Macro-galvanic effect and its influence on corrosion behaviors of friction stir welding joint of 7050-T76 Al alloy
Source abstract
Abstract
Abstract The corrosion behavior of various zones of the 7050-T76 aluminum alloy friction stir welding (FSW) joint and their interaction were studied. The wire beam electrode (WBE) analysis reveals that heat-affected zone (HAZ) adjacent to nugget zone (NZ) receives the most intense negative current and thus presents the intensified susceptibility to corrosion. Both pitting and intergranular corrosion are aggravated greatly in HAZ while suppressed in base material (BM) when the whole FSW joint was put into NaCl solution, indicating the dominating influence from macro-galvanic effect. The coupling relationship between macro-galvanic and micro-galvanic effects is revealed based on the electrochemical analysis.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced Welding Techniques Analysis · Welding Techniques and Residual Stresses · Aluminum Alloy Microstructure Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (47)
Show source-provided references
1. Friction stir welding and processing10.1016/j.mser.2005.07.001 ↗
2. Recent developments in friction stir welding of Al-alloys10.1007/s11665-014-0968-x ↗
3. Relationship between microstructure, microhardness and corrosion sensitivity of an AA 2024-T3 friction stir welded joint10.1016/j.corsci.2011.05.049 ↗
4. Corrosion behavior and mechanical properties of Al-Zn-Mg aluminum alloy weld10.1016/j.corsci.2017.05.007 ↗
5. Characterisation of microstructure, mechanical properties and corrosion behaviour of an AA2219 friction stir weldment10.1016/j.jallcom.2009.11.198 ↗
6. Friction stir welding of aluminium alloys10.1179/174328009X411136 ↗
7. A cast 7050 friction stir weld with scandium: microstructure, corrosion and environmental assisted cracking10.1016/j.msea.2006.03.065 ↗
8. Corrosion susceptibility of peened friction stir welded 7075 aluminum alloy joints10.1016/j.corsci.2008.09.031 ↗
9. The corrosion and environmentally assisted cracking behavior of high strength aluminum alloys friction stir welds: 7075-T651 vs. 7050-T7451
10. The time-temperature-corrosion susceptibility in a 7050-T7451 friction stir weld10.1016/j.msea.2008.03.039 ↗
11. Localized corrosion susceptibility of Al-Li-Cu-Mg-Zn alloy AF/C458 due to interrupted quenching from solutionizing temperature10.1007/s11661-001-0046-5 ↗
12. Characterisation and understanding of the corrosion behaviour of the nugget in a 2050 aluminum alloy friction stir welding joint10.1016/j.corsci.2013.04.001 ↗
13. Effect of varying conditions of exposure to an aggressive medium on the corrosion behavior of the 2050 Al-Cu-Li alloy10.1016/j.corsci.2014.04.042 ↗
14. Effect of processing parameters on the corrosion behaviour of friction stir processed AA 2219 aluminum alloy10.1016/j.solidstatesciences.2008.11.007 ↗
15. Influence of processing parameters on induced energy, mechanical and corrosion properties of FSW butt joint of 7475 AA10.1007/s11665-011-0074-2 ↗
16. The effect of welding parameters on the corrosion behaviour of friction stir welded AA2024–T35110.1016/j.corsci.2006.05.038 ↗
17. Anodising and corrosion resistance of AA 7050 friction stir welds10.1016/j.corsci.2016.10.015 ↗
18. Improvement in corrosion resistance of friction stir welded aluminum alloys with micro arc oxidation coatings10.1016/j.scriptamat.2008.01.033 ↗
19. Improvement of weld temperature distribution and mechanical properties of 7050 aluminum alloy butt joints by submerged friction stir welding10.1016/j.matdes.2011.06.021 ↗
20. Use of silane films modified with Y2O3 nanoparticles for improved corrosion resistance of AA 606110.1179/175035211X13171296654479 ↗
21. Corrosion behaviour of different tempers ofAA7075 aluminum alloy10.1016/j.electacta.2004.01.046 ↗
22. A study on corrosion behavior of friction stir welded and tungsten inert gas welded AA2014 aluminum alloy10.1016/j.corsci.2018.01.012 ↗
23. Corrosion behaviour of friction stir welded AA7108 T79 aluminum alloy10.1016/j.corsci.2005.02.020 ↗
24. Effects of friction stir welding on microstructure of 7075 aluminum10.1016/S1359-6462(96)00344-2 ↗
25. Corrosion behaviour of friction stir-welded AA6005-T6 using a bobbin tool10.1016/j.corsci.2016.04.046 ↗
26. Influence of multi-Pass friction stir processing on the corrosion behavior of an Al-Mg-Si alloy10.1149/2.1091603jes ↗
27. Achieving superior corrosion resistance in friction stir processed AA6005-T6 aluminum alloy joints10.1149/06426.0029ecst ↗
28. Ma · 2003 · 221
29. Donford · 1998
30. Corrosion of friction-stir welded aluminum alloys 2024 and 219510.1023/A:1026710422951 ↗
31. Microstructural investigation of friction stir welded 7050-T651 aluminum10.1016/S1359-6454(02)00449-4 ↗
32. Temperature evolution, microstructure and mechanical properties of friction stir welded thick 2219-O aluminum alloy joints10.1016/j.matdes.2008.09.021 ↗
33. Corrosion study of the friction stir lap joint of AA7050-T76511 on AA2024-T3 using the scanning vibrating electrode technique10.1016/j.corsci.2015.02.029 ↗
34. SVET, SKP and EIS study of the corrosion behaviour of high strength Al and Al–Li alloys used in aircraft fabrication10.1016/j.corsci.2014.03.001 ↗
35. Investigation of mechanical and corrosion properties of an Al-Zn-Mg-Cu alloy under various ageing conditions and interface analysis of η’ precipitate10.1016/j.matdes.2015.06.183 ↗
36. Ageing behavior and stress corrosion cracking resistance of a non-isothermally aged Al–Zn–Mg–Cu alloy10.1016/j.msea.2014.03.023 ↗
37. Microstructure mapping in friction stir welds of 7449 aluminum alloy using SAXS10.1016/j.actamat.2006.06.015 ↗
38. Accelerated precipitation and growth of phases in an Al-Zn-Mg-Cu alloy processed by surface abrasion
39. Intergranular corrosion following friction stir welding of aluminum alloy 7075-T65110.5006/1.3283950 ↗
40. Effect of precipitate state on the stress corrosion behavior of 7050 aluminum alloy10.1016/j.matchar.2016.01.022 ↗
41. Effect of tool pin-tip profiles on material flow and mechanical properties of friction stir welding thick AA7075-T6 alloy joints10.1007/s00170-016-8886-8 ↗
42. Three-dimensional visualization of material flow during friction stir welding of steel and aluminum10.1007/s11665-014-1202-6 ↗
43. A look in the corrosion of aluminum alloy friction stir welds10.1016/j.scriptamat.2007.10.043 ↗
44. The effect of quench rate and overageing temper on the corrosion behaviour of AA705010.1016/j.corsci.2013.10.010 ↗
45. Mechanism of low exfoliation corrosion resistance due to slow quenching in high strength aluminium alloy10.1016/j.corsci.2014.11.024 ↗
46. Area relationships in galvanic corrosion10.5006/0010-9312-27.10.436 ↗
47. Galvanic corrosion of Al alloys-III. The effect of area ratio10.1016/S0010-938X(75)80019-9 ↗