Transient and steady state crack growth kinetics for stress corrosion cracking of a cold worked 316L stainless steel in oxygenated pure water at different temperatures
Source abstract
Abstract
Abstract The stress corrosion cracking (SCC) growth kinetics for a cold worked 316L stainless steel was continuously monitored in high purity water at different temperatures and dissolved oxygen (DO) levels under a K (or K max ) of 30 MPa m 0.5 . The total SCC test time was more than 8000 h to make sure the steady state crack growth rate under each test condition could be reached. Crack growth rate (CGR) increases with increasing temperature in the range 110–288 °C. A typical intergranular-cracking mode is identified. Depending on the previous test condition, especially the temperature, three kinds of crack growth kinetics, i.e., increasing with testing time then becoming steady, being constant during the whole period, or decreasing with test time then becoming steady, are identified and discussed. Time-dependent and testing history-dependent crack growth modes were confirmed in two series of tests in 2 ppm DO and 7.5 ppm DO pure water. The apparent activation energies are calculated and compared with other data in different environments under different applied loading levels for understanding the cracking mechanism.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Corrosion Behavior and Inhibition · Non-Destructive Testing Techniques
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (27)
Show source-provided references
1. Ford · Corrosion · 1979 · 35 · 56910.5006/0010-9312-35.12.569 ↗
2. Andresen · Materials Science and Engineering A: Structural Materials Properties Microstructure and Processing · 1988 · 103 · 16710.1016/0025-5416(88)90564-2 ↗
3. R.L. Jones, G.M. Gordon, G.H. Neils, Environmental degradation of materials in boiling water reactors, in: Proceedings of the Fourth International Symposium Environmental Degradation Materials Nuclear Power Systems-Water Reactors, NACE, 1989, pp. 1–10.
4. T.M. Angeliu, P.L. Andresen, E. Hall, J.A. Sutliff, S. Sitzman, R.M. Horn, Intergranular Stress Corrosion Cracking of Unsensitized Stainless Steels in BWR Environments, in: Proceedings of the Ninth International Symposium Environmental Degradation Materials Nuclear Power Systems-Water Reactors, TMS, 1999, pp. 311–317.10.1002/9781118787618.ch31 ↗
5. T. Shoji, Progress in the mechanistic understanding of BWR SCC and its implication to the prediction of SCC growth behavior in plants, in: Proceedings of the 11th International Symposium Environmental Degradation Materials Nuclear Power Systems-Water Reactors, ANS, 2003, pp. 588–598.
6. Suzuki · Maintenology · 2004 · 3 · 65
7. A.K. Agrawal, G.A. Begley, R.W. Staehle, Stress Corrosion of Sensitized and Quench Annealed Type 304 Stainless Steels in High Purity Water, Corroion/78, NACE, Paper No. 187, 1978.
8. Ruther · Corrosion · 1988 · 44 · 79110.5006/1.3584950 ↗
9. Andresen · Corrosion · 1993 · 49 · 71410.5006/1.3316104 ↗
10. Weeks · Corrosion Science · 1985 · 25 · 75710.1016/0010-938X(85)90009-5 ↗
11. Hale · Journal of Engineering Materials and Technology: Transactions ASME · 1986 · 108 · 4410.1115/1.3225840 ↗
12. R. Magdowski, M.O. Speidel, Effect of Temperature on Stress Corrosion Crack Growth in Austenitic Stainless Steels Exposed to Water, Corrosion/90, NACE, Paper No. 291, 1990.
13. A. Jenssen, C. Jansson, Effects of temperature on crack growth rate in sensitized type 304 stainless steel in pure and sulfate bearing BWR environments, in: Proceedings of the 10th International Symposium Environmental Degradation Materials Nuclear Power Systems-Water Reactors, NACE, 2001 (CDROM).
14. P.L. Andresen, T.M. Angeliu, L.M. Young, Effect of Martensite and Hydrogen on SCC of Stainless Steels and Alloy 600, Corrosion/2001, NACE, Paper No.228, 2001.
15. Mostovoy · Journal of Materials · 1967 · 2 · 661
16. H. Nakajima, T. Shoji, M. Kikuchi, H. Nitsuma, M. Shindo, Detecting acoustic emission during cyclic crack growth in simulated BWR environments, in: S.J. Hudak, R.J. Bucci (Eds.), ASTM STP 738, ASTM, 1981, p. 139.10.1520/STP33458S ↗
17. Z.P. Lu, T. Shoji, Y. Takeda, Y. Ito, S. Yamazaki, N. Tsuchiya, Effects of loading mode and temperature on stress corrosion cracking growth behaviour of strain-hardened 316L stainless steels in oxygenated pure water, in: Proceedings of the 13th International Symposium Environmental Degradation Materials Nuclear Power Systems-Water Reactors, August 2007.
18. Z.P. Lu, A. Kai, Y. Ito, Y. Takeda, T. Shoji, SCC growth behavior of cold worked 316L stainless steel in oxygenated pure water at different temperatures, in: Proceedings of the 52nd Japan Conference Materials and Environments, JSCE, 2005, p. 205.
19. T. Shoji, S. Suzuki, R.G. Ballinger, Theoretical prediction of SCC growth behavior-threshold and plateau growth rate, in: Proceedings of the Seventh International Symposium Environmental Degradation Materials Nuclear Power Systems-Water Reactors, NACE, 1995, pp. 881–891.
20. P.L. Andresen, Probabilistic Interpretation of SCC Initiation and Growth, Corrosion/99. NACE, Paper No. 446, 1999.
21. G.B. Naumov, B.N. Ryzhenko, I.L. Khodakovsky, Translated by G.J. Soleimani, Handbook of Thermodynamic Data, US Geological Survey, Menlo Park, 1974.
22. Vankeerberghen · Corrosion Science · 2002 · 44 · 142510.1016/S0010-938X(01)00151-2 ↗
23. P.M. Scott, C. Benhamou, An overview of recent observation and interpretation of IGSCC in nickel base alloys in PWR primary water, in: Proceedings of the 10th International Symposium Environmental Degradation Materials Nuclear Power Systems-Water Reactors, NACE, 2001 (CDROM).
24. Ford · Corrosion · 1996 · 52 · 37510.5006/1.3292125 ↗
25. T. Shoji, Z.P. Lu, Y. Takeda, Understanding the threshold conditions for stress corrosion cracking in light water reactor environments based on the deformation/oxidation mechanism, in: ASME Pressure Vessels and Piping Division Conference (ASME PVP 2007/Creep8), ASME, Paper No. PVP2007-26183, 2007.10.1115/PVP2007-26183 ↗
26. Bard · 2001
27. Turnbull · Corrosion Science · 1997 · 39 · 78910.1016/S0010-938X(97)89342-0 ↗