Abstract The effect of SO42− on the corrosion behavior of 316 L stainless steel (SS) in molten FLiNaK (LiF-NaF-KF: 46.5–11.5–42 mol.%) salt was studied. Results reveal that the SO42− in the salt remarkably accelerates the corrosion of 316 L SS by promoting the dissolution of Cr, leading to increasing intergranular corrosion of the alloy. On the other hand, the results of structural characterization indicate that the SO42− can react with Mn to form MnS at the grain boundaries of the alloy. The galvanic couple between MnS and steel matrix could further accelerate the intergranular corrosion of 316 L SS in molten fluoride salt environments.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Molten salt chemistry and electrochemical processes · High Temperature Alloys and Creep
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (44)
Show source-provided references
1. The U.S. DOE Nuclear Energy Research Advisory Committee and the Generation IV International Forum, A technology Roadmap for Generation IV Nuclear Energy Systems, GIF-002-00, 2002.
2. Rosenthal · 1972
3. The molten salt reactor (MSR) in generation IV: overview and perspectives10.1016/j.pnucene.2014.02.014 ↗
4. Sohal · 2010
5. Williams · 2006
6. Corrosion behavior of ZrC-SiC composite ceramics in LiF-NaF-KF molten salt at high temperatures10.1016/j.ceramint.2015.06.143 ↗
7. Effect of oxygen on the corrosion of SiC in LiF-NaF-KF molten salt10.1016/j.corsci.2015.11.014 ↗
8. Materials corrosion in molten LiF-NaF-KF salt10.1016/j.jfluchem.2008.05.008 ↗
9. High-temperature corrosion behavior of superalloys in molten salts-A review10.1080/10408436.2016.1243090 ↗
10. The high-temperature corrosion of Hastelloy N alloy (UNS N10003) in molten fluoride salts analysed by STXM, XAS, XRD, SEM, EPMA, TEM/EDS10.1016/j.corsci.2016.02.010 ↗
11. White · 2010
12. Effect of dissolved oxygen content on stress corrosion cracking of a cold worked 316L stainless steel in simulated pressurized water reactor primary water environment10.1016/j.jnucmat.2013.11.027 ↗
13. The role of deformation mechanisms in flow localization of 316L stainless steel10.1016/j.jnucmat.2006.05.047 ↗
14. Effect of nitrogen on high temperature low cycle fatigue behaviors in type 316L stainless steel10.1016/S0022-3115(97)00360-7 ↗
15. Keiser · 1977
16. Keiser · 1977
17. Metallurgical study on corrosion of austenitic steels in molten salt LiF-BeF2 (Flibe)10.1016/j.jnucmat.2008.12.317 ↗
18. Corrosion of 316 stainless steel in high temperature molten Li2BeF4 (FLiBe) salt10.1016/j.jnucmat.2015.03.004 ↗
19. Corrosion of 316L stainless steel alloy and Hastelloy-N superalloy in molten eutectic LiF-NaF-KF salt and interaction with graphite10.13182/NT13-95 ↗
20. Corrosion of reduced activation ferritic martensitic steel JLF-1 in purified Flinak at static and flowing conditions10.1016/j.fusengdes.2010.03.064 ↗
21. Effect of moisture on corrosion of Ni-based alloys in molten alkali fluoride FLiNaK salt environments10.1016/j.jnucmat.2013.02.021 ↗
22. Effect of CrF3 on the corrosion behaviour of Hastelloy-N and 316L stainless steel alloys in FLiNaK molten salt10.1016/j.corsci.2017.12.008 ↗
23. Effects of the oxidants H2O and CrF3 on the corrosion of pure metals in molten (Li,Na,K)F10.1016/j.corsci.2015.11.032 ↗
24. Effects of Cr3+ on the corrosion of SiC in LiF–NaF–KF molten salt10.1016/j.corsci.2016.10.026 ↗
25. Corrosion of SiC induced by Hastelloy N alloy and its corrosion products in LiF-NaF-KF molten salt10.1016/j.corsci.2016.03.029 ↗
26. Shaffer · 1971
27. Effects of SO42− ions on the corrosion of GH3535 weld joint in FLiNaK molten salt10.1016/j.jnucmat.2017.05.020 ↗
28. Why stainless steel corrodes10.1038/415770a ↗
29. Real time pit initiation studies on stainless steels: the effect of sulphide inclusions10.1016/j.corsci.2006.10.025 ↗
30. Composition changes around sulphide inclusions in stainless steels, and implications for the initiation of pitting corrosion10.1016/j.corsci.2010.07.021 ↗
31. The MnTe-MnS system
32. Chemical reactions involved in the initiation of hot corrosion of B-1900 and NASA-TRW VIA10.1149/1.2123928 ↗
33. Chemical reactions involved in the initiation of hot corrosion of IN-73810.1149/1.2115455 ↗
34. Roine · 2006
35. Mcbride · 1993
36. Thermodynamic properties of inorganic material
37. Knacke · 1991
38. Chase · 1998
39. Effect of S Content on the MnS Precipitation in steel with oxide nuclei10.2355/isijinternational.36.1014 ↗
40. SVET, AFM and AES study of pitting corrosion initiated on MnS inclusions by microinjection10.1016/S0010-938X(02)00222-6 ↗
41. The composition of the boundary region of MnS inclusions in stainless steel and its relevance in triggering pitting corrosion10.1016/j.corsci.2004.05.023 ↗
42. Effects of sulfur addition on pitting corrosion and machinability behavior of super duplex stainless steel containing rare earth metals: part 210.1016/j.corsci.2010.07.002 ↗
43. Surface analysis of corrosion pits initiated at MnS inclusions in 304 stainless steel10.1149/1.2069458 ↗
44. Influence of inclusions on early corrosion development of ultra-low carbon bainitic steel in NaCl solution10.5006/1837 ↗