Abstract

The corrosion resistances and passivation of austenitic 316L and duplex 2205 powder metallurgical (P/M) steels, produced by gas atomizing and hot isostatic pressing (HIP), have been compared with those of their conventional cast counterparts. P/M 316L steel is shown to have significantly higher pitting corrosion resistance than conventional 316L steel in 0.5 M HCl. This effect is ascribed to the fine grained microstructure of the P/M 316L steel yielding an improved passive layer. The latter hypothesis is supported by photoelectron spectroscopy data demonstrating differences between the thickness and composition of the passive layers for the 316L steels.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · High Temperature Alloys and Creep · Corrosion Behavior and Inhibition

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (41)

Show source-provided references
1. Surface-analysis of passive state10.1016/0010-938X(90)90095-M ↗
2. The composition of the surface during passivation of stainless steels10.5006/1.3577318 ↗
3. B. Brox, I. Olefjord, Preferential Dissolution of Iron during Polarization of Stainless Steels in: Stainless Steel 84, The institute of metals, London, UK, Gothenburg, Sweden, 1984.
4. The passivity of iron–chromium alloys10.1016/0010-938X(89)90060-7 ↗
5. Passive films on stainless steels – chemistry, structure and growth10.1016/S0013-4686(02)00841-1 ↗
6. Investigation of corrosion and wear properties of Fe based metal matrix composites consolidated by sintering and hot isostatic pressing10.1179/003258910X12678035166656 ↗
7. Microstructure and corrosion properties of nitrogen stainless steel 316L produced by hipping10.1179/003258904225015428 ↗
8. Development of powder metallurgy high nitrogen stainless steel10.4028/www.scientific.net/MSF.638-642.1811 ↗
9. Corrosion behavior of P/M components for gasoline injectors
10. HIP powder metal near-net shapes for demanding environment and applications10.1016/S1006-706X(08)60064-3 ↗
11. G. Raisson, Technical development for NS and NNS parts in Europe, in: International Conference on Hot Isostatic Pressing, Kobe, Japan, 2011.
12. High nitrogen corrosion resistant austenitic stainless steels produced by HIP P/M processing10.4028/www.scientific.net/MSF.318-320.635 ↗
13. Development of properties of P/M austenitic stainless steels by nitrogen infusion10.2355/isijinternational.36.938 ↗
14. Super duplex stainless-steels10.1179/mst.1992.8.8.685 ↗
15. Chloride-induced stress corrosion cracking10.5006/1.3293641 ↗
16. Corrosion behaviour and microstructure in 254 SMO-comparison between conventional and P/M HIP production
17. Corrosion behavior of vacuum sintered duplex stainless steels10.1016/j.jmatprotec.2007.03.014 ↗
18. Corrosion behaviour of duplex stainless steels sintered in nitrogen10.1016/j.corsci.2008.10.003 ↗
19. Pitting corrosion behaviour of PM austenitic stainless steels sintered in nitrogen–hydrogen atmosphere10.1016/j.corsci.2006.10.009 ↗
20. Effect of nitrogen content on precipitation during isothermal annealing of P/M high nitrogen austenitic stainless steels10.4028/www.scientific.net/MSF.318-320.673 ↗
21. P/M processing routes for high nitrogen martensitic stainless steels
22. Atmospheric oxidation of a Nb–Zr alloy studied with XPS10.1016/S0010-938X(03)00139-2 ↗
23. Calculation of electron inelastic mean free paths (IMFPs) VII. Reliability of the TPP-2M IMFP predictive equation10.1002/sia.1526 ↗
24. The passivity of AISI 316L stainless steel in 0.05M H2SO410.1007/s10800-009-0016-y ↗
25. XPS analysis of manganese in stainless steel passive films on 1.4432 and the lean duplex 1.416210.1016/j.corsci.2010.03.014 ↗
26. Corrosion behavior and passive film chemistry of 216L stainless steel in sulphuric acid10.1007/s10853-008-2976-4 ↗
27. Production and breakdown of passivity of metals10.1016/S0010-938X(67)80023-4 ↗
28. Mechanisms of Pitting Corrosion
29. Pitting and sulfide inclusions in steel10.1016/S0010-938X(74)80047-8 ↗
30. K.R. Tretheway, J. Chamberlain, Crevice and pitting corrosion, in: Corrosion for Students of Science and Engineering, Longman Group UK Limited, 1988.
31. Chaotic analysis of electrochemical noise measured on stainless-steel10.1149/1.2044205 ↗
32. Electrochemistry of chromium-base binary metallic glasses10.1016/0025-5416(88)90390-4 ↗
33. Jones · 1996
34. Electrochemical conditions within small pits10.1016/0010-938X(76)90117-7 ↗
35. XPS study of the growth and reactivity of Fe/Mno thin-films10.1016/0039-6028(95)00190-5 ↗
36. The Influence of nitrogen and molybdenum on passive films formed on the austenoferritic stainless-steel-2205 studied by AES and XPS10.1016/0010-938X(94)00148-Y ↗
37. Electrochemical corrosion behaviour of nanocrystalline materials–a review10.1016/S1005-0302(10)60001-1 ↗
38. The remarkable effect of austenitic stainless steel in sulphuric acid solution and the effect of repetitive temperature cycling10.1016/j.corsci.2009.07.010 ↗
39. Graph theory and the passivity of binary alloys10.1016/S0010-938X(00)00038-X ↗
40. On the origin of the spontaneous potential oscillations observed during galvanostatic deposition of layers of Cu and Cu2O in alkaline citrate solutions10.1016/j.jelechem.2006.05.019 ↗
41. Högfeldt · 1982