at 1300°C in air10.1016/j.corsci.2007.03.044 ↗
28. Insights into high temperature oxidation of Al2O3-forming Ti3AlC210.1016/j.corsci.2012.01.011 ↗
29. Interfacial segregation, pore formation, and scale adhesion on NiAl alloys10.1007/s11085-005-1954-3 ↗
30. Improved Cr2O3 adhesion by Ce ion implantation in the presence of interfacial sulfur segregation10.1016/j.actamat.2006.07.047 ↗
31. Correlation between the microstructure, growth mechanism, and growth kinetics of alumina scales on a FeCrAlY alloy10.1007/s11661-007-9342-z ↗
32. Growth mechanisms of oxide scales on ODS alloys in the temperature range 1000–1100°C10.1002/maco.19900411204 ↗
33. High temperature healing of Ti2AlC: on the origin of inhomogeneous oxide scale10.1016/j.scriptamat.2011.03.031 ↗
34. Mechanism of isothermal oxidation of the intermetallic TiAl and of TiAl alloys10.1007/BF00665663 ↗
35. Surface analytical investigations on the oxidation behaviour of TiAl-base intermetallics10.1007/BF00321386 ↗
36. Oxidation induced lifetime limits of thin walled, iron based, alumina forming, oxide dispersion strengthened alloy components10.1179/mst.1994.10.2.126 ↗
37. Cyclic oxidation of Ti3AlC2 at 1000–1300°C in air10.1016/j.corsci.2010.09.033 ↗
38. Microstructure and residual stress of alumina scale formed on Ti2AlC at high temperature in Air10.1007/s11085-007-9063-0 ↗
39. Synthesis and characterization of Ti3AlC210.1111/j.1151-2916.2000.tb01281.x ↗
40. Evaluated material properties for a sintered α-alumina10.1111/j.1151-2916.1997.tb03074.x ↗
41. Low temperature dependencies of the elastic properties of Ti4AlN3, Ti3Al1.1C1.8 and Ti3SiC210.1063/1.372080 ↗
42. Determination of the growth stress and strain in α-Al2O3 in scales during the oxidation of Fe–22Cr–4.8Al–0.3Y alloy10.1016/S1359-6454(97)00306-6 ↗
43. Long-term oxidation and phase transformations in aluminized CMSX-4 superalloys10.1016/j.surfcoat.2004.07.091 ↗
44. Deformation and fracture mechanisms of Al2O3/Nb/Al2O3 composites under compression10.3139/146.018070 ↗
45. A first-principles investigation of the phase stability of Ti2AlC with Al vacancies10.1016/j.scriptamat.2007.09.048 ↗