Carbon steel corrosion under anaerobic–aerobic cycling conditions in near-neutral pH saline solutions – Part 1: Long term corrosion behaviour

B.W.A. Sherar, P.G. Keech, D.W. Shoesmith

Corrosion Science· Volume 53· Issue 11
Publisher page

Abstract

Abstract The influence of anaerobic–aerobic cycling on pipeline steel corrosion was investigated in near-neutral carbonate/sulphate/chloride solution (pH 9) over 238 days. The corrosion rate increased and decreased as exposure conditions were switched between redox conditions. Two distinct corrosion morphologies were observed. The majority of the surface corroded uniformly to produce a black magnetite/maghemite layer approximately 4.5 μm thick. The remaining surface was covered with an orange tubercle, approximately 3–4 mm in cross section. Analysis of the tubercle cross section revealed a single large pit approximately 275 μm deep. Repeated anaerobic–aerobic cycling localized the corrosion process within this tubercle-covered pit.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Corrosion Behavior and Inhibition · Building materials and conservation · Concrete Corrosion and Durability

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (20)

Show source-provided references
1. C.L. Durr, J.A. Beavers, Techniques for Assessment of Soil Corrosivity, in: CORROSION/98, NACE, Houston, TX, 1998.10.5006/C1998-98667 ↗
2. Indicator minerals formed during external corrosion of line pipe
3. External corrosion of line pipe - A summary of research activities
4. Evaluation of deoxygenation as a corrosion control measure for ballast tanks10.5006/1.3278153 ↗
5. External corrosion of line pipe part I: indentification of bacterial corrosion in the field
6. Localized dissolution of millscale-covered pipeline steel surfaces10.5006/1.3287824 ↗
7. Nominally anaerobic corrosion of carbon steel in near-neutral ph saline environments10.5006/1.3381566 ↗
8. Application of Mossbauer spectroscopy to the study of corrosion10.1023/B:HYPE.0000024714.84742.fd ↗
9. Carbon steel corrosion under anaerobic–aerobic cycling in near-neutral pH saline solutions. Part 2: Corrosion Mechanism10.1016/j.corsci.2011.07.008 ↗
10. Bockris · 1970
11. B. Sherar, P. Keech, Z. Qin, F. King, R. Worthingham, D. Shoesmith, Long Term Corrosion Behaviour of Carbon Steel During Anaerobic to Aerobic Cycling Under Near-Neutral pH Saline and Sulphide Conditions, in: IPC 2010, ASME, Calgary, AB, 2010.10.1115/IPC2010-31164 ↗
12. Electrochemical polarization: I A theoretical analysis of the shape of polarization curves10.1149/1.2428496 ↗
13. F. King, T.R. Jack, Role of Redox and Corrosion Potentials in the Corrosion of Line Pipe Steel in, Pipeline Research Council International, 2001.10.55274/R0010374 ↗
14. The preparation of magnetite, goethite, hematite and maghemite of pigment quality from mill scale iron waste10.1016/j.dyepig.2006.01.038 ↗
15. Mechanism of oxide film formation on iron in simulating groundwater solutions: Raman spectroscopic studies10.1016/S0010-938X(97)00141-8 ↗
16. Raman-spectroscopic investigation of the structure of silicate-glasses. 3 Raman intensities and structural units in sodium-silicate glasses10.1063/1.442472 ↗
17. Effect of silicon content on the corrosion properties of calcium-modified weathering steel in a chloride environment10.5006/1.3277648 ↗
18. Characterisation of initial atmospheric corrosion carbon steels by field exposure and laboratory simulation10.1016/j.corsci.2007.01.009 ↗
19. In situ studies of filiform corrosion of iron10.1149/1.1645263 ↗
20. Oxide formation and conversion on carbon steel in mildly basic solutions10.1016/j.electacta.2009.05.020 ↗