journal article·2020-04

Cyclic oxidation behaviour of Ti/TiAlN composite multilayer coatings deposited on titanium alloy

Mingming Zhang, Yuxian Cheng, Li Xin, Jianxiu Su, Yongfeng Li, Shenglong Zhu, Fuhui Wang

Corrosion Science· Volume 166
Publisher page

Abstract

Abstract Cyclic oxidation behavior of titanium alloy coated with Ti/TiAlN composite multilayer coatings with various Ti layer thicknesses and TiAlN single layer coatings with different thicknesses was investigated at 750 °C. Ti(0.3 μm)/TiAlN multilayer coating exhibited excellent oxidation resistance. However, cracks formed in thick TiAlN single layer and Ti(0.15 μm)/TiAlN composite multilayer coatings, and titania nodules formed in thin TiAlN single layer coating. Cracking of Ti(0.15 μm)/TiAlN multilayer coating was due to that stress of coating could not be accommodated and relieved by ductile Ti phase owing to entire nitridation of Ti layers to layers composed of TiN and Ti2N.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Metal and Thin Film Mechanics · High-Temperature Coating Behaviors · Intermetallics and Advanced Alloy Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (58)

Show source-provided references
1. Effect of temperature on oxidation behaviour of Ga-containing near-α Ti alloy10.1016/j.corsci.2018.01.018 ↗
2. Electrochemical behaviour of passive film formed on the surface of Ti-6Al-4V alloys fabricated by electron beam melting10.1016/j.corsci.2018.09.010 ↗
3. Microstructure and erosive wear behaviors of Ti6Al4V alloy treated by plasma Ni alloying10.1016/j.apsusc.2015.10.231 ↗
4. Solid particle erosion mechanisms of protective coatings for aerospace applications10.1016/j.surfcoat.2014.08.037 ↗
5. Ti-N multilayer systems for compressor airfoil sand erosion protection10.1016/j.surfcoat.2009.09.053 ↗
6. Microstructural aspects of plain aluminide and Pt-aluminide coatings on Ti-base alloy IMI-83410.1016/j.intermet.2005.02.006 ↗
7. Silicide coatings on Ti-6Al-1Mn (at.%) alloy and their oxidation resistance10.1016/j.surfcoat.2017.12.004 ↗
8. Microstructures and oxidation behavior of NiCrAlCoY-Al composite coatings on Ti-6Al-4V alloy substrate via high-energy mechanical alloying method10.1016/j.jallcom.2016.10.171 ↗
9. Microstructure and oxidation resistance of a NiCrAlY/Al2O3-sprayed coating onTi-19Al-10Nb-Valloy10.1016/j.ceramint.2016.04.148 ↗
10. The effects of several coatings on cyclic oxidation resistance of TiAl intermetallics10.1016/S0257-8972(98)00645-8 ↗
11. Cyclic oxidation behaviour of the titanium alloys Ti-6242 and Ti-17 with Ti-Al-Cr-Y coatings at 600 and 700 °C in air10.1016/j.surfcoat.2013.02.021 ↗
12. Fabrication and oxidation behavior of Cr2AlC coating on Ti6242 alloy10.1016/j.surfcoat.2010.01.002 ↗
13. Novel coating systems produced by the combined cathodic arc/unbalanced magnetron sputtering for environmental protection of titanium alloys10.1016/S0257-8972(02)00063-4 ↗
14. Oxide scales formation in nano-crystalline TiAlCrSiYN PVD coatings at elevated temperature10.1016/j.ijrmhm.2009.09.003 ↗
15. Effects of silicon and multilayer structure of TiAl(Si)N coatings on the oxidation resistance of Ti6Al4V10.1016/j.surfcoat.2013.04.003 ↗
16. Oxidation protection of commercial-purity titanium by Na2O-CaO-SiO2 and SiO2-Al2O3-CaO-Na2O glass-ceramic coatings10.1016/j.ceramint.2014.08.075 ↗
17. Glass-ceramic coatings on titanium alloys for high temperature oxidation protection: oxidation kinetics and microstructure10.1016/j.corsci.2013.04.041 ↗
18. Solid particle erosion mechanisms of hard protective coatings10.1016/j.surfcoat.2013.07.050 ↗
19. Effect of ion bombardment on structural, mechanical, erosion and corrosion properties of Ti-Si-C-N nanocomposite coatings10.1016/j.surfcoat.2014.09.006 ↗
20. Nanolayered multilayer Ti/TiN coatings: Role of bi-layer thickness and annealing on solid particle erosion behaviour at elevated temperature10.1016/j.surfcoat.2018.10.007 ↗
21. Structural, mechanical, and sand erosion properties of TiN/Zr/ZrN multilayer coatings10.1016/j.vacuum.2015.09.026 ↗
22. Film thickness effect on mechanical properties and milling performance of nano-structured multilayer PVD coated tools10.1016/j.surfcoat.2016.09.026 ↗
23. Solid particle erosion of thick PVD coatings on CFRP10.1016/j.wear.2014.05.016 ↗
24. The influence of the coating thickness on its strength properties and on the milling performance of PVD coated inserts10.1016/S0257-8972(03)00678-9 ↗
25. Erosion resistant titanium based PVD coatings on CFRP10.1016/j.wear.2013.01.045 ↗
26. Research on cavitation erosion and wear resistance performance of coatings10.1016/j.engfailanal.2015.06.003 ↗
27. The corrosion resistance and wear resistance of thick TiN coatings deposited by arc ion plating10.1016/S0257-8972(01)01284-1 ↗
28. Improvement of the corrosion resistance of PVD hard coating-substrate systems10.1016/S0257-8972(99)00551-4 ↗
29. Structural, mechanical and corrosion resistance properties of Ti/TiN bilayers deposited by magnetron sputtering on AISI 316L10.1016/j.surfcoat.2017.05.075 ↗
30. Damage evolution and mechanism of TiN/Ti multilayer coatings in sand erosion condition10.1016/j.surfcoat.2018.08.062 ↗
31. Microstructure evolution and corrosion resistance of multi interfaces Al-TiAlN nanocomposite films on AZ91D magnesium alloy10.1016/j.surfcoat.2018.09.019 ↗
32. Mechanical properties and tribological behavior of magnetron sputtered TiAlN/TiAl multilayer coatings10.1016/j.surfcoat.2018.09.001 ↗
33. Influence of Ti/TiAlN-multilayer designs on their residual stresses and mechanical properties10.1016/j.apsusc.2011.05.013 ↗
34. Investigation of anomalous physical properties of multilayer nanolaminate (TiAl)N/Cu coatings by electron spectroscopy techniques10.1002/sia.3290 ↗
35. Optimization and thermal stability of TiAlN/Mo multilayers10.1016/j.surfcoat.2005.02.099 ↗
36. Mechanical properties and thermal stability of TiAlN/Ta multilayer film deposited by ion beam assisted deposition10.1016/j.apsusc.2014.03.099 ↗
37. Ti-Al-N/Mo-Si-B multilayers: An architectural arrangement for high temperature oxidation resistant hard coatings10.1016/j.surfcoat.2017.08.032 ↗
38. Atomic scale investigations of thermally treated nano-structured Ti-Al-N/Mo-Si-B multilayers10.1016/j.surfcoat.2018.06.026 ↗
39. Mechanical and tribological properties of Ti/TiAlN duplex coatings on high and low alloy tool steels10.1016/j.vacuum.2009.08.001 ↗
40. The influence of multilayer design on residual stress gradients in Ti/TiAlN systems10.4028/www.scientific.net/MSF.768-769.264 ↗
41. Influence of substrate pre-treatments on residual stresses and tribo-mechanical properties of TiAlN-based PVD coatings10.1016/j.surfcoat.2014.08.075 ↗
42. Effect of ductile layers in mechanical behaviour of TiAlN thin coatings10.1016/S0924-0136(03)00454-0 ↗
43. Development of wear resistant pressing moulds for the production of diamond composites10.1016/j.jmatprotec.2008.11.005 ↗
44. Zhang · 2018
45. X-ray photoelectron spectroscopy studies of Ti1-xAlxN (0≤x≤0.83) high temperature oxidation: the crucial role of Al concentration10.1016/j.surfcoat.2019.06.081 ↗
46. High thickness Ti/TiN multilayer thin coatings for wear resistant applications10.1016/j.surfcoat.2006.03.042 ↗
47. Samsonov · 1982
48. Fatigue improvement in low temperature plasma nitrided Ti-6Al-4V alloy10.1016/j.msea.2014.10.008 ↗
49. Oxidation of metastable single-phase polycrystalline Ti0.5Al0.5N films: kinetics and Mechanisms10.1063/1.345664 ↗
50. Residual stress development in UMS TiN coatings10.1016/j.surfcoat.2005.08.049 ↗
51. Residual stresses in nitride hard coatings prepared by magnetron sputtering and arc evaporation10.1016/0257-8972(95)08235-2 ↗
52. Depth distribution of residual stress in graded (Ti, Al) N coating and fatigue properties of coated stainless steel10.4028/www.scientific.net/MSF.595-598.223 ↗
53. Mechanical behavior of (Ti,Al)N coatings exposed to elevated temperatures and an oxidative environment10.1016/S0257-8972(00)00939-7 ↗
54. Effect of heating on the residual stresses in TiN films investigated using synchrotron radiation10.1016/j.vacuum.2008.04.068 ↗
55. Investigations on structural, elastic, thermodynamic and electronic properties of TiN, Ti2N and Ti3N2 under high pressure by first-principles10.1016/j.jpcs.2016.05.012 ↗
56. Internal stress and adherence of titanium nitride coatings10.1116/1.573683 ↗
57. Localised oxidation defects in TiAlN/CrN superlattice structured hard coatings grown by cathodic arc/ unbalanced magnetron deposition on various substrate materials10.1016/S0257-8972(99)00571-X ↗
58. Mechanical Properties and Oxidation Behavior of a Graded (Ti,Al)N Coating Deposited by Arc-Ion Plating10.1007/s11085-006-9015-0 ↗