Microstructure and corrosion resistance of Cr/Cr2N multilayer film deposited on the surface of depleted uranium
Source abstract
Abstract
Abstract Depleted uranium is widely used in national defence and nuclear energy fields. However, the inferior corrosion resistance limits its application. A Cr/Cr 2 N film was prepared by magnetron sputtering on the uranium to improve its corrosion resistance. The Cr/Cr 2 N film exhibits modulation structure. The introduction of the Cr/Cr 2 N increases the corrosion potential; the corresponding current density decreases about three orders of magnitude. After polarization corrosion, the surface morphology of the Cr/Cr 2 N-coated on uranium keeps integrated. Only a thin layer of film (∼40 nm) is oxidized. The Cr/Cr 2 N film shows great potential in improving oxidation and corrosion resistance of depleted uranium.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Metal and Thin Film Mechanics · Nuclear Materials and Properties · Fusion materials and technologies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (28)
Show source-provided references
1. Wilkinson · 1962
2. A review of the rates of reaction of uranium with oxygen and water vapour at temperatures up to 300°C10.1016/0022-3115(81)90557-2 ↗
3. Oxidation of mechanisms and catalytic properties of the actinides10.1016/0079-6786(84)90003-7 ↗
4. The kinetics of the uranium–oxygen–water vapour reaction between 40 and 100°C10.1016/0022-3115(86)90030-9 ↗
5. Studies of the kinetics and mechanism of the oxidation of uranium by dry and moist air A model for determining the oxidation rate over a wide range of temperatures and water vapour pressures10.1016/0022-3115(94)90200-3 ↗
6. Corrosion of uranium in air and water vapor: consequences for environmental dispersal10.1016/S0925-8388(98)00639-2 ↗
7. Depleted uranium and radiation-induced lung cancer and leukaemia10.1259/bjr.74.884.740677 ↗
8. Toxicity of depleted uranium10.1016/S0140-6736(00)03605-9 ↗
9. L.J. Weirick, Hot-dipped tin–zinc on U-0. 75 w/o Ti, SAND-79-0478, pp. 1–46.
10. Assessment of corrosion-resistant coatings for a depleted uranium-0.75 titanium alloy10.1016/0257-8972(91)90126-H ↗
11. Adhesion and corrosion behavior of Al–Zn and TiN/Ti/TiN coatings on a DU-0.75wt.% Ti alloy10.1016/0257-8972(91)90037-W ↗
12. TiN, TiN gradient and Ti/TiN multi-layer protective coatings on Uranium10.1016/j.surfcoat.2006.09.126 ↗
13. Long-term amorphisation of C+and N2+ implanted layers on a uranium surface10.1016/S0925-8388(02)00017-8 ↗
14. Passivation of uranium towards air corrosion by N2+and C+ion implantation10.1016/S0022-3115(00)00335-4 ↗
15. Superhard coatings materials10.1557/mrs2003.56 ↗
16. Different approaches to superhard coatings and nanocomposites10.1016/j.tsf.2004.10.053 ↗
17. High-temperature oxidation of CrN/AlN multilayer coatings10.1016/j.apsusc.2005.02.105 ↗
18. Corrosion-wear behaviour of PVD Cr/CrN multilayer coatings for gear applications10.1016/j.triboint.2008.06.015 ↗
19. Multi-technique study of corrosion resistant CrN/Cr/CrN and CrN:C coatings10.1016/j.surfcoat.2005.11.128 ↗
20. Magnetron sputtering: a review of recent developments and applications10.1016/S0042-207X(99)00189-X ↗
21. Effect of bilayer period on properties of Cr/CrN multilayer coatings produced by laser ablation10.1016/j.surfcoat.2007.12.036 ↗
22. Investigation of atmospheric corrosion of Zn using ac impedance and differential pressure meter10.1016/j.electacta.2004.01.033 ↗
23. The effect of preferred orientation on the mechanical properties of chromium nitride coatings deposited on SKD11 by unbalanced magnetron sputtering10.1016/S0167-577X(02)00958-8 ↗
24. Surface analysis of electrochemically stripped CrN coatings10.1016/j.surfcoat.2006.08.110 ↗
25. XPS investigations of chromium nitride thin films10.1016/j.surfcoat.2005.02.091 ↗
26. Repetitive nucleation of corrosion pits on stainless steel and the effects of surface roughness10.1149/1.1416503 ↗
27. The effect of temperature on the nucleation of corrosion pits on titanium in Ringer’s physiological solution10.1016/j.biomaterials.2004.02.023 ↗
28. Combined anodic/cathodic transient currents within nucleating pits on Al–Fe alloy surfaces10.1016/j.corsci.2010.11.008 ↗