Hot corrosion behavior of NiCoCrAlYTa coating deposited on Inconel alloy substrate by high velocity oxy-fuel spraying upon exposure to molten V 2 O 5 -containing salts
Source abstract
Abstract
Abstract The corrosion behavior of the HVOF-sprayed NiCoCrAlYTa coating upon exposure to molten V2O5 and molten mixture of 50 wt.% V2O5 + 50 wt.% Na2SO4 at 800–1000 °C was discussed. The hardness, elastic modulus and contact stiffness of the coating were determined by nano-indentation test. Results indicate that the coating exhibits good corrosion resistance, which is ascribed to the formation of Al and Cr oxide protective film. The generation of hard phases Al2O3 and Cr2O3 with loose structure and Laves phase Cr2Ta lead to the increase of the hardness and elastic modulus of the corroded coatings and the decrease of contact stiffness.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: High-Temperature Coating Behaviors · Advanced materials and composites · High Entropy Alloys Studies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (47)
Show source-provided references
1. Evolution of hot corrosion behavior of YSZ-Ta2O5 composites with different YSZ/Ta2O5 ratios10.1111/ijac.12224 ↗
2. Hot corrosion behavior of a centimeter Fe-based amorphous composite coating prepared by laser cladding in molten Na2SO4+K2SO4 salts10.1016/j.surfcoat.2015.03.022 ↗
3. Hot corrosion of some superalloys and role of high-velocity oxy-fuel spray coatings—a review10.1016/j.surfcoat.2004.10.056 ↗
4. High temperature corrosion behaviour of some Fe-, Co- and Ni-base superalloys in the presence of Y2O3 as inhibitor10.1016/j.apsusc.2009.03.040 ↗
5. Hot corrosion behavior of solution precursor and atmospheric plasma sprayed thermal barrier coatings10.1016/j.corsci.2015.05.034 ↗
6. Hot corrosion behavior of LaTi2Al9O19 ceramic exposed to vanadium oxide at temperatures of 700–950°C in air10.1016/j.corsci.2015.12.024 ↗
7. High-temperature oxidation and hot corrosion studies on NiCrAlY coatings deposited by flame-spray technique10.1007/s11666-015-0237-z ↗
8. Hot corrosion in gas turbine components10.1016/S1350-6307(00)00035-2 ↗
9. Hot corrosion of YSZ/Al2O3 dispersed NiCrAlY plasma-sprayed coatings in Na2SO4–10wt.% NaCl melt10.1016/j.corsci.2010.04.007 ↗
10. Preparation and hot corrosion behaviour of Pt modified AlSiY coating on a Ni-based superalloy10.1016/j.corsci.2015.12.007 ↗
11. Effect of alumina dispersion on oxidation behavior as well as friction and wear behavior of HVOF-sprayed CoCrAlYTaCSi coating at elevated temperature up to 1000°C10.1016/j.actamat.2015.05.025 ↗
12. Hot corrosion behaviour of HVOF-sprayed NiCrBSi coatings on Ni- and Fe-based superalloys in Na2SO4–60% V2O5 environment at 900°C10.1016/j.actamat.2005.10.009 ↗
13. Hot corrosion behavior of HVOF-sprayed CoNiCrAlYSi coatings in a sulphate environment10.1016/j.vacuum.2015.09.015 ↗
14. Corrosion and erosion–corrosion behaviour of activated combustion high-velocity air fuel sprayed Fe-based amorphous coatings in chloride-containing solutions10.1016/j.corsci.2015.05.044 ↗
15. Hot corrosion and performance of nickel-based coatings
16. Improving hot corrosion resistance of cobalt based superalloy (Superco-605) using HVOF sprayed oxide alloy powder coating10.1007/s12666-015-0605-x ↗
17. Erosion of thermal spray MCr–Cr3C2 cermet coatings10.1016/S0043-1648(98)00298-1 ↗
18. Hot corrosion performance of AlO-CrO/NiCoCrAlYTa and AlO/NiCoCrAlYTa coatings deposited by atmospheric plasma spraying
19. Microstructure and mechanical properties of NiCoCrAlYTa alloy processed by press and sintering route10.1016/j.matchar.2015.02.001 ↗
20. Atom probe tomographic study of L10 martensite in a Pt-modified NiCoCrAlYTa bond coating10.1016/j.corsci.2013.07.041 ↗
21. Stepwise depletion of coating elements as a result of hot corrosion of NiCrAlY coatings10.1007/s11665-013-0774-x ↗
22. Comparison of oxidation resistance of NiCoCrAlTaY-coated and −uncoated Mar-M247 superalloys in the air at 1150°C10.1007/s10853-011-6041-3 ↗
23. Isothermal oxidation behavior of NiCoCrAlTaY coating deposited by high velocity air-fuel spraying10.1007/s11666-012-9740-7 ↗
24. Isothermal oxidation behaviour of NiCoCrAlYTa coatings produced by HVOF spraying and tribomet™ process10.1007/s11085-013-9422-y ↗
25. Microstructural evolution on NiCoCrAIYTa coated AM-3 single crystal superalloy—influence of pre-creep treatments10.1080/10426919508935044 ↗
26. Laser-induced microstructural modifications in a vacuum plasma sprayed NiCoCrAlYTa coating10.1016/0257-8972(87)90099-5 ↗
27. Hot corrosion behaviour of D-gun sprayed NiCoCrAlYTa coated superalloys at 900°C in molten salt environment10.1179/026708410X12459349720132 ↗
28. The single-crystal Raman spectra of nearly opaque materials: iron(III) oxide and chromium(III) oxide10.1039/j19700000980 ↗
29. Crystal structure and vibrational spectra of AlVO4. A DFT study10.1021/jp046055v ↗
30. Generation of Brønsted acid sites on Al2O3-supported Ta2O5 calcined at high temperatures10.1016/j.cattod.2012.02.035 ↗
31. Raman spectroscopic study of Ni/Al2O3 catalyst10.1016/S1386-1425(98)00312-6 ↗
32. Phase transitions in yttrium oxide at high pressure studied by Raman spectroscopy10.1016/S0025-5408(99)00205-6 ↗
33. Amorphous to crystalline transformation in Ta2O5 studied by Raman spectroscopy10.1002/jrs.3142 ↗
34. Self-repairing behavior of oxidation diffusion layer and phase transformation mechanism during tensile test of 19Cr duplex stainless steels with various Mn content10.1016/j.corsci.2014.10.046 ↗
35. TiO2/vanadate (Sr10V6O25, Ni3V2O8, Zn2V2O7) heterostructured photocatalysts with enhanced photocatalytic activity for photoreduction of CO2 into CH410.1039/C5NR05332C ↗
36. Temperature-dependent vibrational spectroscopic and X-ray diffraction investigation of nanosized nickel chromite10.1016/j.molstruc.2014.11.007 ↗
37. Cobalt chromite obtained by thermal decomposition of oxalate coordination compounds10.1016/j.ceramint.2014.07.009 ↗
38. High temperature corrosion behavior of a unidirectionally solidified Al2O3/YAG eutectic composite10.2109/jcersj.111.87 ↗
39. Hot corrosion of materials: a fluxing mechanism?10.1016/S0010-938X(01)00057-9 ↗
40. Hot corrosion behaviour of a cobalt-base super-alloy K40S with and without NiCrAlYSi coating10.1016/j.corsci.2011.02.022 ↗
41. The role of sodium in the accelerated oxidation phenomenon termed sulfidation10.1007/BF02813266 ↗
42. Hardness and modulus measurements on oxide scales10.1080/09603409.1994.11689480 ↗
43. Structural, electrical and mechanical properties of NiO thin films grown by pulsed laser deposition10.1016/j.apsusc.2010.07.006 ↗
44. Mechanical properties of interface layers between cosintered alumina and spinel compacts10.1179/1743676114Y.0000000180 ↗
45. Effect of residual stresses and prediction of possible failure mechanisms on thermal barrier coating system by finite element method10.1007/s11666-010-9512-1 ↗
46. Deformation behaviour of intermetallic NiAl–Ta alloys with strengthening Laves phase for high-temperature applications IV. Effects of processing10.1016/S0966-9795(98)00137-X ↗
47. Alloys based on Cr–Cr2Ta containing Si10.1016/j.intermet.2013.11.002 ↗