journal article·2021-02

Effect of cathodic polarisation on stress corrosion cracking behaviour of a Ni(Fe, Al)-maraging steel in artificial seawater

Tianliang Zhao, Shiqi Wang, Zhiyong Liu, Cuiwei Du, Xiaogang Li

Corrosion Science· Volume 179
Publisher page

Abstract

Abstract The effect of cathodic polarisation on stress corrosion cracking (SCC) behaviour of peak-aged Ni(Fe, Al)-maraging steel in artificial seawater was investigated. The steel shows better compatibility of strength and hydrogen embrittlement (HE) resistance than reported 18Ni-type maraging steels when potential is above −850 mV. This advantage stems from the abundant and evenly dispersed Ni(Fe, Al) nanoprecipitates. SCC occurs above −850 mV in a transgranular/intergranular-mixed manner involving a mechanics-dominant-anodic-dissolution-promoted mechanism and below −850 mV in an intergranular manner along parent austenite grain boundaries involving HE. For interpreting the HE mechanism, a novel model is proposed based on hydrogen-weakening interatomic bonds.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Corrosion Behavior and Inhibition · Microstructure and Mechanical Properties of Steels

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (76)

Show source-provided references
1. Hydrogen embrittlement of ultra high strength 300 grade maraging steel10.1016/j.corsci.2015.06.022 ↗
2. Effect of 4-(N,N-diethylamino)benzaldehyde thiosemicarbazone on the corrosion of aged 18 Ni 250 grade maraging steel in phosphoric acid solution10.1016/j.corsci.2011.07.014 ↗
3. Materials science: share corrosion data10.1038/527441a ↗
4. Hydrogen embrittlement of an automotive 1700 MPa martensitic advanced high-strength steel10.1016/j.corsci.2020.108726 ↗
5. Fundamental investigation of stress corrosion cracking of E690 steel in simulated marine thin electrolyte layer10.1016/j.corsci.2018.12.029 ↗
6. Stress corrosion cracking of E690 steel as a welded joint in a simulated marine atmosphere containing sulphur dioxide10.1016/j.corsci.2015.08.039 ↗
7. Crack growth behaviour of E690 steel in artificial seawater with various pH values10.1016/j.corsci.2019.108336 ↗
8. Electrochemical corrosion, hydrogen permeation and stress corrosion cracking behavior of E690 steel in thiosulfate-containing artificial seawater10.1016/j.corsci.2018.08.048 ↗
9. Crack tip chemistry and electrochemistry of environmental cracks in AA 705010.1016/j.corsci.2006.12.001 ↗
10. Modelling the electrochemical crack size effect on stress corrosion crack growth rate10.1016/j.corsci.2017.06.016 ↗
11. Environmentally assisted cracking mechanism of pipeline steel in near-neutral pH groundwater10.1016/j.corsci.2010.02.020 ↗
12. The effect of crack tip environment on crack growth behaviour of a low alloy steel at cathodic potentials in artificial seawater10.1016/j.jmst.2020.04.034 ↗
13. Quanttitative study of the corrosion evolution and stress corrosion cracking of high strength aluminum alloys in solution and thin electrolyte layer containing Cl-
14. A mechanism behind hydrogen-assisted fatigue crack growth in ferrite-pearlite steel focusing on its behavior in gaseous environment at elevated temperature10.1016/j.corsci.2020.108558 ↗
15. Effects of cathodic polarisation on corrosion fatigue life of E690 steel in simulated seawater10.1016/j.ijfatigue.2018.01.008 ↗
16. Mechanistic aspect of near-neutral pH stress corrosion cracking of pipelines under cathodic polarisation10.1016/j.corsci.2011.10.002 ↗
17. Predictive approaches to stress corrosion cracking failure10.1016/0010-938X(80)90128-6 ↗
18. Combined effect of cathodic potential and sulfur species on calcareous deposition, hydrogen permeation, and hydrogen embrittlement of a low carbon bainite steel in artificial seawater10.1016/j.corsci.2019.07.013 ↗
19. A generalised model for hydrogen embrittlement
20. Hydrogen-enhanced localised plasticity—a mechanism for hydrogen-related fracture10.1016/0921-5093(94)90975-X ↗
21. The role of hydrogen and other interstitials in the mechanical behavior of metals, metall10.1007/s13632-016-0319-4 ↗
22. Environmentally assisted cracking: overview of evidence for an adsorption-induced localised-slip process10.1016/0001-6160(88)90113-7 ↗
23. Hydrogen thermal desorption relevant to delayed-fracture susceptibility of high-strength steels10.1007/s11661-001-0265-9 ↗
24. Birnbaum · 1997
25. Mechanisms of hydrogen assisted cracking - a review
26. Environmentally assisted cracking of 18%Ni maraging steel10.1016/j.corsci.2009.04.011 ↗
27. Stress corrosion cracking of maraging steel weldments10.1179/026708303225010632 ↗
28. Susceptibility to pitting and stress corrosion cracking of aged 18 wt.% Ni maraging alloy in synthetic sea water10.1016/0921-5093(90)90259-6 ↗
29. Hydrogen embrittlement of a Ti-strengthened 250 grade maraging steel10.1007/s11665-997-0011-6 ↗
30. Embrittlement of T-200 maraging steel in a hydrogen sulfide solution10.1016/j.corsci.2004.06.017 ↗
31. Environmentally assisted cracking susceptibility of dark etched HAZ/ parent metal interface region of 18Ni 250 maraging steel weldment10.1016/j.msea.2020.138911 ↗
32. Microstructure effect on hydrogen-induced cracking in TM210 maraging steel10.1016/j.msea.2013.07.097 ↗
33. Beneficial effect of reversed austenite on the intergranular corrosion resistance of martensitic stainless steel10.1016/j.corsci.2019.02.020 ↗
34. Stress corrosion cracking behaviour of gas tungsten arc and friction stir maraging steel welds10.1016/j.matpr.2018.08.186 ↗
35. Microstructural evolution and mechanical properties of maraging steel produced by wire+arc additive manufacture process10.1016/j.matchar.2017.12.002 ↗
36. The effect of prior austenite grain size on hydrogen embrittlement of Co-containing 18Ni 300 maraging steel10.1016/j.ijhydene.2019.05.074 ↗
37. Microstructural evolution in 13Cr–8Ni–2.5Mo–2Al martensitic precipitation-hardened stainless steel10.1016/j.msea.2004.12.002 ↗
38. Response of hydrogen trapping capability to microstructural change in tempered Fe–0.2C martensite10.1016/j.scriptamat.2004.11.008 ↗
39. Effect of aging treatment on apparent hydrogen solubility and trapping in a new generation maraging steel10.1016/j.scriptamat.2020.03.013 ↗
40. Quantitative analysis on hydrogen trapping of TiC particles in steel10.1007/s11661-006-0004-3 ↗
41. Diffusion and trapping of hydrogen due to elastic interaction with η-Ni3Ti precipitates in Custom 465® stainless steel10.1016/j.ijhydene.2019.09.197 ↗
42. A review of underlying reasons for intergranular cracking for a variety of failure modes and materials and examples of case histories10.1016/j.engfailanal.2019.02.027 ↗
43. The effect of grain size and aging on hydrogen embrittlement of a maraging steel10.1016/j.corsci.2008.06.044 ↗
44. Hydrogen effects on the interaction between dislocations10.1016/S1359-6454(97)00349-2 ↗
45. Experimental study of hydrogen embrittlement in maraging steels10.1016/j.prostr.2017.12.049 ↗
46. Corrosion fatigue crack initiation and initial propagation mechanism of E690 steel in simulated seawater10.1016/j.msea.2017.09.078 ↗
47. Effect of prior austenite grain boundaries on corrosion fatigue behaviors of E690 high strength low alloy steel in simulated marine atmosphere10.1016/j.msea.2019.138884 ↗
48. A study on stress corrosion cracking and hydrogen embrittlement of Jethete M152 martensitic stainless steel10.1016/j.msea.2018.10.091 ↗
49. Hydrogen embrittlement (HE) phenomena and mechanisms
50. Interaction between hydrogen and cyclic stress and its role in fatigue damage mechanism10.1016/j.corsci.2019.05.028 ↗
51. Ultrastrong steel via minimal lattice misfit and high-density nanoprecipitation10.1038/nature22032 ↗
52. Mechanistic aspect of non-steady electrochemical characteristic during stress corrosion cracking of an X70 pipeline steel in simulated underground water10.5006/1153 ↗
53. Stress corrosion cracking behavior of X70 pipe steel in an acidic soil environment10.1016/j.corsci.2008.05.011 ↗
54. Stress-induced hydrogen redistribution and corresponding fracture behavior of Q960E steel at different hydrogen content10.1016/j.msea.2020.138963 ↗
55. Microstructure and strain path in deep-drawing10.1016/0001-6160(77)90083-9 ↗
56. Deformation mechanism and texture and microstructure evolution during high-speed rolling of AZ31B Mg sheets10.1007/s10853-008-3021-3 ↗
57. EBSD study of micromechanisms involved in high deformation ability of DP steels10.1016/j.matdes.2015.07.134 ↗
58. Pits formation and stress corrosion cracking behavior of Q345R in hydrofluoric acid10.1016/j.corsci.2020.108443 ↗
59. Influence of inclusions on initiation of pitting corrosion and stress corrosion cracking of X70 steel in near-neutral pH environment10.1016/j.corsci.2018.11.007 ↗
60. Mechanism-related modelling of pit evaluation in the CrNiMoV steel in simulated environment of low pressure nuclear steam turbine10.1016/j.matdes.2016.05.058 ↗
61. Gutman · 1994
62. Stress corrosion cracking of ultrahigh strength martensite steel Cr9Ni5MoCo14 in 3.5% NaCl solution10.1016/j.ast.2014.03.004 ↗
63. Effect of cathodic potentials on the hydrogen embrittlement susceptibility of 10Ni5CrMo steel10.20964/2019.09.17 ↗
64. Effect of cathodic potential on stress corrosion cracking behavior of different heat-affected zone microstructures of E690 steel in artificial seawater
65. Characteristics of hydrogen embrittlement in high-pH stress corrosion cracking of X100 pipeline steel in carbonate/ bicarbonate solution10.1016/j.conbuildmat.2020.120124 ↗
66. Mechanistic aspect of stress corrosion cracking of X80 pipeline steel under non-stable cathodic polarisation10.1016/j.elecom.2014.08.016 ↗
67. Effect of sulfate-reducing bacteria and cathodic potential on stress corrosion cracking of X70 steel in sea-mud simulated solution10.1016/j.msea.2018.02.007 ↗
68. Hydrogen embrittlement of high strength steam turbine last stage blade steels: comparison between PH17-4 steel and PH13-8Mo steel10.1016/j.msea.2018.10.086 ↗
69. Hydrogen embrittlement susceptibility and permeability of two ultra-high strength steels10.1016/j.corsci.2005.05.042 ↗
70. Aging condition and trapped hydrogen effects on the mechanical behavior of a precipitation hardened martensitic stainless steel10.1016/j.jallcom.2019.07.112 ↗
71. Understanding how hydrogen influences the mechanical properties of iron and steel
72. Hydrogen embrittlement: mechanisms
73. The predominant role of strain-induced vacancies in hydrogen embrittlement of steels: overview10.1016/j.actamat.2018.12.013 ↗
74. Hydrogen related fracture of metals
75. Hydrogen-enhanced localisation of plasticity in an austenitic stainless steel10.1007/BF02669644 ↗
76. Birnbaum · 2000